# US 2019/0174578 A1 · SiC HEATER

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0174578 A1
- Document ID: US20190174578A1
- Status: Published application
- Kind: A1
- Application number: 16/322,425
- Filed: 2017-08-02
- Published: 2019-06-06
- Earliest claimed: 2016-08-02
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Applicants: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Hiroaki NAGATOMO; Yuki UCHIKAWA; Yoshihiko MURAKAMI
- Web page: https://patentgrep.com/patent/US20190174578A1

## CPC

- H05B 3/148: {Silicon, e.g. silicon carbide, magnesium silicide, heating transistors or diodes}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/089: containing boron
- C03C 3/091: containing aluminium
- C03C 8/16: with vehicle or suspending agents, e.g. slip
- C04B 35/575: obtained by pressure sintering
- H05B 3/03: Electrodes
- H05B 3/06: Heater elements structurally combined with coupling elements or holders
- H05B 3/12: characterised by the composition or nature of the conductive material
- H05B 3/14: the material being non-metallic
- H05B 3/20: Heating elements having extended surface area substantially in a two-dimensional [2D] plane, e.g. plate-heater (H05B3/62, H05B3/68, H05B3/78, H05B3/84 take precedence)
- C04B 2235/3826: Silicon carbides
- C04B 2235/383: Alpha silicon carbide
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/5454: nanometer sized, i.e. below 100 nm
- C04B 2235/5472: Bimodal, multi-modal or multi-fraction
- C04B 2235/77: Density
- C04B 2235/9607: Thermal properties, e.g. thermal expansion coefficient
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

This SiC heater includes a heating element having a thin plate-shaped silicon carbide sintered body and an insulating coat film formed on a surface of the silicon carbide sintered body, a pair of electrodes for conducting electricity in the heating element, and a heater base that holds the heating element from one surface side while insulating the heating element from heat from the heating element, the insulating coat film is located on a surface of the silicon carbide sintered body opposite to the heater base, an electrical resistivity at room temperature of the insulating coat film is 109 Ω·cm or more, a thermal expansion coefficient of the insulating coat film is 2×10−6/K or more and 6×10−6/K or less, SiO2 is included as a matrix, 1% by weight or more and 35% by weight or less of a first additive component including at least one of B2O3 and Al2O3 is contained, and 1% by weight or more and 35% by weight or less of a second additive component including at least one of MgO and CaO is contained.

## Claims

### Claim 1

A SiC heater comprising:
a heating element comprising a thin plate-shaped silicon carbide sintered body and an insulating coat film formed on a surface of the silicon carbide sintered body;
a pair of electrodes for conducting electricity in the heating element; and
a heater base that holds the heating element from one surface side while blocking the heat from the heating element,
wherein the insulating coat film is located on a surface of the silicon carbide sintered body, the surface being on the reverse side of the heater base-side surface,
an electrical resistivity at room temperature of the insulating coat film is 109 Ω·cm or more,
a thermal expansion coefficient of the insulating coat film is 2×10−6/K or more and 6×10−6/K or less,
the insulating coat film includes SiO2 as a matrix,
the insulating coat film contains a first additive component including at least one of B2O3 and Al2O3,
a proportion of the first additive component is 1% by weight or more and 35% by weight or less of a total weight of the insulating coat film,
the insulating coat film contains a second additive component including at least one of MgO and CaO, and
a proportion of the second additive component is 1% by weight or more and 35% by weight or less of the total weight of the insulating coat film.

### Claim 2 (depends on 1)

The SiC heater according to claim 1,
wherein the second additive component further includes BaO.

### Claim 3 (depends on 2)

The SiC heater according to claim 2,
wherein the second additive component includes all of BaO, MgO, and CaO.

### Claim 4 (depends on 3)

The SiC heater according to claim 3,
wherein a total of contents of MgO and CaO of the second additive component is equal to or more than and twice or less than a content of BaO.

### Claim 5 (depends on 1)

The SiC heater according to claim 1,
wherein a shape of the heating element is a substantial S shape in a plan view having two slits notched from two facing sides of a substantially square shape or a substantially rectangular shape in a plan view toward opposite sides respectively, and both end portions of the substantial S shape are respectively connected to the pair of electrodes.

### Claim 6 (depends on 1)

The SiC heater according to claim 1,
wherein the insulating coat film is made of at least one of borosilicate glass or aluminosilicate glass.

### Claim 7 (depends on 1)

The SiC heater according to claim 1,
wherein a proportion of the first additive component is 1% by weight or more and 30% by weight or less of the total weight of the insulating coat film.

### Claim 8 (depends on 1)

The SiC heater according to claim 1,
wherein a bonded sintered body density of the silicon carbide sintered body is 2.5 g/cm3 or more, and an electrical resistivity at 25° C. is 0.1 Ω·cm or more and 100 Ω·cm or less.

### Claim 9 (depends on 2)

The SiC heater according to claim 2,
wherein a shape of the heating element is a substantial S shape in a plan view having two slits notched from two facing sides of a substantially square shape or a substantially rectangular shape in a plan view toward opposite sides respectively, and both end portions of the substantial S shape are respectively connected to the pair of electrodes.

### Claim 10 (depends on 2)

The SiC heater according to claim 2,
wherein the insulating coat film is made of at least one of borosilicate glass or aluminosilicate glass.

### Claim 11 (depends on 2)

The SiC heater according to claim 2,
wherein a proportion of the first additive component is 1% by weight or more and 30% by weight or less of the total weight of the insulating coat film.

### Claim 12 (depends on 2)

The SiC heater according to claim 2,
wherein a sintered body density of the silicon carbide sintered body is 2.5 g/cm3 or more, and an electrical resistivity at 25° C. is 0.1 Ω·cm or more and 100 Ω·cm or less.

### Claim 13 (depends on 3)

The SiC heater according to claim 3,
wherein a shape of the heating element is a substantial S shape in a plan view having two slits notched from two facing sides of a substantially square shape or a substantially rectangular shape in a plan view toward opposite sides respectively, and both end portions of the substantial S shape are respectively connected to the pair of electrodes.

### Claim 14 (depends on 3)

The SiC heater according to claim 3,
wherein the insulating coat film is made of at least one of borosilicate glass or aluminosilicate glass.

### Claim 15 (depends on 3)

The SiC heater according to claim 3,
wherein a proportion of the first additive component is 1% by weight or more and 30% by weight or less of the total weight of the insulating coat film.

### Claim 16 (depends on 3)

The SiC heater according to claim 3,
wherein a sintered body density of the silicon carbide sintered body is 2.5 g/cm3 or more, and an electrical resistivity at 25° C. is 0.1 Ω·cm or more and 100 Ω·cm or less.

### Claim 17 (depends on 4)

The SiC heater according to claim 4,
wherein a shape of the heating element is a substantial S shape in a plan view having two slits notched from two facing sides of a substantially square shape or a substantially rectangular shape in a plan view toward opposite sides respectively, and both end portions of the substantial S shape are respectively connected to the pair of electrodes.

### Claim 18 (depends on 4)

The SiC heater according to claim 4,
wherein the insulating coat film is made of at least one of borosilicate glass or aluminosilicate glass.

### Claim 19 (depends on 4)

The SiC heater according to claim 4,
wherein a proportion of the first additive component is 1% by weight or more and 30% by weight or less of the total weight of the insulating coat film.

### Claim 20 (depends on 4)

The SiC heater according to claim 4,
wherein a sintered body density of the silicon carbide sintered body is 2.5 g/cm3 or more, and an electrical resistivity at 25° C. is 0.1 Ω·cm or more and 100 Ω·cm or less.