# US 2019/0173088 A1 · Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0173088 A1
- Document ID: US20190173088A1
- Status: Published application
- Kind: A1
- Application number: 16/161,978
- Filed: 2018-10-16
- Published: 2019-06-06
- Earliest claimed: 2017-12-05
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Chengdu LIANG; Huafeng HUANG; Qisen HUANG
- Web page: https://patentgrep.com/patent/US20190173088A1

## CPC

- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/625: {Carbon or graphite}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A battery is provided in the present disclosure. The battery includes: a positive electrode plate including a positive current collector and a positive active material layer; a negative electrode plate including a positive current collector and a negative active material layer; and an electrolyte. The positive current collector includes an insulation layer used to support a conductive layer and the conductive layer used to support the positive active material layer and located above at least one surface of the insulation layer. The conductive layer has a thickness of D2 which satisfies: 300 nm≤D2≤2 μm. A protective layer is arranged on at least one surface of the conductive layer. The negative current collector is a copper foil current collector having a thickness of 6 μm to 12 μm.

## Claims

### Claim 1

A battery, comprising
a positive electrode plate comprising a positive current collector and a positive active material layer;
a negative electrode plate comprising a negative current collector and a negative active material layer, and
an electrolyte,
wherein the positive current collector comprises an insulation layer and at least one conductive layer, the insulation layer is used to support the at least one conductive layer, each of the at least one conductive layer is used to support the positive active material layer and is located above at least one surface of the insulation layer, and each of the at least one conductive layer has a thickness of D2 satisfying: 300 nm≤D2≤2 μm,
wherein at least one protective layer is arranged on at least one surface of each of the at least one conductive layer, and
wherein the negative current collector is a copper foil current collector having a thickness of 6 μm to 12 μm.

### Claim 2 (depends on 1)

The battery according to claim 1, wherein the at least one conductive layer is made of a metallic conductive material, and the metallic conductive material is preferably selected from a group consisting of aluminum, copper, nickel, titanium, silver, nickel-copper alloy, aluminum-zirconium alloy, or combinations thereof; and
wherein the at least one protective layer is made of a metal oxide material, and the metal oxide material is preferably selected from a group consisting of aluminum oxide, cobalt oxide, chromium oxide, nickel oxide, or combinations thereof.

### Claim 3 (depends on 1)

The battery according to claim 1, wherein one of the at least one protective layer is arranged on a surface of one of the at least one conductive layer facing away from the insulation layer.

### Claim 4 (depends on 1)

The battery according to claim 1, wherein another one of the at least one protective layer is arranged on a surface of one of the at least one conductive layer facing the insulation layer.

### Claim 5 (depends on 3)

The battery according to claim 3, wherein another one of the at least one protective layer is arranged on a surface of one of the at least one conductive layer facing the insulation layer.

### Claim 6 (depends on 1)

The battery according to claim 1, wherein each of the at least one protective layer has a thickness of D3 satisfying: D3≤ 1/10 D2 and 1 nm≤D3≤200 nm, preferably 10 nm≤D3≤50 nm.

### Claim 7 (depends on 1)

The battery according to claim 1, wherein the positive active material layer comprises a positive active material, a binder, and a conductive additive, and wherein a mass percentage of the conductive additive to the positive active material layer is larger than or equal to 0.8 wt %.

### Claim 8 (depends on 1)

The battery according to claim 1, wherein the electrolyte has a room temperature conductivity of 6.0 mS/cm to 9.0 mS/cm.

### Claim 9 (depends on 1)

The battery according to claim 1, wherein the at least one conductive layer is made of aluminum, and the thickness of the conductive layer satisfies 500 nm≤D2≤1.5 μm; and
wherein the at least one protective layer is made of nickel oxide or aluminum oxide, and the at least one protective layer includes two protective layers arranged on two opposite surfaces of one of the at least one conductive layer.

### Claim 10 (depends on 9)

The battery according to claim 9, wherein the thickness of the protective layer arranged on the surface of the one of the at least one conductive layer facing away from the insulation layer is greater than the thickness of the protective layer arranged on the surface of the one of the conductive layer facing the insulation layer.

### Claim 11 (depends on 1)

The battery according to claim 1, wherein the insulation layer has a thickness of D1 satisfying: 1 μm≤D1≤20 μm, preferably 2 μm≤D1≤10 μm, and more preferably 2 μm≤D1≤6 μm;
preferably, the insulation layer is made of an organic polymer insulation material, and the organic polymer insulation material is preferably selected from a group consisting of polyamide, polyethylene terephthalate, polyimide, polyethylene, polypropylene, polystyrene, polyvinyl chloride, acrylonitrile-butadiene-styrene copolymer, polybutylene terephthalate, poly-p-phenylene terephthalamide, ethylene propylene rubber, polyformaldehyde, epoxy resin, phenol-formaldehyde resin, polytetrafluoroethylene, polyvinylidene fluoride, silicone rubber, polycarbonate, or combinations thereof.