# US 2019/0173013 A1 · Method of producing film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0173013 A1
- Document ID: US20190173013A1
- Status: Published application
- Kind: A1
- Application number: 16/270,289
- Filed: 2019-02-07
- Published: 2019-06-06
- Earliest claimed: 2016-09-27
- Assignees: FUJIFILM Corporation
- Applicants: FUJIFILM Corporation
- Inventors: Seigo NAKAMURA; Hiroyuki YAEGASHI
- Web page: https://patentgrep.com/patent/US20190173013A1

## CPC

- H10K 71/15: characterised by the solvent used
- B05D 1/26: performed by applying the liquid or other fluent material from an outlet device in contact with, or almost in contact with, the surface
- B05D 1/42: by non-rotary members
- H10D 30/67: Thin-film transistors [TFT] {(Stacked nanowire, nanosheet or nanoribbon FETs H10D30/501)}
- H10D 30/6733: {Multi-gate TFTs}
- H10K 10/484: {characterised by the channel regions}
- H10K 71/12: using liquid deposition, e.g. spin coating
- H10K 77/10: Substrates, e.g. flexible substrates
- H10K 85/731: {Liquid crystalline materials}
- B05D 2252/02: of indefinite length
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a method of producing a high-quality film having a thin film and high uniformity in film thickness or the like. The method of producing a film includes supplying a raw material solution containing a solvent and a material that forms a film onto a substrate and drying the solvent to form the film on the substrate. A coating blade holding the raw material solution on the substrate is used, and the coating blade has a facing surface which faces a surface of the substrate and at least one side surface which is provided in the periphery of the facing surface and is in contact with the raw material solution. The solvent of the raw material solution is dried along a specific direction to form the film.

## Claims

### Claim 1

A method of producing a film, comprising:
supplying a raw material solution containing a solvent and a material that forms a film onto a substrate and drying the solvent to form the film on the substrate,
wherein a coating blade holding the raw material solution on the substrate is used,
the coating blade has a facing surface which faces a surface of the substrate and at least one side surface which is provided in the periphery of the facing surface and is in contact with the raw material solution,
a position of the coating blade is fixed to the surface of the substrate, and
the solvent of the raw material solution is dried along a specific direction to form the film.

### Claim 2

A method of producing a film, comprising:
supplying a raw material solution containing a solvent and a material that forms a film onto a substrate and drying the solvent to form the film on the substrate,
wherein a coating blade holding the raw material solution on the substrate is used,
the coating blade has a facing surface which faces a surface of the substrate, at least one side surface which is provided in the periphery of the facing surface and is in contact with the raw material solution, and an open part that opens at least a part in the periphery of the raw material solution,
the substrate is moved in a direction toward the open part from the center of the raw material solution, and
the solvent of the raw material solution is dried along a specific direction to form the film.

### Claim 3 (depends on 1)

The method of producing a film according to claim 1,
wherein at least three surfaces, which are the facing surface and two side surfaces of the coating blade, are in contact with the raw material solution.

### Claim 4 (depends on 1)

The method of producing a film according to claim 1,
wherein the specific direction in which the raw material solution is dried is determined by at least one surface from among the facing surface and at least two side surfaces of the coating blade.

### Claim 5 (depends on 1)

The method of producing a film according to claim 1,
wherein the specific direction in which the raw material solution is dried is determined only by one surface from among the facing surface and at least two side surfaces of the coating blade.

### Claim 6 (depends on 5)

The method of producing a film according to claim 5,
wherein the specific direction in which the raw material solution is dried is determined only by the facing surface of the coating blade.

### Claim 7 (depends on 1)

The method of producing a film according to claim 1,
wherein the coating blade has two side surfaces, and
two side surfaces are respectively perpendicular to the surface of the substrate and provided so as to face each other.

### Claim 8 (depends on 1)

The method of producing a film according to claim 1,
wherein the facing surface of the coating blade is inclined with respect to the surface of the substrate.

### Claim 9 (depends on 8)

The method of producing a film according to claim 8,
wherein a tilt angle of the facing surface of the coating blade with respect to the surface of the substrate is in a range of 1° to 6°.

### Claim 10 (depends on 1)

The method of producing a film according to claim 1,
wherein a film growth interface of the raw material solution held on the substrate by the coating blade is curved toward the center of the raw material solution.

### Claim 11 (depends on 10)

The method of producing a film according to claim 10,
wherein the substrate is moved while the raw material solution is supplied to a space between the surface of the substrate and the coating blade so that the film is continuously formed.

### Claim 12 (depends on 1)

The method of producing a film according to claim 1,
wherein, in a case where a boiling point of the solvent of the raw material solution is set as Tb° C. and a substrate temperature is set as Ts° C., the substrate temperature Ts is held at a temperature satisfying an expression of “Tb−50° C.≤Ts≤Tb”.

### Claim 13 (depends on 1)

The method of producing a film according to claim 1,
wherein the film is formed of a material having an aligning property.

### Claim 14 (depends on 13)

The method of producing a film according to claim 13,
wherein the material having an aligning property is a material or an organic semiconductor that forms a crystal.

### Claim 15 (depends on 2)

The method of producing a film according to claim 2,
wherein at least three surfaces, which are the facing surface and two side surfaces of the coating blade, are in contact with the raw material solution.

### Claim 16 (depends on 2)

The method of producing a film according to claim 2,
wherein the specific direction in which the raw material solution is dried is determined by at least one surface from among the facing surface and at least two side surfaces of the coating blade.

### Claim 17 (depends on 2)

The method of producing a film according to claim 2,
wherein the specific direction in which the raw material solution is dried is determined only by one surface from among the facing surface and at least two side surfaces of the coating blade.

### Claim 18 (depends on 2)

The method of producing a film according to claim 2,
wherein the coating blade has two side surfaces, and
two side surfaces are respectively perpendicular to the surface of the substrate and provided so as to face each other.

### Claim 19 (depends on 2)

The method of producing a film according to claim 2,
wherein the facing surface of the coating blade is inclined with respect to the surface of the substrate.

### Claim 20 (depends on 2)

The method of producing a film according to claim 2,
wherein a film growth interface of the raw material solution held on the substrate by the coating blade is curved toward the center of the raw material solution.