# US 2019/0172990 A1 · Semiconductor light-emitting apparatus having multiple semiconductor light-emitting elements and its manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0172990 A1
- Document ID: US20190172990A1
- Status: Published application
- Kind: A1
- Application number: 16/202,783
- Filed: 2018-11-28
- Published: 2019-06-06
- Earliest claimed: 2017-12-06
- Assignees: Stanley Electric Co., Ltd.
- Applicants: Stanley Electric Co., Ltd.
- Inventors: Mitsunori HARADA; Kaori TACHIBANA
- Web page: https://patentgrep.com/patent/US20190172990A1

## CPC

- H10H 20/857: Interconnections, e.g. lead-frames, bond wires or solder balls
- H10H 20/8514: {characterised by their shape, e.g. plate or foil}
- H10H 20/856: Reflecting means
- H10W 90/00: Package configurations
- H10H 20/0361: {of wavelength conversion means}
- H10H 20/0362: {of encapsulations}
- H10H 20/0364: {of interconnections}
- H10H 20/853: characterised by their shape
- H10H 20/854: characterised by their material, e.g. epoxy or silicone resins
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor light-emitting apparatus includes: a wiring substrate; multiple semiconductor light-emitting elements mounted via multiple eutectic layers, respectively, on the wiring substrate; and a wavelength-converting plate via multiple transparent adhesive layers on upper surfaces of the semiconductor light-emitting elements, respectively. A standard deviation of thicknesses of the transparent adhesive layers is smaller than a standard deviation of thicknesses of the eutectic layers.

## Claims

### Claim 1

A semiconductor light-emitting apparatus comprising:
a wiring substrate;
multiple semiconductor light-emitting elements mounted via multiple eutectic layers, respectively, on said wiring substrate; and
a wavelength-converting plate via multiple transparent adhesive layers on upper surfaces of said semiconductor light-emitting elements, respectively,
a standard deviation of thicknesses of said transparent adhesive layers being smaller than a standard deviation of thicknesses of said eutectic layers.

### Claim 2 (depends on 1)

The semiconductor light emitting apparatus as set forth in claim 1, wherein each of said multiple transparent adhesive layers comprises a eutectic temperature liquid transparent adhesive layer which maintains a liquid state even at a eutectic temperature of said multiple eutectic layers,
a thermosetting temperature of said eutectic temperature liquid transparent adhesive layer being lower than said eutectic temperature,
a time period for said eutectic temperature liquid transparent adhesive layer in a heated and cooled state whose temperature temporarily becomes higher than said eutectic temperature to change from a thermosetting starting point to a thermosetting ending point is larger than a time period for said multiple eutectic layers in said heated and cooled state to change from a eutectic starting point to a eutectic ending point.

### Claim 3 (depends on 2)

The semiconductor light-emitting apparatus as set forth in claim 2, wherein said eutectic temperature liquid layer comprises silicone resin.

### Claim 4 (depends on 2)

The semiconductor light-emitting apparatus as set forth in claim 2, wherein a thickness of said eutectic temperature liquid transparent adhesive layer is 2 μm to 15 μm.

### Claim 5 (depends on 1)

The semiconductor light-emitting apparatus as set forth in claim 1, further comprising a reflective layer surrounding sidewalls of said multiple semiconductor light-emitting elements and a sidewall of said wavelength-converting plate.

### Claim 6

A method for manufacturing a semiconductor light-emitting apparatus, comprising:
forming multiple eutectic material layers on multiple first electrode patterns, respectively, of a wiring substrate;
mounting multiple semiconductor light-emitting elements with second electrode patterns on its lower surface on said multiple eutectic material layers, respectively;
mounting a plate on said multiple semiconductor light-emitting elements via multiple eutectic temperature liquid layers, respectively, said multiple eutectic temperature liquid layers maintaining a liquid state even at a eutectic temperature of said multiple eutectic material layers;
heating and cooling said multiple eutectic material layers and said multiple temperature liquid layers so that said multiple eutectic material layers are cured to multiple eutectic layers with said multiple first electrode patterns and said multiple second electrode patterns, while said plate is adhered via said multiple eutectic temperature liquid layers to said multiple semiconductor light-emitting elements by the surface tension phenomenon.

### Claim 7 (depends on 6)

The method as set forth in claim 6, further comprising:
removing said plate and said eutectic temperature liquid layers after said heating and cooling; and
mounting a wavelength-converting plate via multiple transparent adhesive layers on said multiple semiconductor light-emitting elements after said removing.

### Claim 8 (depends on 7)

The method. as set forth in claim 7, wherein each of said multiple eutectic temperature liquid layers comprise silicone oil.

### Claim 9 (depends on 8)

The method as set forth in claim 8, wherein said plate comprises a glass plate.

### Claim 10 (depends on 6)

The method as set forth in claim 6, wherein said plate comprises a wavelength-converting plate.

### Claim 11 (depends on 10)

The method as set forth in claim 10, wherein each of said multiple transparent adhesive layers comprises a eutectic temperature liquid transparent adhesive layer which maintains a liquid state even at a eutectic temperature of said multiple eutectic layers,
a thermosetting temperature of said eutectic temperature liquid transparent adhesive layer being lower than said eutectic temperature,
a time period for said eutectic temperature liquid transparent adhesive layer in a heated and cooled state whose temperature temporarily becomes higher than said eutectic temperature to change from a thermosetting starting point to a thermosetting ending point is larger than a time period for said multiple eutectic layers in said heated and cooled state to change from a eutectic starting point to a eutectic ending point.

### Claim 12 (depends on 11)

The method as set forth in claim 11, wherein said eutectic temperature liquid transparent adhesive layer comprises silicone resin.

### Claim 13 (depends on 11)

The method as set forth in claim 11, wherein a thickness of said eutectic temperature liquid transparent adhesive layer is 2 μm to 15 μm.

### Claim 14 (depends on 6)

The method as set forth in claim 6, further comprising forming a reflective layer surrounding sidewalls of said multiple semiconductor light-emitting elements and a sidewall of said wavelength-converting plate.

### Claim 15 (depends on 9)

The method as set forth in claim 9, further comprising forming a reflective layer surrounding sidewalls of said multiple semiconductor light-emitting elements and a sidewall of said wavelength-converting plate.