# US 2019/0172800 A1 · Sensor and heater for stimulus-initiated fracture of a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0172800 A1
- Document ID: US20190172800A1
- Status: Published application
- Kind: A1
- Application number: 16/257,304
- Filed: 2019-01-25
- Published: 2019-06-06
- Earliest claimed: 2016-07-26
- Assignees: Palo Alto Research Center Incorporated
- Applicants: Palo Alto Research Center Incorporated
- Inventors: Christopher L. Chua; JengPing Lu; Gregory Whiting; Scott J. Limb; Rene A. Lujan; Qian Wang
- Web page: https://patentgrep.com/patent/US20190172800A1

## CPC

- H10W 42/405: {using active circuits}
- H03K 19/17768: for security
- H10F 71/103: {including only Group IV materials}
- H10W 20/493: {Fuses, i.e. interconnections changeable from conductive to non-conductive}
- H10W 40/10: Arrangements for heating
- H10W 42/40: protecting against tampering, e.g. unauthorised inspection or reverse engineering
- H10W 44/00: Electrical arrangements for controlling or matching impedance
- H10W 70/692: Ceramics or glasses
- H10D 18/00: Thyristors
- H10F 77/206: {for devices having potential barriers}
- H10F 77/247: {comprising indium tin oxide [ITO]}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H03K: PULSE TECHNIQUE (measuring pulse characteristics G01R; modulating sinusoidal oscillations with pulses H03C; transmission of digital information H04L; discriminator circuits detecting phase difference between two signals by counting or integrating cycles of oscillation H03D3/04; automatic control, starting, synchronisation or stabilisation of generators of electronic oscillations or pulses where the type of generator is irrelevant or unspecified H03L; coding, decoding or code conversion, in general H03M)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A self-destructing device includes a stressed substrate with a heater thermally coupled to the stressed substrate. The device includes a power source and trigger circuitry comprising a sensor and a switch. The sensor generates a trigger signal when exposed to a trigger stimulus. The switch couples the power source to the heater in response to the trigger signal When energized by the power source, the heater generates heat sufficient to initiate self-destruction of the stressed substrate.

## Claims

### Claim 1

A method of forming a photodiode comprising:
depositing a first electrode layer over a substrate;
depositing a first doped layer of an active region over the first electrode layer;
depositing an intrinsic layer over the first doped layer;
depositing a second doped layer of the active region over the intrinsic layer;
depositing a second electrode layer over the second doped layer; and
patterning the first electrode layer, the first doped layer, the intrinsic layer, the second doped layer, and the second electrode layer to form the photodiode in not more than two mask steps.

### Claim 2 (depends on 1)

The method of claim 1, wherein the patterning comprises:
patterning the first electrode layer and the first doped layer in a first patterning step using a first mask;
patterning the second electrode layer, the second doped layer, and the intrinsic layer in a second patterning step using a second mask; and
during the second patterning step removing the first doped layer in unprotected regions in a self-aligned manner.

### Claim 3 (depends on 1)

The method of claim 1, further comprising forming an adhesion promoting surface on the substrate, wherein depositing the first electrode layer comprises depositing the first electrode layer on the adhesion promoting surface.

### Claim 4 (depends on 3)

The method of claim 3, wherein forming the adhesion promoting surface comprises depositing a layer of silicon oxide, silicon nitride, or silicon oxynitride by plasma-enhanced chemical vapor deposition.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second electrode layer is configured to transmit a trigger stimulus to the active region of the photodiode.

### Claim 6 (depends on 1)

The method of claim 1, wherein depositing the second electrode layer comprises forming an optical filter that substantially attenuates wavelengths of light that are outside a wavelength band of a trigger stimulus and substantially passes wavelengths of light that are within the wavelength band of the trigger stimulus.

### Claim 7 (depends on 1)

The method of claim 1, wherein:
the substrate comprises a stressed substrate; and
the stressed substrate comprising at least one tensile stress layer having a residual tensile stress and at least one compressive stress layer having a residual compressive stress and being mechanically coupled to the at least one tensile stress layer such that the at least one tensile stress layer and the at least one compressive stress layer are self-equilibrating.

### Claim 8 (depends on 1)

The method of claim 1, wherein:
the substrate comprises a stressed substrate; and
the stressed substrate comprises chemically tempered glass.

### Claim 9

A method of forming a photodiode comprising:
depositing a first electrode layer over a stressed substrate;
depositing a first doped layer of an active region over the first electrode layer;
depositing an intrinsic layer over the first doped layer;
depositing a second doped layer of the active region over the intrinsic layer;
depositing a second electrode layer over the second doped layer; and
patterning the first electrode layer, the first doped layer, the intrinsic layer, the second doped layer, and the second electrode layer to form the photodiode.

### Claim 10 (depends on 9)

The method of claim 9, wherein the patterning comprises patterning the first electrode layer, the first doped layer, the intrinsic layer, the second doped layer, and the second electrode layer to form the photodiode in not more than two mask steps.

### Claim 11 (depends on 9)

The method of claim 9, wherein the patterning comprises:
patterning the first electrode layer and the first doped layer in a first patterning step using a first mask;
patterning the second electrode layer, the second doped layer, and the intrinsic layer in a second patterning step using a second mask; and
during the second patterning step removing the first doped layer in unprotected regions in a self-aligned manner.

### Claim 12 (depends on 9)

The method of claim 9, further comprising forming an adhesion promoting surface on the stressed substrate, wherein depositing the first electrode layer comprises depositing the first electrode layer on the adhesion promoting surface.

### Claim 13 (depends on 12)

The method of claim 12, wherein forming the adhesion promoting surface comprises depositing a layer of silicon oxide, silicon nitride, or silicon oxynitride by plasma-enhanced chemical vapor deposition.

### Claim 14 (depends on 9)

The method of claim 9, wherein the second electrode layer is configured to transmit a trigger stimulus to the active region of the photodiode.

### Claim 15 (depends on 9)

The method of claim 9, wherein depositing the second electrode layer comprises forming an optical filter that substantially attenuates wavelengths of light that are outside a wavelength band of a trigger stimulus and substantially passes wavelengths of light that are within the wavelength band of the trigger stimulus.

### Claim 16 (depends on 9)

The method of claim 9, wherein the stressed substrate includes at least one tensile stress layer having a residual tensile stress and at least one compressive stress layer having a residual compressive stress and being mechanically coupled to the at least one tensile stress layer such that the at least one tensile stress layer and the at least one compressive stress layer are self-equilibrating.

### Claim 17 (depends on 9)

The method of claim 9, wherein the stressed substrate comprises chemically tempered glass.

### Claim 18

A method of forming a photodiode comprising:
depositing a first electrode layer over a stressed substrate;
depositing a first doped layer of an active region over the first electrode layer;
depositing a second doped layer of the active region over the first doped layer;
depositing a second electrode layer over the second doped layer; and
patterning the first electrode layer, the first doped layer, the second doped layer, and the second electrode layer to form the photodiode.

### Claim 19 (depends on 18)

The method of claim 18, wherein the patterning comprises patterning the first electrode layer, the first doped layer, the second doped layer, and the second electrode layer to form the photodiode in not more than two mask steps.

### Claim 20 (depends on 18)

The method of claim 18, wherein the patterning comprises:
patterning the first electrode layer and the first doped layer in a first patterning step using a first mask;
patterning the second electrode layer and the second doped layer in a second patterning step using a second mask; and
during the second patterning step removing the first doped layer in unprotected regions in a self-aligned manner.

### Claim 21 (depends on 18)

The method of claim 18, further comprising forming an adhesion promoting surface on the stressed substrate, wherein depositing the first electrode layer comprises depositing the first electrode layer on the adhesion promoting surface.

### Claim 22 (depends on 21)

The method of claim 21, wherein forming the adhesion promoting surface comprises depositing a layer of silicon oxide, silicon nitride, or silicon oxynitride by plasma-enhanced chemical vapor deposition.

### Claim 23 (depends on 18)

The method of claim 18, wherein the second electrode layer is configured to transmit a trigger stimulus to the active region of the photodiode.

### Claim 24 (depends on 18)

The method of claim 18, wherein depositing the second electrode layer comprises forming an optical filter that substantially attenuates wavelengths of light that are outside a wavelength band of a trigger stimulus and substantially passes wavelengths of light that are within the wavelength band of the trigger stimulus.

### Claim 25 (depends on 18)

The method of claim 18, wherein the stressed substrate includes at least one tensile stress layer having a residual tensile stress and at least one compressive stress layer having a residual compressive stress and being mechanically coupled to the at least one tensile stress layer such that the at least one tensile stress layer and the at least one compressive stress layer are self-equilibrating.

### Claim 26 (depends on 18)

The method of claim 18, wherein the stressed substrate comprises chemically tempered glass.