# US 2019/0172747 A1 · Modulating the microstructure of metallic interconnect structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0172747 A1
- Document ID: US20190172747A1
- Status: Published application
- Kind: A1
- Application number: 16/267,695
- Filed: 2019-02-05
- Published: 2019-06-06
- Earliest claimed: 2017-02-27
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Roger A. Quon; Michael Rizzolo; Chih-Chao Yang
- Web page: https://patentgrep.com/patent/US20190172747A1

## CPC

- H10W 20/059: {by reflowing or applying pressure}
- C23C 14/046: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 14/568: {Transferring the substrates through a series of coating stations (C23C14/562 takes precedence)}
- C23C 14/5806: {Thermal treatment}
- C23C 14/5873: {Removal of material}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C 16/56: After-treatment
- C23C 18/52: using reducing agents for coating with metallic material not provided for in a single one of groups C23C18/32 - C23C18/50
- H10P 72/00: Handling or holding of wafers, substrates or devices during manufacture or treatment thereof
- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Tooling apparatus and methods are provided to fabricate semiconductor devices in which controlled thermal annealing techniques are utilized to modulate microstructures of metallic interconnect structures. For example, an apparatus includes a single platform semiconductor processing chamber having first and second sub-chambers. The first sub-chamber is configured to receive a semiconductor substrate comprising a metallization layer formed on a dielectric layer, wherein a portion of the metallization layer is disposed within an opening etched in the dielectric layer, and to form a stress control layer on the metallization layer. The second sub-chamber comprises a programmable hot plate which is configured to perform a thermal anneal process to modulate a microstructure of the metallization layer while the stress control layer is disposed on the metallization layer, and without an air break between the process modules of forming the stress control layer and performing the thermal anneal process.

## Claims

### Claim 1

A method, comprising:
forming a dielectric layer on a substrate;
patterning the dielectric layer to form an opening in the dielectric layer;
depositing a layer of metallic material on the dielectric layer to fill the opening with metallic material;
forming a stress control layer on the layer of metallic material; and
performing a thermal anneal process to modulate a microstructure of the deposited layer of metallic material from a first microstructure to a second microstructure while the stress control layer is disposed on the layer of metallic material;
wherein the thermal anneal process is performed using a programmable hot plate which is programmed to perform a controlled thermal anneal cycle with active heating and active cooling periods; and
wherein the thermal anneal process is performed without an air break between the steps of forming the stress control layer and performing the thermal anneal process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle is performed over a period of time ranging from about 30 seconds to about 5 hours.

### Claim 3 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle is performed over a temperature setting of the programmable hot plate from about 0 degrees Celsius to about 800 degrees Celsius.

### Claim 4 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle comprises at least one ramp-up heating period in which a temperature setting of the programmable hot plate increases at a rate of about 10 degrees Celsius per minute, or greater.

### Claim 5 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle comprises at least one ramp-down cooling period in which a temperature setting of the programmable hot plate decreases at a rate of about 2 degrees Celsius per minute or greater.

### Claim 6 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle comprises at least one soaking period in which a temperature setting of the programmable hot plate is maintained constant for a period of time at a temperature level which is below a critical temperature of the layer of metallic material at which stress relaxation of the metallic material occurs during a heating period of the controlled thermal anneal cycle.

### Claim 7 (depends on 1)

The method of claim 1, wherein the controlled thermal anneal cycle is performed in a gas atmosphere which comprises at least one of nitrogen, hydrogen, and helium.

### Claim 8 (depends on 1)

The method of claim 1, wherein the stress control layer comprises at least one of tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, cobalt, cobalt tungsten phosphide, ruthenium, ruthenium nitride, ruthenium, ruthenium nitride, iridium, rhodium, manganese, nickel, and alloys of such materials.

### Claim 9 (depends on 1)

The method of claim 1, wherein the layer of metallic material comprises at least one of copper, aluminum, tungsten, cobalt, ruthenium, iridium, rhodium, nickel, and alloys of such materials.

### Claim 10 (depends on 1)

The method of claim 1, comprising performing a wet deposition process to form the stress control layer on the layer of metallic material.

### Claim 11 (depends on 1)

The method of claim 1, comprising performing a dry deposition process to form the stress control layer on the layer of metallic material.

### Claim 12 (depends on 1)

The method of claim 1, further comprising performing a furnace thermal anneal process to reflow the layer of metallic material prior to forming the stress control layer on the reflowed layer of metallic material.

### Claim 13 (depends on 1)

The method of claim 1, wherein the first microstructure comprises a polycrystalline microstructure and wherein the second microstructure comprises an average grain size which is greater than an average grain size of the polycrystalline microstructure.

### Claim 14 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises an interlevel dielectric layer of a back-end-of-line structure formed on the semiconductor substrate.

### Claim 15

A method, comprising:
forming wafer comprising a dielectric layer formed on an upper surface of a wafer substrate, wherein the dielectric layer comprises an opening etched in a surface of the dielectric layer;
inputting the wafer into a single platform semiconductor processing chamber which is configured to process the wafer, the single platform semiconductor processing chamber comprising a first sub-chamber, a second sub-chamber, and a third sub-chamber;
depositing a layer of metallic material to fill the opening and cover the surface of the dielectric layer with the metallic material, in the first sub-chamber;
depositing a stress control layer on the layer of metallic material, in the second sub-chamber; and
performing a thermal anneal process in the third sub-chamber using a programmable hot plate to modulate a microstructure of the layer of metallic material from a first microstructure to a second microstructure while the stress control layer is disposed on the layer of metallic material, wherein the programmable hot plate is programmed to perform a controlled thermal anneal cycle with active heating and active cooling stages;
wherein the thermal anneal process is performed without an air break between the steps of depositing the stress control layer and performing the thermal anneal process.

### Claim 16 (depends on 15)

The method of claim 15, further comprising performing a furnace thermal anneal process in a fourth sub-chamber of the single platform semiconductor processing chamber, wherein the furnace thermal anneal process is performed to reflow the layer of metallic material prior to depositing the stress control layer on the reflowed layer of metallic material in the second sub-chamber.

### Claim 17 (depends on 15)

The method of claim 15, wherein the controlled thermal anneal cycle is performed over a period of time ranging from about 30 seconds to about 5 hours.

### Claim 18 (depends on 15)

The method of claim 15, wherein the controlled thermal anneal cycle is performed over a temperature setting of the programmable hot plate from about 0 degrees Celsius to about 800 degrees Celsius.

### Claim 19 (depends on 15)

The method of claim 15, wherein the controlled thermal anneal cycle comprises:
at least one ramp-up heating period in which a temperature setting of the programmable hot plate increases at a rate of about 10 degrees Celsius per minute, or greater;
at least one ramp-down cooling period in which a temperature setting of the programmable hot plate decreases at a rate of about 2 degrees Celsius per minute, or greater; and
at least one soaking period in which a temperature setting of the programmable hot plate is maintained constant for a period of time at a temperature level which is below a critical temperature of the layer of metallic material at which stress relaxation of the metallic material occurs during a heating period of the controlled thermal anneal cycle.

### Claim 20 (depends on 15)

The method of claim 15, wherein:
the stress control layer comprises at least one of tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, cobalt, cobalt tungsten phosphide, ruthenium, ruthenium nitride, ruthenium, ruthenium nitride, iridium, rhodium, manganese, nickel, and alloys of such materials; and