# US 2019/0172715 A1 · Manufacturing method of a semiconductor device with efficient edge structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0172715 A1
- Document ID: US20190172715A1
- Status: Published application
- Kind: A1
- Application number: 16/209,680
- Filed: 2018-12-04
- Published: 2019-06-06
- Earliest claimed: 2017-12-05
- Assignees: STMicroelectronics S.r.l.
- Applicants: Stmicroelectronics S.R.L.
- Inventors: Edoardo ZANETTI; Simone RASCUNÁ; Mario Giuseppe SAGGIO; Alfio GUARNERA; Leonardo FRAGAPANE; Cristina TRINGALI
- Web page: https://patentgrep.com/patent/US20190172715A1

## CPC

- H10P 30/21: {of electrically active species}
- H10D 8/051: {of Schottky diodes}
- H10D 8/60: Schottky-barrier diodes
- H10D 8/605: {of the trench conductor-insulator-semiconductor barrier type, e.g. trench MOS barrier Schottky rectifiers [TMBS]}
- H10D 12/031: {of IGBTs}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 30/665: {having edge termination structures}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/104: {having particular shapes of the bodies at or near reverse-biased junctions, e.g. having bevels or moats}
- H10D 62/106: {having supplementary regions doped oppositely to or in rectifying contact with regions of the semiconductor bodies, e.g. guard rings with PN or Schottky junctions}
- H10D 62/8325: {Silicon carbide}
- H10D 64/0121: {to Group IV semiconductors}
- H10D 64/0123: {to silicon carbide}
- H10P 30/2042: {into crystalline silicon carbide}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A manufacturing method of an electronic device includes: forming a drift layer of an N type; forming a trench in the drift layer; forming an edge-termination structure alongside the trench by implanting dopant species of a P type; and forming a depression region between the trench and the edge-termination structure by digging the drift layer. The steps of forming the depression region and the trench are carried out at the same time. The step of forming the depression region comprises patterning the drift layer to form a structural connection with the edge-termination structure having a first slope, and the step of forming the trench comprises etching the drift layer to define side walls of the trench, which have a second slope steeper than the first slope.

## Claims

### Claim 1

A manufacturing method of an electronic device, comprising:
forming a drift layer having a top surface and a first conductivity;
forming a trench in the drift layer by etching the drift layer starting from the top surface;
forming an edge-termination structure laterally to said trench by implanting dopant species which have a second conductivity different from the first conductivity; and
forming a depression region between said trench and said edge-termination structure by etching the drift layer starting from the top surface, wherein:
forming the depression region and forming the trench are carried out at the same time,
forming the depression region comprises patterning the drift layer to have a first slope, and
forming the trench comprises etching the drift layer to define side walls of the trench which have a second slope steeper than the first slope.

### Claim 2 (depends on 1)

The method according to claim 1, wherein forming at the same time the depression region and the trench comprises:
forming a first etching mask having a first opening and a second opening;
forming a second etching mask that extends into a first portion of the second opening of the first etching mask and leaves uncovered a first portion of the drift region that was exposed by the second opening, said second etching mask having a ramp with a thickness that decreases according to the first slope; and
carrying out an etching that forms the recess by removing a second portion of the drift layer exposed through the first opening and forms the depression region by removing the first portion of the drift region, removing at least a portion of the ramp of the second etching mask, and removes a third portion of the drift region that was uncovered by removing the at least a portion of the ramp.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the first etching mask is made of TEOS and the second etching mask is made of photoresist.

### Claim 4 (depends on 2)

The method according to claim 2, wherein carrying out the etching includes etching using an inductively coupled plasma.

### Claim 5 (depends on 4)

The method according to claim 4, wherein said etching is carried out using O2/SF6/HBr, a pressure of 10-15 mTorr in the etching chamber, a plasma source having a power between 600 W and 800 W, and a bias power between 70 W and 150 W.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said first slope is comprised between 10° and 60° and said second slope is comprised between 80° and 90°.

### Claim 7 (depends on 1)

The method according to claim 1, further comprising implanting dopant species, which have the second conductivity, in the drift region at a bottom of the trench.

### Claim 8 (depends on 7)

The method according to claim 7, wherein implanting dopant species includes implanting the dopant species in the depression region and in a portion of the drift layer between the depression region and the edge termination structure, thereby forming an implanted anode region that contacts the edge termination structure.

### Claim 9 (depends on 7)

The method according to claim 7, further comprising, prior to the implanting step, forming a hard mask on top of the top surface, the hard mask having an opening defined by side walls of the hard mask, wherein forming the trench includes etching the drift layer through the opening in the hard mask and the implanting step includes defining one or more surface regions of the drift layer, which have the first type of conductivity.

### Claim 10 (depends on 9)

The method according to claim 9, further comprising forming a metal layer in direct contact with said one or more surface regions of the drift layer, thus forming one or more Schottky junctions.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the drift layer is made of silicon carbide.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the first conductivity is of an N type and the second conductivity is of a P type.

### Claim 13 (depends on 1)

The method according to claim 1, wherein said electronic device is a power diode, the method further including:
forming an anode contact at said top surface of the drift layer; and
forming a cathode contact below the drift layer.

### Claim 14

A method, comprising:
forming a mask on a top surface of a semiconductor body, the mask including a first opening defined by first side walls having a first slope and a second opening defined by second sidewalls with one of the second side walls being a ramp having a second slope that is less than the first slope;
forming a trench in the semiconductor body by etching the semiconductor body through the first opening; and
forming a depression region in the semiconductor body by etching the semiconductor body through the second opening, etching at least a portion of the ramp, and etching a portion of the semiconductor body that was exposed by etching the at least a portion of the ramp, wherein forming the depression region and forming the trench are carried concurrently.

### Claim 15 (depends on 14)

The method according to claim 14, further comprising:
forming an edge-termination structure laterally to said trench by implanting dopant species which have a second conductivity different from the first conductivity; and
implanting further dopant species in the depression region and in a portion of the semiconductor body between the depression region and the edge termination structure, thereby forming an implanted anode region that contacts the edge termination structure.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the mask includes a first mask layer that defines the first opening and a second mask layer that includes the ramp.

### Claim 17 (depends on 14)

The method according to claim 14, wherein said electronic device is a power diode, the method further including:
forming an anode contact at said top surface of the semiconductor body; and
forming a cathode contact at a bottom surface of the semiconductor body.

### Claim 18

A method of making a Junction-Barrier Schottky (JBS) diode, comprising:
forming a trench in a semiconductor body having top and bottom surfaces and a first conductivity, forming the trench including etching the semiconductor body starting from the top surface, the trench being defined by side walls of the semiconductor body that have a first slope;
forming an edge-termination structure laterally to said trench by implanting dopant species which have a second conductivity different from the first conductivity;
forming a depression region between said trench and said edge-termination structure by etching the drift layer starting from the top surface concurrently with forming the trench, the depression region comprises patterning the drift layer to have a second slope that is less than the first slope;
implanting dopant species, which have the second conductivity, in the semiconductor body at a bottom of the trench to form one or more first surface regions of the second conductivity between plural second surface regions of the semiconductor body, which have the first type of conductivity;
forming an anode contact at the top surface of the semiconductor body, the anode contact contacting the first and second surface regions; and
forming a cathode contact at the bottom surface of the semiconductor body.

### Claim 19 (depends on 18)

The method according to claim 18, further comprising:
forming a first etching mask having a first opening and a second opening;
forming a second etching mask that extends into a first portion of the second opening of the first etching mask and leaves uncovered a first portion of the semiconductor body that was exposed by the second opening, said second etching mask having a ramp with a thickness that decreases according to the first slope; and
carrying out an etching that forms the recess by removing a second portion of the drift layer exposed through the first opening and forms the depression region by removing the first portion of the drift region, removing at least a portion of the ramp of the second etching mask, and removes a third portion of the semiconductor body that was uncovered by removing the at least a portion of the ramp.

### Claim 20 (depends on 18)

The method according to claim 18, wherein said first slope is comprised between 10° and 60° and said second slope is comprised between 80° and 90°.