# US 2019/0170419 A1 · Method for manufacturing an ice projectile

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0170419 A1
- Document ID: US20190170419A1
- Status: Published application
- Kind: A1
- Application number: 16/321,245
- Filed: 2017-06-09
- Published: 2019-06-06
- Earliest claimed: 2016-07-29
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Frédérik GUYON
- Web page: https://patentgrep.com/patent/US20190170419A1

## CPC

- F25C 1/00: Producing ice (F25C3/00 takes precedence)
- B24C 1/003: {using material which dissolves or changes phase after the treatment, e.g. ice, CO2}
- F01D 21/045: {special arrangements in stators or in rotors dealing with breaking-off of part of rotor}
- F02C 7/05: having provisions for obviating the penetration of damaging objects or particles
- F05D 2260/12: Testing on a test bench
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- F25C: PRODUCING, WORKING OR HANDLING ICE
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F02C: GAS-TURBINE PLANTS; AIR INTAKES FOR JET-PROPULSION PLANTS; CONTROLLING FUEL SUPPLY IN AIR-BREATHING JET-PROPULSION PLANTS (construction of turbines F01D; jet-propulsion plants F02K; construction of compressors or fans F04; generating combustion products of high pressure or high velocity F23R; using gas turbines in compression refrigeration plants F25B11/00)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The invention relates to a method for producing an ice projectile. The method comprises the steps of: providing a quantity of water; providing a quantity of alcohol corresponding to at least 5 wt.-% of the quantity of water; mixing the quantity of water with the quantity of alcohol; transferring the mixture to means for cooling and solidifying the mixture to form a piece of ice; cooling the mixture in the cooling and solidifying means to a mixture-solidification temperature in order to produce at least one piece of ice; and launching the or each piece of ice at a target using launching means.

## Claims

### Claim 1

A method for manufacturing and using an ice projectile wherein it comprises the steps of:
providing an amount of water;
providing an amount of alcohol corresponding to at least 5 weight % of the amount of water;
mixing the amount of water and the amount of alcohol;
transferring the mixture to means for cooling and solidifying the mixture into a block of ice;
cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice,
projecting the, or each, block of ice on a target, by projection means.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice, has a transition temperature range in which the mixture has an aqueous phase composed of solid crystals mainly composed of water, the solid crystals being surrounded by a liquid solution mainly composed of alcohol.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed at a rate higher than or equal to 0.5 K per second.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed at a rate lower than or equal to 0.5 K per second.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed by stirring the mixture to maintain the homogeneity thereof.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the step of projecting the, or each, block of ice is carried out at a temperature comprised between 60K and 250K.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the cooling and solidifying means comprise at least one mold for shaping at least one block of ice.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the cooling and solidifying means comprise at least one tube allowing cooling and shaping at least one block of ice.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the, or each, tube is connected to projection means allowing projecting the, or each, block of ice positioned in the corresponding tube.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the cooling and solidifying means comprise at least one cryostat.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the alcohol belongs to the group comprising ethanol, methanol, butanol and propanol.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the amount of alcohol is provided by an alcoholic solution having a purity higher than or equal to 90%.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the water is provided by an aqueous solution taken from distilled water and demineralized water.

### Claim 14 (depends on 2)

The method according to claim 2, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed at a rate higher than or equal to 0.5 K per second.

### Claim 15 (depends on 2)

The method according to claim 2, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed at a rate lower than or equal to 0.5 K per second.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the step of cooling the mixture in the means for cooling and solidifying the mixture into a block of ice, down to a solidification temperature of the mixture, in order to obtain at least one block of ice is performed by stirring the mixture to maintain the homogeneity thereof.

### Claim 17 (depends on 2)

The method according to claim 2, wherein the step of projecting the, or each, block of ice is carried out at a temperature comprised between 60K and 250K.

### Claim 18 (depends on 3)

The method according to claim 3, wherein the step of projecting the, or each, block of ice is carried out at a temperature comprised between 60K and 250K.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the cooling and solidifying means comprise at least one mold for shaping at least one block of ice.

### Claim 20 (depends on 3)

The method according to claim 3, wherein the cooling and solidifying means comprise at least one mold for shaping at least one block of ice.