# US 2019/0169499 A1 · Method For Controlling Gallium Content in Gadolinium-Gallium Garnet Scintillators

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0169499 A1
- Document ID: US20190169499A1
- Status: Published application
- Kind: A1
- Application number: 16/266,457
- Filed: 2019-02-04
- Published: 2019-06-06
- Earliest claimed: 2015-12-01
- Assignees: Siemens Medical Solutions USA, Inc.
- Applicants: Siemens Medical Solutions USA, Inc.
- Inventors: Peter Carl Cohen; Alexander Andrew Carey; Mark S. Andreaco
- Web page: https://patentgrep.com/patent/US20190169499A1

## CPC

- C09K 11/7701: {Chalogenides}
- C09K 11/7774: {Aluminates}
- C09K 11/7769: {Oxides (C09K11/7768 takes precedence)}
- G01T 1/2023: {Selection of materials}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)

## Abstract

Disclosed herein is a method including manufacturing a powder having a composition of formula (1), M1aM2bM3cM4dO12 (1) where O represents oxygen, M1, M2, M3, and M4 represents a first, second, third, and fourth metal that are different from each other, where the sum of a+b+c+d is about 8, where “a” has a value of about 2 to about 3.5, “b” has a value of 0 to about 5, “c” has a value of 0 to about 5 “d” has a value of 0 to about 1, where “b” and “c”, “b” and “d”, or “c” and “d” cannot both be equal to zero simultaneously, where M1 is a rare earth element comprising gadolinium, yttrium, lutetium, scandium, or a combination of thereof, M2 is aluminum or boron, M3 is gallium, and M4 is a dopant; and heating the powder to a temperature of 500 to 1700° C. in an oxygen containing atmosphere to manufacture a crystalline scintillator.

## Claims

### Claim 1

A method comprising:
blending together nanometer and/or micrometer-sized particles that comprise M1, M2, M3 and M4 to produce a powder having a composition that comprises the formula (1):
M1aM2bM3cM4dO12 (1)
where
O represents oxygen,
M1, M2, M3, and M4 represent a first, second, third, and fourth metal that are different from each other,
the sum of a+b+c+d is about 8, where
“a” has a value of about 2 to about 3.5,
“b” has a value of 2 to about 5,
“c” has a value of 1 to about 5, and
“d” has a value of 0.001 to about 1, where “b” and “c”, “b” and “d”, or “c” and “d” cannot both be equal to zero simultaneously,
M1 is a rare earth element comprising gadolinium, yttrium, lutetium, scandium, or a combination of thereof,
M2 is aluminum or boron,
M3 is gallium, and
M4 is a dopant and comprises one of thallium, copper, silver, lead, bismuth, indium, tin, antimony, tantalum, tungsten, strontium, barium, boron, magnesium, calcium, cerium, yttrium, scandium, lanthanum, lutetium, praseodymium, terbium, ytterbium, samarium, europium, holmium, dysprosium, erbium, thulium or neodymium; and
heating the powder to a temperature of 800 to 1700° C. in an oxygen containing atmosphere to manufacture a crystalline scintillator.

### Claim 2 (depends on 1)

The method of claim 1, where for M1, a portion of the gadolinium can be substituted with one or more of yttrium, lutetium, lanthanum, terbium, praseodymium, neodymium, cerium, samarium, europium, dysprosium, holmium, erbium, ytterbium, or combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, where M2 is aluminum.

### Claim 4 (depends on 1)

The method of claim 1, where “a” has a value about 2.4 to about 3.2, “b” has a value of about 2 to about 3, “c” has a value of about 1 to about 4, and “d” has a value of about 0.001 to about 0.5.

### Claim 5 (depends on 4)

The method of claim 4, where “a” has a value of about 3, “b” has a value of about 2.1 to about 2.5, “c” has a value of about 2 to about 3, and “d” has a value of about 0.003 to about 0.3.

### Claim 6 (depends on 1)

The method of claim 1, further comprising heating the powder to a temperature of 500 to 2000° C. to melt the powder.

### Claim 7 (depends on 6)

The method of claim 6, where the heating of the powder to a temperature of 500 to 2000° C. to melt the powder is conducted prior to the heating of the powder to a temperature of 800 to 1700° C. in an oxygen containing atmosphere to manufacture the crystalline scintillator.

### Claim 8 (depends on 1)

The method of claim 1, where the blending is conducted in a ball mill or a roll mill.

### Claim 9 (depends on 1)

The method of claim 1, where the powder has average particle sizes of 5 nanometers to 500 micrometers.

### Claim 10 (depends on 1)

The method of claim 1, where the crystalline scintillator comprises a single crystal, a polycrystalline material or a combination thereof.

### Claim 11 (depends on 10)

The method of claim 10, where the single crystal is produced by the Czochralski method, the Bridgman technique, the Kyropoulos technique, or the Verneuil technique.

### Claim 12

An article manufactured by a method comprising:
manufacturing a powder having a composition of formula (1),
M1aM2bM3cM4dO12 (1)
where
O represents oxygen,
M1, M2, M3, and M4 represents a first, second, third, and fourth metal that are different from each other,
the sum of a+b+c+d is about 8, where
“a” has a value of about 2 to about 3.5,
“b” has a value of 0 to about 5,
“c” has a value of 0 to about 5, and
“d” has a value of 0 to about 1, where “b” and “c”, “b” and “d”, or “c” and “d” cannot both be equal to zero simultaneously,
M1 is a rare earth element comprising gadolinium, yttrium, lutetium, scandium, or a combination of thereof,
M2 is aluminum or boron,
M3 is gallium, and
M4 is a dopant and comprises one of thallium, copper, silver, lead, bismuth, indium, tin, antimony, tantalum, tungsten, strontium, barium, boron, magnesium, calcium, cerium, yttrium, scandium, lanthanum, lutetium, praseodymium, terbium, ytterbium, samarium, europium, holmium, dysprosium, erbium, thulium or neodymium; and
heating the powder to a temperature of 500 to 1700° C. in an oxygen containing atmosphere to manufacture a crystalline scintillator.

### Claim 13 (depends on 12)

The article of claim 12, where the article is an imaging device.