Methods of Generating Recombinant Spider Silk Protein Fibers
OwnerMaxime Boulet-Audet, Gregory Wilson Rice +5inventors
InventorsMaxime Boulet-Audet, Gregory Wilson Rice, Krystle Marie Moody, Jamie McAusland Bainbridge, Steven Tom, Amir Ahmad Bakhtiary Davijani, Lindsay Wray
Life of this patent
Estimating the term…
Abstract
Provided herein are scalable methods of generating a recombinant silk polypeptide with a coefficient of friction sufficient to form mechanical interactions with other fibers.
Claims37
A plurality of fibers comprising recombinant spider silk polypeptide, wherein the plurality of fibers are generated by:
- dissolving a powder comprising a recombinant spider silk polypeptide into a solvent to generate a spin dope;
- extruding the spin dope into a coagulation bath to form a plurality of precursor fibers;
- and
- subjecting the plurality of precursor fibers to a turbulent air source, thereby generating the plurality of fibers comprising recombinant spider silk polypeptide,
- wherein one or more of the plurality of fibers has a mean coefficient of friction that is greater than 0.60.
A recombinant fiber comprising a recombinant polypeptide, wherein said fiber comprises a mean coefficient of friction of greater than 0.60.
A knitted garment comprising a staple yarn, wherein said staple yarn comprises wool and a plurality of recombinant fibers divided into discrete lengths, wherein said plurality of recombinant fibers comprise silk-like polypeptides, and wherein said plurality of recombinant fibers comprises a mean coefficient of friction of greater than 0.60.
A method of generating a fiber comprising recombinant spider silk polypeptide, comprising:
- dissolving a powder comprising a recombinant spider silk polypeptide into a solvent to generate a spin dope;
- extruding the spin dope into a coagulation bath to form a precursor fiber;
- and
- subjecting the precursor fiber to a turbulent air source, thereby generating the fiber comprising recombinant spider silk polypeptide,
- wherein the fiber comprising recombinant spider silk polypeptide has a mean coefficient of friction that is greater than 0.60.