# US 2019/0164835 A1 · Semiconductor device structure and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0164835 A1
- Document ID: US20190164835A1
- Status: Published application
- Kind: A1
- Application number: 15/821,969
- Filed: 2017-11-24
- Published: 2019-05-30
- Earliest claimed: 2017-11-24
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Wei-Hao LU; Yi-Fang PAI; Tuoh-Bin NG; Li-Li SU; Chii-Horng LI
- Web page: https://patentgrep.com/patent/US20190164835A1

## CPC

- H10D 84/013: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 30/6212: {having fin-shaped semiconductor bodies having non-rectangular cross-sections}
- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/405: {Orientations of crystalline planes}
- H10D 62/834: further characterised by the dopants
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 84/0149: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/8311: {the IGFETs characterised by having different channel structures}
- H10D 84/834: {comprising FinFETs}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3441: {Conductivity type}
- H10P 14/3466: {Crystal orientation}
- H10W 20/20: Interconnections within wafers or substrates, e.g. through-silicon vias [TSV]
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Structures and formation methods of a semiconductor device structure are provided. The semiconductor device structure includes a first fin structure and a second fin structure over a substrate. The semiconductor device structure also includes a gate structure over the first and second fin structure. The semiconductor device structure further includes a source/drain structure over the first and second fin structure. The source/drain structure includes a first semiconductor layer over the first fin structure and a second semiconductor layer over the second fin structure. The source/drain structure also includes a third semiconductor layer covering the first and second semiconductor layers. The third semiconductor layer has a surface with [110] plane orientation.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A method for fabricating a semiconductor device structure, comprising:
forming a first fin structure over a substrate;
forming an isolation feature over the substrate;
forming a gate structure over the first fin structure and the isolation feature;
recessing a portion of the first fin structure that is not directly below the gate structure to form a first recess extending into a portion of the isolation feature that is not directly below the gate structure; and
epitaxially growing a first semiconductor layer in the first recess of the first fin structure at a first temperature in a range of about 400° C. to about 700° C. so that the first semiconductor layer has a surface with [110] plane orientation, wherein the first semiconductor layer has a first dopant concentration of P.

### Claim 17 (depends on 16)

The method as claimed in claim 16, further comprising:
epitaxially growing a second semiconductor layer covering the first semiconductor layer at the first temperature so that the second semiconductor layer has a surface with [110] plane orientation, wherein the second semiconductor layer has a second dopant concentration of P that is greater than the first dopant concentration of P.

### Claim 18 (depends on 17)

The method as claimed in claim 17, further comprising:
forming a second fin structure adjacent to the first fin structure;
recessing the second fin structure to form a second recess adjacent to the gate structure; and
epitaxially growing a third semiconductor layer in the second recess of the second fin structure at the first temperature so that the third semiconductor layer has a surface with [110] plane orientation, wherein the third semiconductor layer has the first dopant concentration of P, the second semiconductor layer has a recess formed between the first semiconductor layer and the third semiconductor layer, and a bottom of the recess is lower than a top surface of the first semiconductor layer.

### Claim 19 (depends on 18)

The method as claimed in claim 18, further comprising:
depositing a dielectric layer over the third semiconductor layer;
etching the dielectric layer and a portion of the third semiconductor layer to form a trench, wherein a bottom of the trench is lower than the top surface of the first semiconductor layer; and
forming a contact to fill the trench.

### Claim 20 (depends on 18)

The method as claimed in claim 18, wherein the first semiconductor layer is separated from the third semiconductor layer by the second semiconductor layer, and wherein the surface of the first semiconductor layer with [110] plane orientation and the surface of the third semiconductor layer with [110] plane orientation face toward each other.

### Claim 21

A method for fabricating a semiconductor device structure, comprising:
forming a first fin structure over a substrate;
forming an isolation feature over the substrate, wherein the first fin structure has a first height over the isolation feature;
forming a gate structure over the first fin structure;
recessing the first fin structure to form a first recess adjacent to the gate structure;
epitaxially growing a first semiconductor layer in the first recess of the first fin structure so that the first semiconductor layer has a surface with [110] plane orientation, wherein the surface of the first semiconductor layer has a first length perpendicular to a top surface of the substrate;
epitaxially growing a second semiconductor layer covering the first semiconductor layer so that the second semiconductor layer has a surface with [110] plane orientation,
forming a capping layer over the second semiconductor layer;
forming a dielectric layer over the capping layer; and
etching the dielectric layer, the capping layer and a portion of the second semiconductor layer to form a trench, wherein a bottommost portion of the trench is lower than a top surface of the first semiconductor layer.

### Claim 22 (depends on 21)

The method as claimed in claim 21, wherein the surface of the second semiconductor layer has a second length perpendicular to the top surface of the substrate, and wherein a ratio of the first length to the first height is in a range from about 40% to about 70%, and a ratio of the second length to the first height is in a range from about 50% to about 80%.

### Claim 23 (depends on 21)

The method as claimed in claim 21, further comprising:
forming a second fin structure over the substrate, wherein the second fin structure has a second height over the isolation feature, and a portion of the second fin structure is covered by the gate structure;
recessing the second fin structure to form a second recess adjacent to the gate structure;
epitaxially growing a third semiconductor layer in the second recess of the second fin structure at a temperature in a range from about 400° C. to about 700° C. so that the third semiconductor layer has a surface with [110] plane orientation, wherein the surface of the second semiconductor layer has a third length perpendicular to the top surface of the substrate, and a ratio of the third length to the second height is in a range from about 40% to about 70%, and
wherein the third semiconductor layer is covered by the second semiconductor layer.

### Claim 24 (depends on 21)

The method as claimed in claim 21, wherein the first semiconductor layer has a first dopant concentration of P, and the second semiconductor layer has a second dopant concentration of P that is greater than the first dopant concentration of P.

### Claim 25 (depends on 24)

The method as claimed in claim 24, wherein the growth process of the first semiconductor layer comprises:
applying PH3, wherein a flow rate of PH3 is in a range from about 100 sccm to about 400 sccm, and
wherein the first semiconductor layer and the second semiconductor layer are grown at a temperature in a range from about 400° C. to about 700° C.

### Claim 26 (depends on 24)

The method as claimed in claim 24, wherein the first dopant concentration of P is in a range from about 1×1020/cm3 to 5×1021/cm3.

### Claim 27

(canceled)

### Claim 28 (depends on 21)

The method as claimed in claim 21, further comprising:
forming a silicide layer on a top surface of the second semiconductor layer exposed by the trench, wherein a bottom surface of the silicide layer is lower than the top surface of the first semiconductor layer; and
forming a contact over the silicide layer, wherein the contact has a V-shaped profile.

### Claim 29

A method for fabricating a semiconductor device structure, comprising:
forming a first fin structure and a second fin structure over a substrate;
forming an isolation feature over the substrate, wherein the first fin structure has a first height over the isolation feature, and the second fin structure has a second height over the isolation feature;
forming a gate structure over the first fin structure and the second fin structure;
recessing the first fin structure and the second fin structure to form a first recess and a second recess adjacent to the gate structure;
epitaxially growing a first semiconductor layer in the first recess of the first fin structure and a second semiconductor layer in the second recess of the second fin structure, wherein a surface of the first semiconductor layer with [110] plane orientation has a first length perpendicular to a top surface of the substrate, and a surface of the second semiconductor layer with [110] plane orientation has a second length perpendicular to the top surface of the substrate, wherein the surface of the first semiconductor layer with [110] plane orientation and the surface of the second semiconductor layer with [110] plane orientation face toward each other; and
epitaxially growing a third semiconductor layer covering the first semiconductor layer and the second semiconductor layer, wherein the first semiconductor layer and the second semiconductor layer are separated by the third semiconductor layer.

### Claim 30 (depends on 29)

The method as claimed in claim 29, wherein a first ratio of the first length to the first height and a second ratio of the second length to the second height are in a range from about 40% to about 70%.

### Claim 31 (depends on 29)

The method as claimed in claim 29, wherein the first semiconductor layer and the second semiconductor layer have a first dopant concentration of a dopant, the third semiconductor layer has a second dopant concentration of the dopant that is greater than the first dopant concentration of the dopant, and the dopant comprises P, As, B, Al or Ga.

### Claim 32 (depends on 29)

The method as claimed in claim 29, wherein the growth process of the first semiconductor layer and the second semiconductor layer comprises:
applying a P-containing precursor at a temperature in a range from about 400° C. to about 700° C.

### Claim 33 (depends on 32)

The method as claimed in claim 32, wherein the P-containing precursor comprises PH3, and a flow rate of PH3 is in a range from about 100 sccm to about 400 sccm.

### Claim 34 (depends on 29)

The method as claimed in claim 29, wherein a surface of the third semiconductor layer with [110] plane orientation has a third length perpendicular to the top surface of the substrate, and a ratio of the third length to the first height is in a range from about 50% to about 80%.

### Claim 35 (depends on 29)

The method as claimed in claim 29, further comprising:
forming a dielectric layer over the third semiconductor layer;
etching the dielectric layer and a portion of the third semiconductor layer to form a trench; and
forming a contact to fill the trench, wherein the contact extends between the first semiconductor layer and the second semiconductor layer.

### Claim 36 (depends on 23)

The method as claimed in claim 23, wherein the surface of the first semiconductor layer with [110] plane orientation and the surface of the third semiconductor layer with [110] plane orientation face toward each other.