# US 2019/0157726 A1 · Secondary Cell with High Recharging Efficiency and Long Term Stability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0157726 A1
- Document ID: US20190157726A1
- Status: Published application
- Kind: A1
- Application number: 16/260,511
- Filed: 2019-01-29
- Published: 2019-05-23
- Earliest claimed: 2016-03-14
- Assignees: Urban Electric Power Inc.
- Applicants: Urban Electric Power Inc
- Inventors: Melissa MENARD; David KAPLIN; Ryan CAMMARATA
- Web page: https://patentgrep.com/patent/US20190157726A1

## CPC

- H01M 10/26: Selection of materials as electrolytes
- H01M 4/244: {Zinc electrodes}
- H01M 4/42: Alloys based on zinc
- H01M 4/50: of manganese
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/622: {being polymers}
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 4/74: Meshes or woven material; Expanded metal
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/24: Alkaline accumulators
- H01M 10/28: Construction or manufacture
- H01M 10/286: {Cells or batteries with wound or folded electrodes}
- H01M 50/103: prismatic or rectangular (H01M50/109, H01M50/11 take precedence)
- H01M 2004/023: {Gel electrode}
- H01M 2300/0014: Alkaline electrolytes
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

A secondary zinc-manganese dioxide secondary cell is disclosed. The cell includes a zinc gel anode, high manganese content cathode in either prismatic or jelly roll form. An aqueous based continuous reel to reel process for formulation and fabrication of the anode and cathode is provided. The cell is contained in a box assembly.

## Claims

### Claim 1

An electrochemical cell comprising:
a cathode comprising manganese dioxide;
an anode; and
a separator disposed between the cathode and the anode,
wherein the cathode comprises a paste, where the paste comprises manganese dioxide and a carbon blend, wherein the carbon blend comprises graphite and a carbon based conductive additive, and wherein a ratio of the graphite to the conductive additive is in a range of from about 7:1 to about 28:1.

### Claim 2 (depends on 1)

The electrochemical cell of claim 1, wherein the paste comprises between about 75% and about 85% manganese dioxide by weight.

### Claim 3 (depends on 1)

The electrochemical cell of claim 1, wherein the graphite comprises at least one of expanded graphite or non-expanded graphite.

### Claim 4 (depends on 1)

The electrochemical cell of claim 1, wherein the carbon based conductive additive comprises at least one of carbon black, carbon nanotubes, or carbon nanofibers.

### Claim 5 (depends on 1)

The electrochemical cell of claim 1, wherein at least one of the graphite or the conductive additive comprises particles in the range of from about 20 to about 30 microns.

### Claim 6 (depends on 1)

The electrochemical cell of claim 1, wherein the conductive additive comprises particles having a size in the range of from about 5 to about 15 microns.

### Claim 7 (depends on 1)

The electrochemical cell of claim 1, wherein the manganese dioxide comprises particles having a size in the range of from about 45 microns to about 55 microns.

### Claim 8 (depends on 1)

The electrochemical cell of claim 1, wherein carbon blend is present in the paste in an amount between about 10% and about 20% by weight of the paste.

### Claim 9 (depends on 1)

The electrochemical cell of claim 1, wherein the paste further comprises a binder.

### Claim 10 (depends on 9)

The electrochemical cell of claim 9, wherein the binder comprises at least one of polytetrafluoroethylene (PTFE), polyethylene, carboxymethyl cellulose, polyvinyl alcohol, or latex, and wherein the paste comprises between about 4% and about 7% by weight of the binder.

### Claim 11 (depends on 1)

The electrochemical cell of claim 1, wherein the paste further comprises an additive comprising at least one of MgO, BaTiO3, CaTiO3, BaOH, Bi2O3, TiO2, or TiB2.

### Claim 12 (depends on 12)

The electrochemical cell of claim 12, wherein the paste comprises between less than or equal to about 1% by weight of the additive.

### Claim 13 (depends on 1)

The electrochemical cell of claim 1, wherein the paste has a porosity in the range of from about 25% to about 35%, and wherein the paste has a density of from about 1.5 g/cm3 to about 2.5 g/cm3.

### Claim 14 (depends on 1)

The electrochemical cell of claim 1, wherein the electrochemical cell has a volumetric energy density of at least about 40 Wh/L per cycle.

### Claim 15

A method comprising:
forming a gel comprising zinc, a binder, and water, wherein the binder comprises a polymer;
coating a current collector with the gel; and
drying the gel on the current collector to form a dried anode.

### Claim 16 (depends on 15)

The method of claim 15, further comprising:
pressing the dried anode to form an anode having a predetermined thickness, wherein the anode is formed as a sheet.

### Claim 17 (depends on 15)

The method of claim 15, wherein the gel comprises a zinc content of 75% or greater by weight of the gel.

### Claim 18 (depends on 15)

The method of claim 15, wherein the gel comprises between about 10% and about 25% water.

### Claim 19 (depends on 15)

The method of claim 15, wherein the dried anode comprises a zinc content of between 85% to 95% by weight.

### Claim 20 (depends on 15)

The method of claim 15, wherein the polymer comprises a homopolymer, and wherein the homopolymer comprises polytetrafluoroethene, carboxymethyl cellulose, polyvinylalcohol, Carbapol®, polyethylene glycol, or any combination thereof.

### Claim 21 (depends on 15)

The method of claim 15, wherein the gel further comprises an additive comprising at least one of zinc oxide, carbon powder, indium compounds, bismuth compounds, lithiated and fibrous compounds, or any combination thereof.

### Claim 22 (depends on 15)

The method of claim 15, wherein the electrical current collector comprises at least one of expanded metal, wire screen, perforated metal, or any combination thereof.

### Claim 23 (depends on 15)

The method of claim 15, wherein the current collector is formed from nickel, nickel plated metal, cold-rolled steel, or any combination thereof.

### Claim 24 (depends on 15)

The method of claim 15, further comprising:
forming a cell comprising the anode, a cathode, and a separator disposed between the anode and the cathode, wherein the separator comprises 1 to 4 layers of cellulose-based sheet, polyethylene-based sheet, polyvinyl alcohol-based sheet, polyvinyl chloride-based sheet, or nonwoven polypropylene sheets, or any combination thereof.