# US 2019/0157547 A1 · Method and system for providing a boron-free magnetic layer in perpendicular magnetic junctions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0157547 A1
- Document ID: US20190157547A1
- Status: Published application
- Kind: A1
- Application number: 15/890,101
- Filed: 2018-02-06
- Published: 2019-05-23
- Earliest claimed: 2017-11-20
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., LTD.
- Inventors: Ikhtiar; Xueti Tang; Mohamad Towfik Krounbi
- Web page: https://patentgrep.com/patent/US20190157547A1

## CPC

- H10N 50/01: Manufacture or treatment
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H01F 10/10: characterised by the composition
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 41/14: for applying magnetic films to substrates
- H01F 41/303: {with exchange coupling adjustment of magnetic film pairs, e.g. interface modifications by reduction, oxidation}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/10: Magnetoresistive devices
- H01F 10/1936: {Half-metallic, e.g. epitaxial CrO2 or NiMnSb films}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A magnetic junction and method for providing the magnetic junction are described. The method includes providing a pinned layer, a nonmagnetic spacer layer and a free layer switchable between stable magnetic states. The nonmagnetic spacer layer is between the pinned and free layers. Providing the pinned layer and/or providing the free layer includes cooling a portion of the magnetic junction, depositing a wetting layer while the portion of the magnetic junction is cooled, oxidizing/nitriding the wetting layer and depositing a boron-free magnetic layer on the oxide/nitride wetting layer. The portion of the magnetic junction is cooled to within a temperature range including temperature(s) not greater than 250 K. The wetting layer has a thickness of at least 0.25 and not more than three monolayers. The wetting layer includes at least one magnetic material. The boron-free magnetic layer has a perpendicular magnetic anisotropy energy greater than an out-of-plane demagnetization energy.

## Claims

### Claim 1

A method for providing magnetic junction residing on a substrate and usable in a magnetic device, the method comprising:
providing a pinned layer, the pinned layer being magnetic;
providing a nonmagnetic spacer layer; and
providing a free layer, the nonmagnetic spacer layer being between the pinned layer and the free layer, the free layer being magnetic and switchable between a plurality of stable magnetic states, wherein at least one of the step of providing the pinned layer and the step of providing the free layer further include
cooling a portion of the magnetic junction to within a temperature range including at least one temperature not greater than 250 K;
depositing a wetting layer while the portion of the magnetic junction is cooled, the wetting layer having a thickness of not more than three monolayers and at least 0.25 monolayer, the wetting layer including at least one magnetic material;
at least one of oxidizing and nitriding the wetting layer to provide a treated wetting layer, the treated wetting layer being an oxide wetting layer for an oxidizing process and a nitride wetting layer for a nitriding process; and
depositing a boron-free magnetic layer on the treated wetting layer while at least the oxide wetting layer for the oxidizing process and the nitride wetting layer for the nitriding process is within the temperature range, the boron-free magnetic layer having a perpendicular magnetic anisotropy energy greater than an out-of-plane demagnetization energy.

### Claim 2 (depends on 1)

The method of claim 1 wherein the temperature range is at least 50K and not greater than 150K.

### Claim 3 (depends on 2)

The method of claim 2 wherein the temperature range is at least 70K and not greater than 100K.

### Claim 4 (depends on 1)

The method of claim 1 wherein the wetting layer has a thickness of at least 0.5 monolayer and not more than two monolayers.

### Claim 5 (depends on 2)

The method of claim 2 wherein the wetting layer has a thickness of at least 0.75 monolayer and not more than 1.25 monolayers.

### Claim 6 (depends on 1)

The method of claim 1 wherein the step of providing the at least one of the free layer and the pinned layer further includes:
annealing the boron-free magnetic layer at a temperature above 300 K.

### Claim 7 (depends on 1)

The method of claim 1 wherein the oxidizing step further includes:
naturally oxidizing the wetting layer.

### Claim 8 (depends on 1)

The method of claim 1 wherein the wetting layer includes at least one of elemental Fe, elemental Co, elemental Ni, elemental Mn, an Fe-containing alloy, a Co-containing alloy, a Ni-containing alloy and a Mn containing alloy.

### Claim 9 (depends on 1)

The method of claim 1 wherein the boron-free magnetic layer includes at least one of elemental Fe, elemental Co, elemental Ni, elemental Mn, an Fe-containing alloy, a Co-containing alloy, a Ni-containing alloy, a Mn containing alloy and a Heusler alloy.

### Claim 10 (depends on 1)

The method of claim 1 wherein the step of providing the wetting layer further includes:
providing the wetting layer on an oxide layer.

### Claim 11 (depends on 10)

The method of claim 10 wherein the nonmagnetic spacer layer includes the oxide layer.

### Claim 12 (depends on 1)

The method of claim 1 wherein the step of providing the at least one of the free layer and the pinned layer further includes:
providing an oxide capping layer on the boron-free magnetic layer.

### Claim 13 (depends on 1)

The method of claim 1 further comprising:
providing an additional nonmagnetic spacer layer; and
providing an additional pinned layer, the additional nonmagnetic spacer layer being between the additional pinned layer and the free layer.

### Claim 14 (depends on 1)

The method of claim 1 wherein the at least one of the free layer and the pinned layer includes a polarization enhancement layer, and wherein the polarization enhancement layer includes the boron-free magnetic layer.

### Claim 15 (depends on 1)

The method of claim 1 wherein the free layer is a multilayer.

### Claim 16 (depends on 1)

The method of claim 1 wherein pinned layer is a multilayer.

### Claim 17 (depends on 1)

The method of claim 1 wherein the free layer is switchable between the plurality of stable magnetic states using at least one of spin transfer torque and spin-orbit coupling torque.

### Claim 18

A method for providing magnetic junction residing on a substrate and usable in a magnetic device, the method comprising:
providing a pinned layer, the pinned layer being magnetic;
providing a nonmagnetic spacer layer; and
providing a free layer, the nonmagnetic spacer layer being between the pinned layer and the free layer, the free layer being magnetic and switchable between a plurality of stable magnetic states using at least one of spin transfer torque and spin-orbit coupling torque, wherein at least one of the step of providing the pinned layer and the step of providing the free layer further include
depositing a wetting layer while the portion of the magnetic junction is cooled, the wetting layer having a thickness of not more than three monolayers and at least 0.25 monolayer, the wetting layer including at least one magnetic material;
at least one of oxidizing and nitriding the wetting layer to provide a treated wetting layer, the treated wetting layer being an oxide wetting layer for an oxidizing process and a nitride wetting layer for a nitriding process;
cooling a portion of the magnetic junction including the treated wetting layer to within a temperature range including at least one temperature not greater than 250 K; and
depositing a boron-free magnetic layer on the treated wetting layer while the portion of the magnetic junction is within the temperature range, the boron-free magnetic layer having a perpendicular magnetic anisotropy energy greater than an out-of-plane demagnetization energy.

### Claim 19

A memory magnetic junction residing on a substrate and comprising:
a plurality of magnetic storage cells, each of the plurality of magnetic storage cells including at least one magnetic junction, the at least one magnetic junction including a free layer, a nonmagnetic spacer layer and a pinned layer, the nonmagnetic spacer layer residing between the pinned layer and the free layer, the free layer being switchable between a plurality of stable magnetic states when a write current is passed through the magnetic junction, at least one of the free layer and the pinned layer including a boron-free magnetic layer, the boron-free magnetic layer having a perpendicular magnetic anisotropy energy greater than an out-of-plane demagnetization energy.