# US 2019/0157540 A1 · Method of forming superconducting wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0157540 A1
- Document ID: US20190157540A1
- Status: Published application
- Kind: A1
- Application number: 16/196,125
- Filed: 2018-11-20
- Published: 2019-05-23
- Earliest claimed: 2017-11-20
- Assignees: Seoul National University R&Db Foundation
- Applicants: Seoul National University R&DB Foundation
- Inventors: Sang-Im YOO; Insung PARK
- Web page: https://patentgrep.com/patent/US20190157540A1

## CPC

- H10N 60/0548: {by deposition and subsequent treatment, e.g. oxidation of pre-deposited material}
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 29/22: Complex oxides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10N 60/0381: {by evaporation, e.g. MBE}
- H10N 60/0632: {Intermediate layers, e.g. for growth control}
- H10N 60/0772: {Processes including the use of non-gaseous precursors}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Provided is a method of forming a superconducting wire, the method including forming a superconducting precursor film on a substrate, the super conducting precursor film containing Re, Ba, and Cu having a composition in which Ba is poor and Cu is rich compared to stoichiometric ReBCO(Gd1Ba2Cu3O7−y, 0≤y≤6, Re: Rare earth element), heating the substrate to melt the superconducting precursor film, providing an oxygen gas having an oxygen partial pressure of about 10 mTorr to about 200 mTorr on the molten superconducting precursor film to form a superconducting layer including an epitaxial superconductor biaxially aligned only in the c-axis direction perpendicular to the substrate, and cooling the substrate.

## Claims

### Claim 1

A method of forming a superconducting wire, the method comprising:
forming a superconducting precursor film on a substrate, the superconducting precursor film containing Re, Ba, and Cu and having a composition in which Ba is poor and Cu is rich compared to stoichiometric ReBCO (Gd1Ba2Cu3O7−y, 0≤y≤0.65, Re: Rare earth element);
heating the substrate to melt the superconducting precursor film;
providing an oxygen gas having an oxygen partial pressure of about 10 mTorr to about 200 mTorr on the molten superconducting precursor film to form a superconducting layer including an epitaxial superconductor biaxially aligned only in the c-axis direction perpendicular to the substrate; and
cooling the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the Re is Gd, and the superconducting precursor film contains Gd, Ba, and Cu in a mixing ratio of 1:1:2.5.

### Claim 3 (depends on 2)

The method of claim 2, wherein
the substrate is heated to a c-axis growth temperature determined according to the oxygen partial pressure, and the c-axis growth temperature is about 774° C. to about 880° C.

### Claim 4 (depends on 3)

The method of claim 3, wherein
the c-axis growth temperature includes a lower limit temperature and an upper limit temperature, and when the oxygen partial pressure increases to about 20 mTorr to about 150 mTorr, the lower limit temperature gradually increases from about 780° C. to about 848° C., and the upper limit temperature gradually increases from about 800° C. to about 866° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein
when the oxygen partial pressure is about 150 mTorr, the lower limit temperature is about 850° C. and the upper limit temperature is about 866° C.

### Claim 6 (depends on 4)

The method of claim 4, wherein
when the oxygen partial pressure is about 100 mTorr, the lower limit temperature is about 832° C. and the upper limit temperature is about 850° C.

### Claim 7 (depends on 4)

The method of claim 4, wherein
when the oxygen partial pressure is about 50 mTorr, the lower limit temperature is about 810° C. and the upper limit temperature is about 830° C.

### Claim 8 (depends on 4)

The method of claim 4, wherein
when the oxygen partial pressure is about 20 mTorr, the lower limit temperature is about 790° C. and the upper limit temperature is about 800° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein
when the oxygen partial pressure is about 10 mTorr, the c-axis growth temperature is about 774° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein
when the oxygen partial pressure is about 200 mTorr, the c-axis growth temperature is about 880° C.