# US 2019/0157073 A1 · Lithography process using photoresist material with photosensitive functional group

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0157073 A1
- Document ID: US20190157073A1
- Status: Published application
- Kind: A1
- Application number: 16/124,063
- Filed: 2018-09-06
- Published: 2019-05-23
- Earliest claimed: 2017-11-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Ming-Hui WENG; Cheng-Han WU; Ching-Yu CHANG; Chin-Hsiang LIN; Siao-Shan WANG
- Web page: https://patentgrep.com/patent/US20190157073A1

## CPC

- G03F 7/0392: {the macromolecular compound being present in a chemically amplified positive photoresist composition}
- G03F 7/0045: {with organic non-macromolecular light-sensitive compounds not otherwise provided for, e.g. dissolution inhibitors}
- G03F 7/0397: {the macromolecular compound having an alicyclic moiety in a side chain}
- G03F 7/70033: {by plasma extreme ultraviolet [EUV] sources}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/693: {characterised by their size, orientation, disposition, behaviour or shape, in horizontal or vertical plane}
- H10P 76/2041: {Photolithographic processes}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods for forming a semiconductor structure including using a photoresist material are provided. The method for forming a semiconductor structure includes forming a material layer over a substrate and forming a photoresist layer over the material layer. The method for forming a semiconductor structure further includes performing an exposure process on the photoresist layer and developing the photoresist layer. In addition, the photoresist layer is made of a photoresist material comprising a photosensitive polymer, and the photosensitive polymer has a first photosensitive functional group bonding to a main chain of the photosensitive polymer and a first acid labile group bonding to the first photosensitive functional group.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
forming a material layer over a substrate;
forming a photoresist layer over the material layer;
performing an exposure process on the photoresist layer; and
developing the photoresist layer,
wherein the photoresist layer is made of a photoresist material comprising a photosensitive polymer, and the photosensitive polymer has a first photosensitive functional group bonding to a main chain of the photosensitive polymer and a first acid labile group bonding to the first photosensitive functional group.

### Claim 2 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the first sensitive functional group is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group.

### Claim 3 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the first photosensitive functional group and the first acid labile group are released from the main chain of the photosensitive polymer to form an —COOH group on the photosensitive polymer after the exposure process is performed.

### Claim 4 (depends on 3)

The method for forming a semiconductor structure as claimed in claim 3, wherein the photosensitive polymer further has a second photosensitive functional group bonding to the main chain of the photosensitive polymer through a covalent bond, and the second photosensitive functional group remains on the main chain of the photosensitive polymer after the exposure process is performed.

### Claim 5 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the photosensitive polymer further has a second acid labile group that bonds to the main chain of the photosensitive polymer, and the first acid labile group is different from the second acid labile group.

### Claim 6 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the first acid labile group bonds to the first photosensitive group through a linker, and the linker is a covalent bond, C1-C10 alkyl group, C1-C10 alkenyl group, or C1-C10 alkynyl group.

### Claim 7 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the photoresist material further comprises a compound having one of the following formulae:
wherein ST3 is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group;
ST3′ is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group; and
ST3″ is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group.

### Claim 8 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the photoresist material further comprises an additional photosensitive compound having an aromatic group substituted with at least one hydroxyl group or at least one thiol group, and the additional photosensitive compound has a molecular weight less than about 2000.

### Claim 9

A method for forming a semiconductor structure, comprising:
forming a material layer over a substrate;
forming a photoresist layer over the material layer;
performing an exposure process on the photoresist layer; and
developing the photoresist layer,
wherein the photoresist layer is made of a photoresist material comprising a first photosensitive compound and a second photosensitive compound, and the first photosensitive compound is a photosensitive polymer having a first acid labile group and a first photosensitive functional group bonding to a main chain of the photosensitive polymer, and the second photosensitive compound has a second photosensitive functional group, and the second photosensitive compound has a molecular weight less than about 3000.

### Claim 10 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the second photosensitive compound has the following formula:
wherein R2, R3, R4 and R5 are individually selected from H, C1-C3 alkyl group, and aryl group and at least one of R2, R3, R4 and R5 comprises the second photosensitive functional group, and the second photosensitive functional group is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group.

### Claim 11 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the second photosensitive compound has one of the following formulae:
wherein R1 is —OH or —SH, and n is a positive integer less than 4.

### Claim 12 (depends on 10)

The method for forming a semiconductor structure as claimed in claim 10, wherein the second photosensitive compound has one of the following formulae:
wherein ST3 is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group;
ST3′ is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group; and
ST3″ is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group.

### Claim 13 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the first acid labile group bonds to the first photosensitive functional group through a linking structure, and the linking structure L1 is a covalent bond, C1-C10 alkyl group, C3-C10 alkenyl group, C3-C10 alkynyl group, or C1-C10 alkoxy group.

### Claim 14 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the first photosensitive functional group is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group

### Claim 15 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the photosensitive polymer further comprises a second acid labile group bonding to the main chain of the photosensitive polymer, and the first acid labile group is different from the second acid labile group.

### Claim 16 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the second photosensitive compound has a molecular weight less than about 2000, and the photosensitive polymer has a weight average molecular weight in a range from about 3000 to about 20000.

### Claim 17

A method for forming a semiconductor structure, comprising:
forming a material layer over a substrate;
forming a photoresist layer over the material layer;
performing an exposure process on the photoresist layer;
developing the photoresist layer to form a patterned photoresist layer; and
patterning the material layer through the patterned photoresist layer,
wherein the photoresist layer is made of a photoresist material comprising a photosensitive polymer, and the photosensitive polymer has a first acid labile group, a second acid labile group different from the first acid labile group, and a first photosensitive functional group, and the first photosensitive functional group bonds to the first acid labile group.

### Claim 18 (depends on 17)

The method for forming a semiconductor structure as claimed in claim 17, wherein the photosensitive polymer is hydrolyzed to release the first acid labile group and the second acid labile group alone with the first photosensitive functional group after the exposure process is performed.

### Claim 19 (depends on 17)

The method for forming a semiconductor structure as claimed in claim 17, wherein the photoresist material further comprises a first photosensitive compound having the following formula:
wherein R2, R3, R4 and R5 are individually selected from H, C1-C3 alkyl group, and aryl group and at least one of R2, R3, R4 and R5 comprises the second photosensitive functional group, and the second photosensitive functional group is a C6-C30 aromatic group substituted with at least one hydroxyl group or at least one thiol group.

### Claim 20 (depends on 17)

The method for forming a semiconductor structure as claimed in claim 17, wherein the photoresist material further comprises a cross-linker, and the cross-linker bonds to the first photosensitive compounds after the exposure process is performed.