# US 2019/0152860 A1 · Spinel refractory granulates which are suitable for elasticizing heavy-clay refractory products, method for their production and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0152860 A1
- Document ID: US20190152860A1
- Status: Published application
- Kind: A1
- Application number: 16/301,786
- Filed: 2017-03-23
- Published: 2019-05-23
- Earliest claimed: 2016-05-19
- Applicants: Refratechnik Holding GmbH
- Inventors: Heinrich Liever; Hilmar Schulze-Bergkamen; Carsten Vellmer
- Web page: https://patentgrep.com/patent/US20190152860A1

## CPC

- C04B 35/0473: {obtained from fused grains}
- C04B 35/10: based on aluminium oxide
- C04B 35/101: Refractories from grain sized mixtures
- C04B 35/26: based on ferrites
- C04B 35/443: Magnesium aluminate spinel
- C04B 35/6261: {Milling}
- C04B 35/6265: {involving reduction or oxidation}
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 35/66: Monolithic refractories or refractory mortars, including those whether or not containing clay {(making or repairing of linings F27D1/16)}
- F27D 1/0006: {Linings or walls formed from bricks or layers with a particular composition or specific characteristics}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3272: Iron oxides or oxide forming salts thereof, e.g. hematite, magnetite
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/5427: millimeter or submillimeter sized, i.e. larger than 0,1 mm
- C04B 2235/5472: Bimodal, multi-modal or multi-fraction
- C04B 2235/6583: Oxygen containing atmosphere, e.g. with changing oxygen pressures
- C04B 2235/763: Spinel structure AB2O4
- C04B 2235/77: Density
- C04B 2235/782: Grain size distributions
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/9607: Thermal properties, e.g. thermal expansion coefficient
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

The invention relates to a granular, refractory mineral elasticizing granulate for refractory products, in particular for basic refractory products. The minerals consist of mono-phased fused spinel mixed crystal or multi-phased fusion products of the ternary system MgO−Fe2O3—Al2O3 of the composition range MgO: 12 to 19.5, in particular 15 to 17 wt.- %, Remainder: Fe2O3 and Al2O3 in a quantity ratio range of Fe2O3 to Al2O3 between 80 to 20 and 40 to 60 wt.- %. Starting from an MgO content between 12 and 19.5 wt.- %, the respective mixed crystals have an Fe2O3 and Al2O3 content in a solid solution out of the limited ranges respectively indicated thereof, such that a total composition of 100% is obtained. In addition, the invention relates to a method for production of the elasticizing granulate and to the use thereof.

## Claims

### Claim 1

A granular, refractory mineral elasticizing granulate for refractory products, the elasticizing granulate comprising a ternary system MgO—Fe2O3—Al2O3 as a mono-phased fused spinel mixed crystal or a multi-phased fused product, the ternary system MgO—Fe2O3—Al2O3 having a composition with the following range:
MgO: 12 to 19.5 wt.- %,
Remainder: Fe2O3 and Al2O3 in a quantity ratio range of Fe2O3 to Al2O3 between 80 to 20 and 40 to 60 wt.- %,
wherein starting from an MgO content between 12 and 19.5 wt.- %, the mixed crystal having an Fe2O3 and Al2O3 content in solid solution out of the limited ranges respectively indicated thereof, such that a total composition of 100% is obtained.

### Claim 2 (depends on 1)

The elasticizing granulate according to claim 1, wherein the elasticizing granulate has a bulk density of ≤3.5, measured according to DIN EN 993-18.

### Claim 3 (depends on 1)

The elasticizing granulate according to claim 1, wherein the elasticizing granulate has less than 15 wt- % of secondary phases.

### Claim 4 (depends on 1)

The elasticizing granulate according to claim 1, wherein the elasticizing granulate has a grain compressive strength between 30 MPa and 50 MPa, measured with reference to DIN EN 13005.

### Claim 5 (depends on 1)

The elasticizing granulate according to claim 1, wherein the elasticizing granulate has a linear coefficient of expansion between 8.5 and 9.5·10−6 K−1.

### Claim 6 (depends on 1)

The elasticizing granulate according to claim 1, wherein the elasticizing granulate has grain sizes between 0 and 6 mm, with the following grain distributions under Gaussian grain distributions:
0.5-1.0 mm 30-40 wt.- %
1.0-2.0 mm 50-60 wt.- %.

### Claim 7 (depends on 1)

A method for producing the mono-phased elasticizing granulate according to claim 1, the method comprising:
mixing
at least one high purity powdered MgO component
at least one high purity powdered Fe2O3-component, and
at least one high purity powdered Al2O3-component
in the composition range according to claim 1,
fusing the mixture in a neutral or reducing atmosphere to a fused product,
cooling the fused product,
crushing the fused product into a granulate and classified, and
converting the granulate via high-temperature oxidation into the mono-phased spinel product.

### Claim 8 (depends on 7)

The method according to claim 7, wherein
at least one raw material for the MgO component is selected from the group consisting of: fused magnesia, sintered magnesia, caustic magnesia, with MgO contents greater than 96 wt- %, and an iron-rich, alpine sintered magnesia,
at least one raw material for the Fe2O3 component is selected from the group consisting of magnetite, hematite, and mill scale, with Fe2O3-contents greater than 90 wt- %, and
at least one raw material for the Al2O3 component is selected from the group consisting of: aluminum oxide in the form of alpha or gamma alumina with Al2O3 contents greater than 98 wt- % and calcined metallurgical bauxite.

### Claim 9 (depends on 7)

The method according to claim 7 wherein the components are mixed and/or crushed in a grinding machine to ≤1 mm.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the mixtures are fused at temperatures between 1,750 and 2,200° C.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the mixtures are compacted before fusing by granulation or compression.

### Claim 12

A basic, ceramic fired or non-fired refractory product in the form of shaped refractory bodies, or in the form of non-shaped refractory masses, the refractory product comprising:
50 to 95 wt- % of at least one granular, basic, refractory material, with grain sizes between 1 and 7 mm;
0 to 20 wt- % of at least one powdered, basic, refractory material, with grain sizes ≤1 mm;
5 to 20 wt- % of at least one granular elasticizing granulate with grain sizes between 0.5 and 4 mm;
0 to 5 wt- % of at least one powdered additive with grain sizes ≤1 mm; and
0 to 5 wt- % of at least one binder normally used for refractory products.

### Claim 13