# US 2019/0152827 A1 · Preparation of quartz glass bodies from silicon dioxide powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0152827 A1
- Document ID: US20190152827A1
- Status: Published application
- Kind: A1
- Application number: 16/061,451
- Filed: 2016-12-16
- Published: 2019-05-23
- Earliest claimed: 2015-12-18
- Assignees: Heraeus Quarzglas GmbH & Co. KG
- Applicants: Heraeus Quarzglas GmbH & Co. KG
- Inventors: Matthias OTTER; Walter LEHMANN; Michael HÜNERMANN; Nils Christian NIELSEN; Martin TROMMER
- Web page: https://patentgrep.com/patent/US20190152827A1

## CPC

- C03B 20/00: Processes specially adapted for the production of quartz or fused silica articles {, not otherwise provided for (C03B19/01, C03B19/066, C03B19/106, C03B19/12, C03B19/14, C03B37/00 take precedence)}
- C01B 33/12: Silica; Hydrates thereof, e.g. lepidoic silicic acid
- C03B 17/04: Forming tubes or rods by drawing from stationary or rotating tools or from forming nozzles
- C03B 19/106: {by chemical vapour deposition; by liquid phase reaction}
- C03B 19/108: {Forming porous, sintered or foamed beads (chemical aspects C03C11/00)}
- C03B 19/1095: {Thermal after-treatment of beads, e.g. tempering, crystallisation, annealing}
- C03B 37/01211: {by inserting one or more rods or tubes into a tube}
- C03B 37/027: Fibres composed of different sorts of glass, {e.g. glass optical fibres}(C03B37/0253, C03B37/028 take precedence)
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03B 5/0336: {Shaft furnaces (C03B5/0338 takes precedence)}
- C03B 5/06: in pot furnaces {(C03B5/02 takes precedence)}
- C03B 2201/03: Impurity concentration specified
- C03B 2201/04: Hydroxyl ion (OH)
- C03B 2201/07: Impurity concentration specified
- C03B 2201/23: doped with hydroxyl groups
- C03B 2203/34: Plural core other than bundles, e.g. double core
- G01N 21/412: {Index profiling of optical fibres}
- G02B 6/02042: {Multicore optical fibres}
- H01J 9/247: {specially adapted for gas-discharge lamps}
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

One aspect relates to a process for the preparation of a quartz glass body, including providing a silicon dioxide granulate, making a glass melt out of silicon dioxide granulate and making a quartz glass body out of at least part of the glass melt. The silicon dioxide granulate is obtained by providing and processing a silicon dioxide powder. One aspect also relates to silicon dioxide granulate, which is obtained by providing a silicon dioxide powder and processing it. One aspect further relates to a quartz glass body which is obtainable by this process. One aspect further relates to a light guide, an illuminant and a formed body, which are each obtainable by further processing of the quartz glass body.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A process for the preparation of a quartz glass body comprising:
providing a silicon dioxide granulate comprising:
providing a silicon dioxide powder; and
processing the silicon dioxide powder to obtain a silicon dioxide granulate,
wherein the silicon dioxide granulate has a greater particle diameter than
the silicon dioxide powder;
making a glass melt out of the silicon dioxide granulate in an oven; and
making a quartz glass body out of at least part of the glass melt;
wherein the silicon dioxide powder comprises:
a BET surface area in a range from 20 to 60 m2/g; and
a bulk density in a range from 0.01 to 0.3 g/cm3.

### Claim 17 (depends on 16)

The process according to claim 16, wherein a silicon dioxide granulate with granules is formed in the processing, wherein the granules have a spherical morphology, and wherein the processing comprises a spray granulation or a roll granulation.

### Claim 18 (depends on 16)

The process according to claim 16, wherein the silicon dioxide powder comprises at least one of:
a carbon content of less than 50 ppm;
a chlorine content of less than 200 ppm;
an aluminium content of less than 200 ppb;
a total content of metals different from aluminium of less than 5 ppm;
at least 70 wt.-% of the powder particles have a primary particle size in a range from 10 to 100 nm;
a tamped density in a range from 0.001 to 0.3 g/cm3;
a residual moisture content of less than 5 wt.-%;
a particle size distribution D10 in a range from 1 to 7 μm;
a particle size distribution D50 in a range from 6 to 15 μm; and
a particle size distribution D90 in a range from 10 to 40 μm;
wherein the wt.-%, ppm and ppb are each based on the total weight of the silicon dioxide powder.

### Claim 19 (depends on 16)

The process according to claim 16, wherein making the glass melt out of the silicon dioxide granulate in an oven comprises:
providing a liquid;
mixing the silicon dioxide powder with the liquid to obtain a slurry; and
granulating the slurry to obtain the silicon dioxide granulate.

### Claim 20 (depends on 16)

The process according to claim 16, further comprising making a hollow body with at least one opening out of the quartz glass body.

### Claim 21

A silicon dioxide granulate, wherein the silicon dioxide granulate comprises:
a BET surface area in a range from 20 to 50 m2/g; and
a bulk density in a range from 0.5 to 1.2 g/cm3.

### Claim 22 (depends on 21)

The silicon dioxide granulate according to claim 21, wherein the silicon dioxide granulate comprises an angle of repose in a range from 23 to 26°.

### Claim 23 (depends on 21)

The silicon dioxide granulate according to claim 21, further comprising at least one of:
a mean particle size in a range from 50 to 500 μm;
a carbon content of less than 50 ppm;
an aluminium content of less than 200 ppb;
a tamped density in a range from 0.7 to 1.3 g/cm3;
a pore volume in a range from 0.1 to 2.5 mL/g;
a particle size distribution D10 in a range from 50 to 150 μm;
a particle size distribution D50 in a range from 150 to 300 μm; and
a particle size distribution D90 in a range from 250 to 620 μm,
wherein the ppm and ppb are each based on the total weight of the silicon dioxide granulate.

### Claim 24 (depends on 16)

A quartz glass body obtained by a process according to claim 16.

### Claim 25 (depends on 24)

The quartz glass body according to claim 24, comprising:
an OH content of less than 500 ppm;
a chlorine content of less than 200 ppm;
an aluminium content of less than 200 ppb;
an ODC content of less than 5·1015/cm3;
a metal content of metals different from aluminium of less than 1 ppm;
a viscosity (p=1013 hPa) in a range from log10 (n (1250° C.)/dPas)=11.4 to log10 (η (1250° C.)/dPas)=12.9 or log10 (η (1300° C.)/dPas)=11.1 to log10 (η (1300° C.)/dPas)=12.2 or log10 (η (1350° C.)/dPas)=10.5 to log10 (η (1350° C.)/dPas)=11.5;
a standard deviation of the OH content of not more than 10%, based on the OH-content of the quartz glass body;
a standard deviation of the Cl content of not more than 10%, based on the Cl content of the quartz glass body;
a standard deviation of the Al content of not more than 10%, based on the Al content of the quartz glass body;
a refractive index homogeneity of less than 10−4;
a cylindrical form;
a tungsten content of less than 100 ppb; and
a molybdenum content of less than 100 ppb,
wherein the ppb and ppm are each based on the total weight of the quartz glass body.

### Claim 26 (depends on 20, 24)

A process for the preparation of a light guide comprising:
providing:
a hollow body with at least one opening obtained by a process according to claim 20, or
a quartz glass body according to claim 24, wherein the quartz glass body is first processed to obtain a hollow body with at least one opening;
introducing one or multiple core rods into the hollow body through the at least one opening to obtain a precursor; and
drawing the precursor in the warm to obtain a light guide with one or multiple cores and a jacket.

### Claim 27 (depends on 20, 24)

A process for the preparation of an illuminant comprising:
providing
a hollow body with at least one opening obtained by a process according to claim 20; or
a quartz glass body according to claim 24, wherein the quartz glass body is first processed to obtain a hollow body;
optionally fitting the hollow body with electrodes; and
filling the hollow body with a gas.

### Claim 28 (depends on 24)

A process for the preparation of a formed body comprising:
providing a quartz glass body according to claim 24; and
forming the quartz glass body to obtain the formed body.

### Claim 29

A use of a silicon dioxide powder for the preparation of quartz glass and of products selected from the group consisting of a light guide, an illuminant and a formed body, wherein the silicon dioxide powder comprises:
a BET surface area in a range from 20 to 60 m2/g; and
a bulk density in a range from 0.01 to 0.3 g/cm3.

### Claim 30 (depends on 29)

The use according to claim 29, wherein the silicon dioxide powder is processed to obtain a silicon dioxide granulate, and wherein the silicon dioxide granulate has a greater particle diameter than the silicon dioxide powder.