# US 2019/0127925 A1 · Mold For Aluminothermic Welding Of A Metal Rail And Repair Method Making Use Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0127925 A1
- Document ID: US20190127925A1
- Status: Published application
- Kind: A1
- Application number: 16/096,999
- Filed: 2017-05-02
- Published: 2019-05-02
- Earliest claimed: 2016-04-29
- Assignees: Pandrol Limited
- Applicants: Pandrol
- Inventors: Pierre Bordery; Frédéric Delcroix
- Web page: https://patentgrep.com/patent/US20190127925A1

## CPC

- E01B 31/15: by planing or filing
- B23K 23/00: Alumino-thermic welding
- E01B 31/13: by milling
- E01B 31/18: Reconditioning or repairing worn or damaged parts on the spot, e.g. applying inlays, building-up rails by welding (E01B31/04 - E01B31/12 take precedence); Heating or cooling of parts on the spot, e.g. for reducing joint gaps, for hardening rails
- B23K 2101/26: Railway- or like rails
- E01B: PERMANENT WAY; PERMANENT-WAY TOOLS; MACHINES FOR MAKING RAILWAYS OF ALL KINDS (derailing or rerailing blocks on track, track brakes or retarders B61K)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The present invention relates in particular to a mold (M) for aluminothermic welding of a metal rail (1), which comprises at least two substantially identical pieces or shells (4), configured to be temporarily assembled opposite one another and on either side of said rail (1) to enclose the head (10), web (11) and foot (12) of this rail (1), each piece or shell (4) having an upper opening (43), which opens onto an internal cavity (44) bounded by walls (45, 46, 48) configured to enclose the head (10), the web (11) and the foot (12) of said rail (1), characterized by the fact that said internal cavity (44) comprises a compressible sealing coating (5) only against the walls (451, 46, 48) configured to enclose said web (11), foot (12) and underside of the head (10), with the exception of the rest of the head (10) and the underside of the foot (12).

## Claims

### Claim 1

A mold for aluminothermic welding of a metal rail, which comprises at least two substantially identical pieces or shells, configured to be temporarily assembled opposite one another and on either side of said rail to enclose the head, web and foot of the rail, each piece or shell having an upper opening, which opens onto an internal cavity bounded by walls configured to enclose the head, the web and the foot of said rail, wherein said internal cavity comprises a compressible sealing coating only against the walls configured to enclose said web, foot and underside of the head, with the exception of the rest of the head and the underside of the foot.

### Claim 2 (depends on 1)

The mold according to claim 1, wherein said coating is refractory felt.

### Claim 3 (depends on 1)

The mold according to claim 1, wherein the thickness of said coating is comprised between 2 and 10 mm.

### Claim 4 (depends on 1)

The mold according to claim 1, wherein the lower part of the piece opposite to the cavity has an inclined cut configured to avoid contact with a system for attaching the rail on a tie.

### Claim 5 (depends on 1)

A method for repairing a rail that has a surface defect at the level of its head, wherein the method comprises the following steps:
removing said defect so as to create a hollowing out on the head of said rail;
positioning the two pieces or shells of a mold according to claim 1 on either side of this rail; and
filling said hollowing out by pouring into said mold, via said upper opening, an aluminothermic welding material.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the web has, substantially in line with the defect to be repaired, a weld seam resulting from electric welding and that the compressible coating is intimately applied on said seam.