# US 2019/0099838 A1 · Combined laser treatment of a solid body to be split

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0099838 A1
- Document ID: US20190099838A1
- Status: Published application
- Kind: A1
- Application number: 16/086,533
- Filed: 2017-03-22
- Published: 2019-04-04
- Earliest claimed: 2016-03-22
- Assignees: Siltectra GmbH
- Applicants: Siltectra GmbH
- Inventors: Ralf Rieske; Marko Swoboda; Jan Richter
- Web page: https://patentgrep.com/patent/US20190099838A1

## CPC

- B23K 26/362: Laser etching
- B23K 26/38: by boring or cutting
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/0736: {into an oval shape, e.g. elliptic shape}
- B23K 26/0823: {Devices involving rotation of the workpiece}
- B23K 26/36: Removing material (B23K26/55, B23K26/57 take precedence)
- B23K 26/40: taking account of the properties of the material involved
- B23K 26/402: involving non-metallic material, e.g. isolators
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- C03B 33/0222: {Scoring using a focussed radiation beam, e.g. laser}
- C03B 33/04: Cutting or splitting in curves, especially for making spectacle lenses
- C03B 33/091: {using at least one focussed radiation beam, e.g. laser beam (C03B33/0955 takes precedence)}
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- B23K 2103/52: {Ceramics}
- B23K 2103/54: {Glass}
- B23K 2103/56: {being semiconducting}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The invention relates to a method for detaching at least one solid body layer (14) from a solid body (1), wherein by means of the modifications (2) a crack guiding region (4) is provided for guiding a crack in order to detach a solid body portion (6), in particular a solid body layer, from the solid body (1). The invention preferably comprises at least the steps: moving the solid body (1) relative to a laser application device (8), successively producing laser beams (10) by means of the laser application device (8) in order to produce respectively at least one modification (2), wherein the laser application device (8) is adjusted for defined production of modifications depending on at least one parameter, in particular the transmission of the solid body at defined locations and for a defined solid body depth, wherein inhomogeneities of the solid body (1) in the region of the affected surface and/or in the region of the affected volume of the solid body (1) can be compensated for by the adjustment of the laser application device (8), detaching the solid body layer (14) from the solid body (1).

## Claims

### Claim 1

A method for detaching at least one solid body layer (14) from a solid body (1), wherein by means of the modifications (2) a crack guiding region (4) is provided for guiding a crack in order to detach a solid body portion (6), in particular a solid body layer, from the solid body (1),
comprising at least the steps:
moving the solid body (1) relative to a laser application device (8), successively producing laser beams (10) by means of the laser application device (8) in order to produce respectively at least one modification (2),
wherein the laser application device (8) is adjusted for the defined production of modifications depending on at least one parameter, in particular the transmission of the solid body at defined locations and for a defined solid body depth,
wherein inhomogeneities of the solid body in the region of the affected surface and/or in the region of the affected volume of the solid body are compensated by the adjustment of the laser application device (8),
detaching the solid body layer (14) from the solid body (1).

### Claim 2 (depends on 1)

The method according to claim 1,
characterized in that
data relating to the parameter or to a plurality of parameters are provided in a data storage device and are supplied to a control device at least before generating the modifications (2), wherein the control device adjusts the laser application device (8) depending on the respective location of the modification (2) to be produced and/or
the laser beams (10) for generating modifications (2) have more energy in regions with low transmission than in regions with high transmission, wherein the laser application device (8) comprises a means, in particular an acousto-optic modulator for adjusting the laser beam energy.

### Claim 3

The method according to one of the preceding claims,
characterized in that
the solid body layer (14) is detached from the solid body (1) along the crack guiding region (4) as a result of the production of modifications or
the solid body (1) is acted upon thermally, in particular cooled, after the production of modifications and as a result of the thermal action the solid body layer (14) is detached from the solid body (1) along the crack guiding region (4) or
a stress generating layer (18) in particular a polymer layer, is arranged or produced on the solid body (1), wherein the polymer layer is preferably arranged or produced on a surface of the solid body layer (14) to be detached, wherein the polymer layer is acted upon thermally, in particular cooled, wherein the polymer layer undergoes a change in its strength in response to the thermal action, with the result that as a result of the change in strength of the polymer layer, mechanical stresses are obtained in the solid body (1), wherein the mechanical stresses bring about a crack propagation along the crack guiding region in order to detach the solid body layer (14) from the solid body (1).

### Claim 4

A method for producing at least one solid body layer (14) which is domed or curved at least in sections,
at least comprising the steps:
moving the solid body (1) relative to the laser application device (8),
successively producing laser beams by means of the laser application device (8) in order to produce respectively at least one modification (2) inside the solid body,
wherein as a result of the modifications (2) a crack guiding region (4) is provided for guiding a crack in order to detach a solid body portion (14), in particular a solid body layer, from the solid body (1),
wherein the modifications bring about a pressure rise in the solid body (1), wherein the solid body layer (14) is detached from the solid body (1) due to the propagation of a crack as a result of the pressure rise along the crack guiding region (4),
wherein at least a portion of the modifications (2) as part of the solid body layer (14) is separated from the solid body (1),
wherein the solid body layer (14) is converted into a curved or domed shape as a result of the modifications (2), wherein the further surface portion of the solid body layer (14) resulting from the crack guiding region (4) is therefore convexly shaped at least in sections.

### Claim 5 (depends on 4)

The method according to claim 4,
characterized in that
the laser beams (10) penetrate into the solid body (1) in the longitudinal direction of the solid body (1) or inclined at an angle of up to 60° with respect to the longitudinal direction (L) of the solid body (1) over an, in particular flat, surface which is preferably part of the solid body layer (14) and
the crack guiding region (4) is formed from several layers of modifications (2), wherein the layers are produced spaced apart from one another or offset in the longitudinal direction (L), and/or
at least a plurality of the modifications (2) have an extension in the longitudinal direction (L) which is between 1 and 50 μm and/or
the laser beams (10) for producing the modifications (2) are introduced into the solid body (1) in such a manner than the numerical aperture is less than 0.8.

### Claim 6

A method for detaching at least one solid body layer (14), in particular a solid body wafer (14) from a solid body or donor substrate (1),
at least comprising the steps:
providing a solid body (1),
producing modifications (2) inside the solid body (1) by means of laser beams (10),
wherein as a result of the modifications (2) a crack guiding region (4) is predefined along which the solid body layer (14) is detached from the solid body (1),
removing material of the solid body (1), in particular to produce a circumferential recess (12), wherein the removal of material takes place in the longitudinal direction of the solid body, wherein the crack guiding region (4) is exposed as a result of the removal of material, detaching the solid body layer (14) from the solid body,
wherein the solid body is weakened by the modifications in the crack guiding region (4) in such a manner that the solid body layer (1) becomes detached from the solid body (1) as a result of the removal of material, or
after the removal of material such a number of modifications is produced that the solid body is weakened in the crack guiding region in such a manner that the solid body layer (1) becomes detached from the solid body (1) or
a stress generating layer (18) is produced or arranged on an in particular flat surface (16) of the solid body (1) aligned at an inclination to the circumferential surface and as a result of a thermal action on the solid body layer (14), mechanical stresses are generated in the solid body (1), wherein a crack for detaching a solid body layer (14) is produced as a result of the mechanical stresses, which crack propagates along the modifications (2) starting from the surface of the solid body exposed by the removal of material or
the solid body is acted upon thermally, in particular cooled after the production of the modifications and as a result of the thermal action, the solid body layer (14) is detached from the solid body (1) along the crack guiding region (4).

### Claim 7 (depends on 6)

The method according to claim 6,
characterized in that
the removal of material takes place starting from an exposed, in particular flat surface of the solid body (1), in particular parallel to the circumferential surface of the solid body (1), in the longitudinal direction (L) of the solid body (1) and spaced apart from the circumferential surface of the solid body (1) at least in sections and/or
the removal of material takes place in the form of a trench (26) running continuously at least in sections, wherein the trench (26) is spaced apart from the circumferential surface preferably by at least 30 μm or at least 100 μm or at least 500 μm or at least 1 mm.

### Claim 8 (depends on 6, 7)

The method according to one of claims 6 to 7,
characterized in that
after detachment of the solid body layer (14), at least the solid body portion (28) of the solid body (1) formed between the trench (26) and the circumferential surface, is removed at least in sections, in particular by the thickness of the previously detached solid body layer (14) or solid body layers (14), in particular is ground, lapped, etched or polished
and/or the removal of material is brought about by means of laser ablation or water jet cutting or etching.

### Claim 9

A method for detaching at least one solid body layer, in particular a solid body wafer (14) from a solid body or donor substrate (1),
at least comprising the steps:
providing a solid body (1),
adjusting a flow behaviour of a gas, in particular air located between the solid body and the laser application device (8), in particular in the region of the radiation course, in order to prevent accumulations of dust in the region of the laser radiation,
producing modifications (2) inside the solid body (1) by means of laser beams (10) of a laser application device (8), wherein a detachment region or crack guiding region is predefined by the modifications (2) along which a detachment of the solid body layer (14) from the solid body (1) takes place,
detaching the solid body layer (14) from the solid body (1),
wherein the solid body (1) is weakened by the modifications (2) in the crack guiding region (4) in such a manner that the solid body layer (14) is detached from the solid body (1) as a result of the removal of material or
after the removal of material such a number of modifications is produced that the solid body is weakened in the crack guiding region in such a manner that the solid body layer (14) becomes detached from the solid body (1) or
a stress generating layer (18) is produced or arranged on an in particular flat surface (16) of the solid body (1) aligned at an inclination to the circumferential surface and as a result of a thermal action on the solid body layer (14), mechanical stresses are generated in the solid body (1), wherein a crack for detaching a solid body layer (14) is produced as a result of the mechanical stresses, which crack propagates along the modifications (2) starting from the surface of the solid body exposed by the removal of material or
the solid body (1) is acted upon thermally, in particular cooled after the production of the modifications and as a result of the thermal action, the solid body layer (14) is detached from the solid body (1) along the crack guiding region (4).

### Claim 10 (depends on 9)

The method according to claim 9,
characterized in that
the adjustment of the flow behaviour is made by supplying a fluid, in particular ionized gas, in the region of the beam course between an objective and the solid body (1) or the adjustment of the flow behaviour is made by producing a negative pressure, in particular a vacuum in the region of the beam course between an objective and the solid body (1).

### Claim 11

A method for detaching at least one solid body layer (14), in particular a solid body wafer (14) from a solid body or donor substrate (1),
at least comprising the steps:
providing a solid body (1),
wherein the solid body (1) has at least one coating (34) whose refractive index is different from the refractive index of the surface of the solid body (1) on which the coating (34) is arranged, or wherein a coating (34) is produced on the solid body (1) whose refractive index is different from the refractive index of the surface of the solid body (1) on which the coating (34) is arranged,
producing modifications (2) inside the solid body (1) by means of laser beams (10) of a laser application device (8), wherein a crack guiding region is predefined by the modifications (2) along which a detachment of the solid body layer (14) from the solid body (1) is accomplished.

### Claim 12 (depends on 11)

The method according to claim 11,
characterized in that
the coating (34) will be or is produced by means of spin coating, wherein the coating (34) comprises nanoparticles, in particular of at least one material selected from the list at least consisting of silicon, silicon carbide, titanium oxide, glass, in particular quartz glass or Al2O3 and/or
a plurality of coatings (34) are arranged or produced above one another, wherein the refractive indices differ from one another, preferably a first coating which is arranged or produced on the solid body (1) has a larger refractive index than an additional coating which is produced on the first coating.

### Claim 13

A method for detaching at least one solid body layer (14), in particular a solid body wafer (14) from a solid body or donor substrate (1),
at least comprising the steps:
providing a solid body (1),
producing modifications (2) inside the solid body (1) by means of laser beams (10) of a laser application device (8), wherein a crack guiding region is predefined by the modifications (2) along which a detachment of the solid body layer (14) from the solid body (1) is accomplished,
wherein the laser radiation is incident on the solid body at the Brewster angle or with a deviation in the range from −5° to +5° from the Brewster angle,
detaching the solid body layer from the solid body,
wherein the solid body is weakened in the crack guiding region (4) as a result of the modifications (2) in such a manner than the solid body layer (14) is detached from the solid body (1) as a result of the removal of material or
after the removal of material such a number of modifications (2) is produced that the solid body is weakened in the crack guiding region in such a manner that the solid body layer (14) is detached from the solid body (1) or
a stress generating layer (18) is produced or arranged on an in particular flat surface (16) of the solid body (1) aligned at an inclination to the circumferential surface and as a result of a thermal action on the solid body layer (14), mechanical stresses are generated in the solid (1), wherein a crack for detaching a solid body layer (14) is produced as a result of the mechanical stresses, which crack propagates along the modifications (2) starting from the surface of the solid body exposed by the removal of material or
the solid body is acted upon thermally, in particular cooled after the production of the modifications and as a result of the thermal action, the solid body layer (14) is detached from the solid body (1) along the crack guiding region (4).

### Claim 14 (depends on 13)

The method according to claim 13,
characterized in that
a compensating device, in particular an optical element such as a diffractive optical element or a continuous wedge is provided to compensate for a spherical aberration in the laser application device (8) resulting from the Brewster angle irradiation.

### Claim 15

A method for detaching at least one solid body layer (14) from a solid body (1), wherein due to modifications (2) a crack guiding region (4) is predefined for guiding a crack for detaching a solid body portion (6), in particular a solid body layer, from the solid body (1),
at least comprising the steps:
moving the solid body (1) relative to a laser application device (8), successively producing laser beams (10) by means of the laser application device (8) to produce respectively at least one modification (2),
detaching the solid body layer (14) from the solid body (1).

### Claim 16 (depends on 15)

The method according to claim 15,
characterized in that
wherein the laser application device (8) is adjusted for the defined generation of modifications depending on at least one parameter, namely the transmission of the solid body (1) at defined points and for a defined solid body depth and/or
wherein the modifications (2) bring about a pressure rise in the solid body (1),
wherein the solid body layer (14) is detached from the solid body (1) as a result of the pressure rise along the crack guiding region due to a crack propagation, wherein at least one portion of the modifications (2) as part of the solid body layer (14) is detached from the solid body (1) and wherein the solid body layer (14) is preferably converted into a curved or domed form as a result of the modifications (2), wherein the further surface portion of the solid body layer (14) resulting from the crack guiding region (4) is therefore convexly shaped at least in sections and/or
wherein the solid body (1) has at least one coating (34) whose refractive index is different from the refractive index of the surface of the solid (1) on which the coating (34) is arranged or wherein a coating (34) is produced on the solid (1), whose refractive index is different from the refractive index of the surface of the solid (1) on which the coating (34) is arranged and/or
wherein the laser radiation is incident on the solid body (1) at the Brewster angle or with a deviation in the range from −10° to +10° from the Brewster angle,
comprising one or more of the steps:
removing material of the solid body (1), in particular to produce a circumferential recess (12), wherein the material is removed in the longitudinal direction of the solid body (1),
wherein the crack guiding region (4) is exposed as a result of the removal of material or adjusting a flow behaviour of a gas, in particular air, located between the solid body (1) and the laser application device (8), in particular in the region of the radiation course, to prevent accumulations of dust in the region of the laser radiation (10).

### Claim 17 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 16)

The method according to claim 16 or claims 1 to 9,
characterized in that
a parameter is the degree of doping of the solid body at a predetermined location or in a predetermined region, in particular inside the solid body, in particular at a distance from the solid body surface,
wherein the degree of doping is preferably determined by the analysis of back-scattered light having an inelastic scattering (Raman scattering), wherein the back-scattered light has a different wavelength or a different wavelength range from emitted light defined for triggering the back-scattering, wherein the back-scattered light is back-scattered from the predefined location or from the predefined region or
wherein the degree of doping is preferably determined by means of an eddy current measurement, wherein conductivity differences in the solid body material are determined.

### Claim 18 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 16, 17)

The method according to one of claims 16 to 17 or according to one of claims 1 to 9,
further comprising the step:
producing a composite structure by arranging or producing layers and/or components (150) on or above an initially exposed surface of the solid body (1), wherein the exposed surface is part of the solid body layer to be detached,
wherein the modifications are produced to form the detachment plane before producing the composite structure.

### Claim 19 (depends on 18)

The method according to claim 18,
characterized in that
before producing the detachment plane the solid body (1) is treated using at least one high-temperature method, wherein the high-temperature method is executed with a temperature between 70° C. and the melting point or evaporation temperature of the material of the solid body (1),
wherein the at least one high-temperature method is an epitaxy method, a doping method or a method using plasma, wherein at least one layer (145) is produced on the solid body (1) by the high-temperature method, wherein the at least one generated layer (145) has predefined parameters, wherein at least one predefined parameter specifies a maximum degree of refraction and/or absorption and/or reflection of laser light waves, wherein the degree of refraction and/or absorption and/or reflection is less than 5% and preferably less than 1% and particularly preferably less than 0.1%.

### Claim 20

The method according to one of the preceding claims,
characterized in that
the modifications are produced by means of multiphoton excitation,
wherein initially at least a plurality of base modifications are produced on an in particular curved line, running homogeneously at least in sections, in particular in the homogeneously running section,
wherein these base modifications are produced with predefined process parameters,
wherein the predefined process parameters preferably comprise the energy per shot and/or the shot density,
wherein at least one value of these process parameters and preferably both values or all the values of these process parameters or more than two values of these process parameters is specified depending on the crystal lattice stability of the solid body,
wherein the value is selected so that the crystal lattice remains intact around the respective base modifications,
wherein further trigger modifications are produced to trigger subcritical cracks,
wherein at least one process parameter for generating trigger modifications is different from at least one process parameter for generating base modifications,
preferably a plurality of process parameters are different from one another and/or the trigger modifications are produced in a direction which is inclined to or spaced apart from the course direction of the line along which the base modifications are generated, wherein the subcritical cracks propagate less than 5 mm.

### Claim 21

The method according to one of the preceding claims,
characterized in that
the solid body material is silicon, wherein the numerical aperture lies between 0.5 and 0.8, in particular 0.65, the irradiation depth is between 200 μm and 400 μm, in particular 300 μm, the pulse spacing is between 1 μm and 5 μm, in particular 2 μm, the line spacing is between 1 μm and 5 μm, in particular 2 μm, the pulse duration is between 50 ns and 400 ns, in particular 300 ns and the pulse energy is between 5 μJ and 15 μJ, in particular 10 μJ
or
the solid body material is SiC, wherein the numerical aperture lies between 0.5 and 0.8, in particular 0.4, the irradiation depth is between 100 μm and 300 μm, in particular 180 μm, the pulse spacing is between 0.1 μm and 3 μm, in particular 1 μm, the line spacing is between 20 μm and 100 μm, in particular 75 μm, the pulse duration is between 1 ns and 10 ns, in particular 3 ns and the pulse energy is between 3 μJ and 15 μJ, in particular 7 μJ.

### Claim 22 (depends on 20, 21)

The method according to one of claim 20 or 21,
characterized in that
the subcritical cracks propagate between 5 μm and 200 μm, in particular between 10 μm and 100 μm or between 10 μm and 50 μm or between 10 μm and 30 μm or between 20 μm and 100 μm or between 20 μm and 50 μm or between 20 μm and 30 μm in the solid
and/or
tear sections between the regions of several lines in which the subcritical cracks have propagated as a result of the stresses that are produced by the glass transition.