# US 2019/0097260 A1 · 3d magnesium battery and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0097260 A1
- Document ID: US20190097260A1
- Status: Published application
- Kind: A1
- Application number: 15/715,915
- Filed: 2017-09-26
- Published: 2019-03-28
- Earliest claimed: 2017-09-26
- Assignees: Toyota Motor Engineering & Manufacturing North America, Inc.; Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Motor Engineering & Manufacturing North America, Inc.; Toyota Jidosha Kabushiki Kaisha
- Inventors: Fuminori Mizuno; Rana Mohtadi; Oscar Tutusaus; Nikhilendra Singh; Timothy S. Arthur; Ruidong Yang; Kensuke Takechi; Chen Ling; Ruigang Zhang
- Web page: https://patentgrep.com/patent/US20190097260A1

## CPC

- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/808: {Foamed, spongy materials}
- H01M 10/0445: {Multimode batteries, e.g. containing auxiliary cells or electrodes switchable in parallel or series connections}
- H01M 10/0468: {Compression means for stacks of electrodes and separators}
- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/466: {Magnesium based}
- H01M 10/04: Construction or manufacture in general (H01M10/058, H01M10/12, H01M10/28, H01M10/38 take precedence)
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

3-D magnesium voltaic cells have a magnesium anode coated on multiple opposing surfaces with a continuous protective/electrolyte layer that is ionically conductive and electronically insulating. The resulting protected 3-D magnesium anode is coated on multiple opposing surfaces with a continuous cathode layer that is electronically and ionically conductive, and includes a magnesium storage medium. Suitable magnesium anodes, in particular, magnesium foam anodes, can be made by pulsed galvanostatic deposition of magnesium on a copper substrate. The protective layer can be formed by electropolymerization of a suitable methylacrylate ester. The continuous cathode layer can be a slurry cathode having powders of an electronic conductor and a reversible magnesium storage component suspended in a magnesium electrolyte solution.

## Claims

### Claim 1

A three dimensional (3-D) magnesium voltaic cell, comprising:
a magnesium foam anode;
a continuous protective layer contacting the magnesium foam anode on substantially all surfaces; the continuous protective layer being electrically insulative and ionically conductive; and
a continuous slurry cathode layer contacting substantially all surfaces of the continuous protective layer, the continuous slurry cathode layer comprising:
a reversible magnesium storage component;
an electronic conductor; and
a magnesium ion conductor.

### Claim 2 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the continuous protective layer comprises a polymer or co-polymer of at least one methacrylic acid ester.

### Claim 3 (depends on 2)

The 3-D magnesium voltaic cell as recited in claim 2, wherein the at least one methacrylic acid ester is selected from the group consisting of poly(glycidyl methacrylate) and poly(3-sulfopropyl methacrylate).

### Claim 4 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the magnesium foam anode is formed entirely of magnesium metal.

### Claim 5 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the magnesium foam anode comprises a magnesium insertion anode.

### Claim 6 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the magnesium foam anode comprises a copper foam substrate having a surface layer of magnesium when at least partially charged.

### Claim 7 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the reversible magnesium storage component comprises a conjugated quinone.

### Claim 8 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the magnesium ion conductor comprises an anion having a formula:
[ByH(y-z-1)RzXi]2−,
[CB(y-1)H(y-z-1)RzXi]−,
[C2B(y-2)H(y-t-j-1)RtXj]−,
[C2B(y-3)H(y-t-j)RtXj]−, or
[C2B(y-3)H(y-t-j-1)RtXj]2,
wherein y is an integer within a range of 6 to 12; (z+i) is an integer within a range of 0 toy; (t+j) is an integer within a range of 0 to (y−1); and X is F, Cl, Br, I, or a combination thereof; and
wherein R is alkyl, aryl, alkoxy, aryloxy, a fluorinated derivative of the aforementioned, or a moiety having any combination of the aforementioned.

### Claim 9 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the magnesium ion conductor comprises Mg(CB11H12)2.

### Claim 10 (depends on 1)

The 3-D magnesium voltaic cell as recited in claim 1, wherein the continuous cathode slurry layer comprises 20 percent, by volume, 5,7,12,14-pentacenetetrone as reversible magnesium storage component, 0.8%, by volume, Ketjen black as electronic conductor, and 79.2%, by volume, 0.3 M Mg(CB11H12)2 in tetraglyme.

### Claim 11

A three-dimensional (3-D) magnesium voltaic cell, comprising:
a magnesium anode, comprising magnesium metal when at least partially charged;
a continuous protective layer contacting the magnesium anode on at least two opposing surfaces to form a protected anode, the continuous protective layer being electrically insulative and ionically conductive; and
a continuous cathode layer contacting the continuous protective layer of the protected anode on at least two opposing surfaces, the continuous cathode layer comprising:
a reversible active material storage component;
an electronic conductor; and
an ionic conductor.

### Claim 12 (depends on 11)

The 3-D magnesium voltaic cell as recited in claim 11, wherein the continuous protective layer has ionic conductivity greater than 0.01 S/cm and electric conductivity less than 10−8 S/cm.

### Claim 13 (depends on 11)

The 3-D magnesium voltaic cell as recited in claim 11, wherein the ionic conductor comprises an electrolyte for conducting a non-magnesium active cation; and the reversible active material storage component comprises a cathode material configured to reversibly store the non-magnesium active cation; the 3-D magnesium voltaic cell thus comprising a dual-ion cell.

### Claim 14 (depends on 13)

The 3-D magnesium voltaic n cell as recited in claim 13, wherein the ionic conductor comprises a sodium electrolyte and the reversible active material storage component comprises a sodium cathode material.

### Claim 15 (depends on 14)

The 3-D magnesium voltaic cell as recited in claim 14, wherein the sodium electrolyte comprises Na(CB11H12).

### Claim 16

A method of making a 3-D magnesium voltaic cell, comprising:
contacting a magnesium anode on at least two opposing sides with a continuous protective layer, to form a protected 3-D magnesium anode; and
coating the continuous protective layer of the protected 3-D magnesium anode on all available surfaces with a continuous cathode layer, thereby forming the 3-D magnesium voltaic cell.

### Claim 17 (depends on 16)

The method as recited in claim 16, further comprising:
electrodepositing a layer of magnesium on a porous copper substrate, thereby forming the magnesium anode.

### Claim 18 (depends on 16)

The method as recited in claim 16, further comprising:
electrodepositing a layer of magnesium on a copper foam substrate, the copper foam substrate having porosity of at least 0.8, thereby forming the magnesium anode.

### Claim 19 (depends on 16)

The method as recited in claim 16, comprising:
electrodepositing a layer of magnesium on a copper substrate via galvanostatic pulsed electrodeposition, thereby forming the magnesium anode.

### Claim 20 (depends on 19)

The method as recited in claim 19, wherein the galvanostatic pulsed electrodeposition includes a pulse duration of about ten seconds and a rest duration of about ten seconds.