# US 2019/0096987 A1 · N-type polysilicon crystal, manufacturing method thereof, and n-type polysilicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0096987 A1
- Document ID: US20190096987A1
- Status: Published application
- Kind: A1
- Application number: 16/120,300
- Filed: 2018-09-02
- Published: 2019-03-28
- Earliest claimed: 2017-09-25
- Assignees: Sino-American Silicon Products Inc.
- Applicants: Sino-American Silicon Products Inc.
- Inventors: Ching-Hung Weng; Cheng-Jui Yang; Yu-Min Yang; Yuan-Hsiao Chang; Bo-Kai Wang; Wen-Huai Yu; Ying-Ru Shih; Sung-Lin Hsu
- Web page: https://patentgrep.com/patent/US20190096987A1

## CPC

- H10D 62/405: {Orientations of crystalline planes}
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 28/06: by normal freezing or freezing under temperature gradient
- C30B 29/06: Silicon
- H10D 62/40: Crystalline structures
- H10D 62/53: the imperfections being within the semiconductor body
- H10D 62/834: further characterised by the dopants
- H10F 71/1221: {comprising polycrystalline silicon}
- H10F 77/1642: {including only Group IV materials}
- Y02E 10/546: Polycrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An N-type polysilicon crystal, a manufacturing method thereof, and an N-type polysilicon wafer are provided. The N-type polysilicon crystal has a slope of resistivity and a slope of defect area percentage. When the horizontal axis is referred to solidified fraction and the vertical axis is referred to resistivity presented by a unit of Ohm·cm (Ω·cm), the slope of resistivity is 0 to −1.8 at the solidified fraction of 0.25 to 0.8. When the horizontal axis is referred to solidified fraction and the vertical axis is referred to defect area percentage (%), the slope of defect area percentage is less than 2.5 at the solidified fraction of 0.4 to 0.8.

## Claims

### Claim 1

An N-type polysilicon crystal, wherein:
the N-type polysilicon crystal has a slope of resistivity, and when a horizontal axis is referred to a solidified fraction and a vertical axis is referred to the resistivity presented by a unit of Ohm·cm (Ω·cm), the slope of resistivity is 0 to −1.8 at the solidified fraction of 0.25 to 0.8; and
the N-type polysilicon crystal has a slope of defect area percentage, and when the horizontal axis is referred to the solidified fraction and the vertical axis is referred to the defect area percentage (%), the slope of defect area percentage is less than 2.5 at the solidified fraction of 0.4 to 0.8.

### Claim 2 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein an average value of a minority carrier lifetime of the N-type polysilicon crystal measured via a μ-PCD method is greater than 20 μs.

### Claim 3 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein the N-type polysilicon crystal is doped with gallium and phosphorous, a doping amount of the gallium is 0.3 ppma to 3 ppma, a doping amount of the phosphorous is 0.02 ppma to 0.2 ppma, and an atomic ratio of the gallium with respect to the phosphorous is between 10 and 20.

### Claim 4 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein the N-type polysilicon crystal comprises an ingot, a brick, or a wafer.

### Claim 5 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein a crystal orientation of the N-type polysilicon crystal at least comprises {111}, {112}, {113}, {315}, and {115}.

### Claim 6 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein the defect area percentage of the N-type polysilicon crystal is less than 2% at the solidified fraction of 0.4 to 0.8.

### Claim 7 (depends on 1)

The N-type polysilicon crystal of claim 1, wherein when an oxygen content in the N-type polysilicon crystal is in a range of greater than or equal to 5 ppma, a carbon content of a corresponding location thereof is greater than or equal to 4 ppma.

### Claim 8 (depends on 7)

The N-type polysilicon crystal of claim 7, wherein the N-type polysilicon crystal comprises a plurality of silicon crystal grains grown along a crystal growth direction, wherein an average crystal grain size of the silicon crystal grains in the crystal growth direction and a resistivity of the N-type polysilicon crystal have opposite changing trends.

### Claim 9 (depends on 8)

The N-type polysilicon crystal of claim 8, wherein the average crystal grain size is less than or equal to 1.3 cm.

### Claim 10 (depends on 1)

An N-type polysilicon wafer obtained by cutting the N-type polysilicon crystal of claim 1, wherein an average value of a minority carrier lifetime of the N-type polysilicon wafer measured via a μ-PCD method is 2 μs to 5 μs.

### Claim 11

A manufacturing method of an n-type polysilicon crystal, comprising:
growing an N-type polysilicon crystal using a crystal growth furnace of a directional solidification system (DSS), wherein a crucible in the crystal growth furnace contains a silicon material and a dopant, a height of the N-type polysilicon crystal is H, and the dopant is located in a region of 0.1 H to 0.3 H from a bottom portion of the crucible.

### Claim 12 (depends on 11)

The manufacturing method of the N-type polysilicon crystal of claim 11, wherein the dopant comprises a particle, a doping sheet, or a combination thereof.

### Claim 13 (depends on 11)

The manufacturing method of the N-type polysilicon crystal of claim 11, wherein the dopant comprises gallium and phosphorous.

### Claim 14 (depends on 13)

The manufacturing method of the N-type polysilicon crystal of claim 13, wherein a doping amount of gallium is 0.3 ppma to 3 ppma, a doping amount of phosphorous is 0.02 ppma to 0.2 ppma, and an atomic ratio of gallium with respect to phosphorous is between 10 and 20.

### Claim 15 (depends on 11)

The manufacturing method of the N-type polysilicon crystal of claim 11, wherein the silicon material comprises a waste wafer.

### Claim 16 (depends on 15)

The manufacturing method of the N-type polysilicon crystal of claim 15, wherein the dopant comprises a particle, and the manufacturing method of the N-type polysilicon crystal further comprises: before the N-type polysilicon crystal is grown, covering a portion of the silicon material by the waste wafer; placing the particle on the waste wafer; and surrounding and covering the particle by a remainder of the silicon material.

### Claim 17 (depends on 15)

The manufacturing method of the N-type polysilicon crystal of claim 15, wherein the dopant comprises a particle and a doping sheet, and the manufacturing method of the N-type polysilicon crystal further comprising: before the N-type polysilicon crystal is grown, covering a portion of the silicon material by the waste wafer; placing the particle on the waste wafer; covering the particle by another waste wafer; placing the doping sheet on the another waste wafer on the particle; and adding a remainder of the silicon material.