# US 2019/0096672 A1 · Systems and Methods for Patterning Features in Tantalum Nitride (TaN) Layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0096672 A1
- Document ID: US20190096672A1
- Status: Published application
- Kind: A1
- Application number: 16/032,759
- Filed: 2018-07-11
- Published: 2019-03-28
- Earliest claimed: 2017-09-26
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Vinh Luong; Isabel Cristina Chu; Ashim Dutta
- Web page: https://patentgrep.com/patent/US20190096672A1

## CPC

- H10P 50/242: {of Group IV materials}
- H10P 50/267: {using plasmas}
- H10P 50/283: {by chemical means}
- H10P 50/287: {by chemical means}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments of systems and methods for patterning features in tantalum nitride (TaN) are described. In an embodiment, a method may include receiving a substrate comprising a TaN layer. The method may also include etching the substrate to expose at least a portion of the TaN layer. Additionally, the method may include performing a passivation process to reduce lateral etching of the TaN layer. The method may further include etching the TaN layer to form a feature therein, wherein the passivation process is controlled to meet one or more target passivation objectives.

## Claims

### Claim 1

A method for treating a substrate, comprising:
receiving a substrate comprising a tantalum nitride (TaN) layer;
etching the substrate to expose at least a portion of the TaN layer;
performing a passivation process to reduce lateral etching of the TaN layer; and
etching the TaN layer to form a feature therein;
wherein the passivation process is controlled to meet one or more target passivation objectives.

### Claim 2 (depends on 1)

The method of claim 1, wherein the performing the passivation process is performed concurrently with etching the TaN layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein performing the passivation process further comprises reducing a number of radicals in a plasma used for etching the TaN layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein performing the passivation process further comprises reducing fluorine (F) radicals in a plasma formed from sulfur hexafluoride (SF6) gas used for etching the TaN layer.

### Claim 5 (depends on 4)

The method of claim 4, further comprising adding hydrogen bromide (HBr) to the SF6 gas, the hydrogen from the HBr reducing a number of F radicals in the SF6 plasma.

### Claim 6 (depends on 1)

The method of claim 1, wherein performing the passivation process further comprises adding a passivation gas to a plasma gas mixture.

### Claim 7 (depends on 6)

The method of claim 6, wherein the passivation gas comprises boron trichloride (BCl3) gas.

### Claim 8 (depends on 6)

The method of claim 6, wherein the passivation gas comprises hydrogen bromide (HBr) gas.

### Claim 9 (depends on 6)

The method of claim 6, wherein the passivation gas comprises fluoroform (CHF3) gas.

### Claim 10 (depends on 6)

The method of claim 6, wherein the passivation gas comprises methane (CH4) gas.

### Claim 11 (depends on 6)

The method of claim 6, wherein controlling the passivation process further comprises controlling a flow rate of the passivation gas.

### Claim 12 (depends on 11)

The method of claim 11, wherein the flow rate of the passivation gas is in a range of 1-50 sccm or a range of 12-24 sccm.

### Claim 14 (depends on 1)

The method of claim 1, wherein controlling the passivation process further comprises controlling a pressure within a processing chamber.

### Claim 15 (depends on 14)

The method of claim 14, wherein the pressure is in a range of 1-100 mT or in a range of 34-60 mT.

### Claim 16 (depends on 1)

The method of claim 1, wherein controlling the passivation process further comprises controlling a temperature within a processing chamber.

### Claim 17 (depends on 16)

The method of claim 16, wherein the temperature is in a range of 30-60 degrees Celsius.

### Claim 18 (depends on 1)

The method of claim 1 the passivation gas comprises boron trichloride (BCl3) gas and hydrogen bromide (HBr) gas.

### Claim 19 (depends on 1)

The method of claim 1 wherein the passivation process and etching process are iterated to meet passivation objectives.

### Claim 20

A method of treating a substrate, the method comprising:
providing an input patterned feature comprising a patterning layer and a tantalum nitride (TaN) layer in a process chamber;
performing a series of material open processes on the patterning layer using a mask, the open processes creating an intermediate patterned feature;
performing a passivation process and an etch process on the intermediate feature, the passivation process using a boron-containing and/or a hydrogen-containing gas mixture, the passivation process and the etch process generating an output patterned feature;
adjusting one or more operating variables of the passivation process and the etch process in order to achieve one or more process objectives.

### Claim 21 (depends on 20)

The method of claim 20 wherein the one or more operating variables comprise one or more of a flow rate of the boron-containing gas, flowrate of the hydrogen-containing gas, a ratio of the flowrate of the boron-containing gas to the hydrogen-containing gas, flowrate of other gases including argon, SF6, a high frequency power, a low frequency power, a pressure in the process chamber, and electrostatic chuck temperature.

### Claim 22 (depends on 20)

The method of claim 20 wherein the one or more process objectives comprise one or more of a target etch rate of the TaN layer, a target profile of the patterned feature comprising a target base width, a target neck width, a target cap width, a target height, and/or a target total height of the output patterned feature.