Fine cellulose fiber and production method for same
AssigneeKRI, Inc.
InventorsLianzhen LIN, Ayako MARUTA, Masanori HORI
Life of this patent
Estimating the term…
Loading patent…
AssigneeKRI, Inc.
InventorsLianzhen LIN, Ayako MARUTA, Masanori HORI
Estimating the term…
Provided is a method of producing fine cellulose fibers that are nanosized, that have a high crystallinity degree, and that are less vulnerable to fiber shape damage, the method including impregnating cellulose with a fibrillation solution to fibrillate the cellulose without mechanical crushing, and modifying the cellulose. The method of producing cellulose microfibrils of the present invention includes impregnating cellulose with a fibrillation solution containing a carboxylic acid vinyl ester or an aldehyde and an aprotic solvent having a donor number of 26 or more to fibrillate the cellulose. The aldehyde is at least one kind of aldehyde selected from the group consisting of an aldehyde represented by the following formula (1), paraformaldehyde, cinnamaldehyde, perillaldehyde, vanillin, and glyoxal: R1—CHO (1) where R1 represents a hydrogen atom, an alkyl group having 1 to 16 carbon atoms, an alkenyl group, a cycloalkyl group, or an aryl group.
A method of producing fine cellulose fibers, comprising impregnating cellulose with a fibrillation solution containing an aprotic solvent having a donor number of 26 or more and a carboxylic acid vinyl ester or an aldehyde to fibrillate the cellulose,
Surface-modified fine cellulose fibers, which have an average fiber diameter of from 2 nm to 800 nm and an aspect ratio of from 40 to 1,000, and which are dispersible in an organic solvent or a resin having a SP value of 10 or less.
Dependencies are inferred from the claim text.