# US 2019/0084862 A1 · Coatings for glass-shaping molds and molds comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0084862 A1
- Document ID: US20190084862A1
- Status: Published application
- Kind: A1
- Application number: 16/137,730
- Filed: 2018-09-21
- Published: 2019-03-21
- Earliest claimed: 2017-09-21
- Assignees: Entegris, Inc.
- Applicants: Entegris, Inc.
- Inventors: Troy SCOGGINS; Rex Gerald Sheppard; Carlo Waldfried
- Web page: https://patentgrep.com/patent/US20190084862A1

## CPC

- C03B 11/086: {of coated dies (use of materials as release or lubricating compositions C03B40/02)}
- C03B 40/00: Preventing adhesion between glass and glass or between glass and the means used to shape it {, hold it or support it}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45555: {applied in non-semiconductor technology}
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- C23C 28/42: {characterized by the composition of the alternating layers}
- C03B 2215/03: defined by material properties or parameters, e.g. relative CTE of mould parts
- C03B 2215/05: Press-mould die materials
- C03B 2215/10: Die base materials
- C03B 2215/20: Oxide ceramics
- C03B 2215/31: Two or more distinct intermediate layers or zones
- C03B 2215/32: of metallic or silicon material
- C03B 2215/34: of ceramic or cermet material, e.g. diamond-like carbon
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Described are glass-forming molds made of a graphite mold body and a coating formed by atomic layer deposition, with the coating being made of alumina or a combination of alumina and yttria.

## Claims

### Claim 1

A glass-forming mold comprising:
a fine-grained graphite mold body having one or more mold features,
a coating on the one or more mold features, the coating being formed by atomic layer deposition and comprising an alumina layer or layers of alumina and yttria.

### Claim 2 (depends on 1)

The mold of claim 1, wherein the coating has a coefficient of thermal expansion that is within 1 part per million/° C. of the coefficient of thermal expansion of the graphite mold body.

### Claim 3 (depends on 1)

The mold of claim 1, wherein the fine-grained graphite has a grain size that is not greater than 10 microns.

### Claim 4 (depends on 1)

The mold of claim 1, wherein a thickness of the coating is between 10 nanometers and 500,000 nanometers.

### Claim 5 (depends on 1)

The mold of claim 1, wherein the coating consists essentially of alumina.

### Claim 6 (depends on 1)

The mold of claim 1, wherein the coating consists essentially of alternating layers of alumina and yttria.

### Claim 7 (depends on 1)

The mold of claim 1, wherein the mold is free of surface discontinuities that are greater than about 25 microns from the average surface plane of the mold.

### Claim 8

A method of making a glass-forming mold comprising:
providing a fine-grained mold body, and
depositing a coating on the mold body by atomic layer deposition, the coating comprising an alumina layer or layers of alumina and yttria.

### Claim 9 (depends on 8)

The method of claim 8, wherein the coating has a coefficient of thermal expansion that is within 1 part per million/° C. of the coefficient of thermal expansion of the graphite mold body.

### Claim 10 (depends on 8)

The method of claim 8, wherein the fine-grained graphite has a grain size that is not greater than 10 microns.

### Claim 11 (depends on 8)

The method of claim 8, wherein a thickness of the coating is between 10 nanometers and 500,000 nanometers.

### Claim 12 (depends on 8)

The method of claim 8, wherein the coating consists essentially of alumina.

### Claim 13 (depends on 8)

The method of claim 8, wherein the coating consists essentially of alternating layers of alumina and yttria.

### Claim 14 (depends on 8)

The method of claim 8, wherein the mold is free of surface discontinuities that are greater than about 25 microns from the average surface plane of the mold.

### Claim 15

A method of forming a glass article comprising:
providing a fine-grained mold body;
depositing a coating on the mold body by atomic layer deposition, the coating comprising an alumina layer or layers of alumina and yttria; and
contacting a surface of the mold with softened glass.

### Claim 16 (depends on 15)

The method of claim 15, wherein the softened glass is softened alumino-silicate glass.