# US 2019/0058193 A1 · Method for producing lithium-ion, sodium-ion and potassium-ion batteries with increased safety

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0058193 A1
- Document ID: US20190058193A1
- Status: Published application
- Kind: A1
- Application number: 15/766,210
- Filed: 2016-10-06
- Published: 2019-02-21
- Earliest claimed: 2015-10-09
- Assignees: River Road Research, Inc.
- Applicants: River Road Research, Inc.
- Inventors: Radu Popa; Kenneth H. Nealson; Vily M. Cimpoiasu
- Web page: https://patentgrep.com/patent/US20190058193A1

## CPC

- H01M 4/604: {containing aliphatic main chain polymers}
- C09B 68/423: {Cationic groups}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 10/052: Li-accumulators
- H01M 2004/027: {Negative electrodes}
- H01M 2200/00: Safety devices for primary or secondary batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C09B: ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES {, e.g. PIGMENTS}; MORDANTS; LAKES (fermentation or enzyme using processes to synthesise a desired chemical compound C12P)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing lithiated pyomelanin (LPM), sodiated pyomelanin (SPM) and potassiated pyomelanin (PPM) is provided. A method is also provided for improving the safety of lithium-ion (Li-ion), sodium-ion (Na-ion) and potassium-ion (K-ion) batteries. The method employs using LPM, SPM or PPM in the negative compartment (anode) of the batteries. These LPM Li-ion, SPM Na-ion and PPM K-ion batteries have decreased tendencies to overheat and/or explode.

## Claims

### Claim 1

A method for producing lithiated pyomelanin (LPM) comprising:
dissolving melanin in an alkaline lithium solution or in a solution comprising a mixture comprising:
LiOH; or
NaOH/KOH and a Li salt,
thereby producing an alkaline solution of lithium ions (Li+) comprising the melanin;
reducing the alkaline lithium solution comprising the melanin using a reducing agent or using a cathode of an electrochemical cell at an electrical potential ≤0.8V;
in a reducing environment and/or in an electrical potential ≤0.8V and under anaerobic conditions, titrating the alkaline lithium solution comprising the melanin to neutral pH;
in the reducing environment and/or in the electrical potential ≤0.8V and under anaerobic conditions, dialyzing the mixture relative to dH2O, thereby producing a solution comprising LPM;
under anaerobic conditions, freezing the solution comprising LPM; and
lyophilizing the solution comprising LPM to remove water; thereby producing LPM.

### Claim 2 (depends on 1)

The method of claim 1 wherein the dialyzing is conducted under cold conditions.

### Claim 3 (depends on 1)

The method of claim 1 wherein the dialyzing is conducted using a low cutoff dialysis membrane or filter.

### Claim 4

A method for producing sodiated pyomelanin (SPM) comprising:
dissolving melanin in an alkaline sodium solution or in a solution comprising a mixture comprising:
NaOH; or
KOH and a sodium salt,
thereby producing an alkaline solution of sodium ions (Na+) comprising the melanin;
reducing the alkaline sodium solution comprising the melanin using a reducing agent or using a cathode of an electrochemical cell at an electrical potential ≤0.8V;
in a reducing environment and/or in an electrical potential ≤0.8V and under anaerobic conditions, titrating the alkaline sodium solution comprising the melanin to neutral pH;
in the reducing environment and/or in the electrical potential ≤0.8V and under anaerobic conditions, dialyzing the mixture relative to dH2O, thereby producing a solution comprising SPM;
under anaerobic conditions, freezing the solution comprising SPM; and
lyophilizing the solution comprising SPM to remove water; thereby producing SPM.

### Claim 5 (depends on 4)

The method of claim 4 wherein the dialyzing is conducted under cold conditions.

### Claim 6 (depends on 4)

The method of claim 4 wherein the dialyzing is conducted using a low cutoff dialysis membrane or filter.

### Claim 7

A method for producing potassiated pyomelanin (PPM) comprising:
dissolving melanin in an alkaline potassium solution or in a solution comprising a mixture comprising:
KOH; or
NaOH and a potassium salt,
thereby producing an alkaline solution of potassium ions (K+) comprising the melanin;
reducing the alkaline potassium solution comprising the melanin using a reducing agent or using a cathode of an electrochemical cell at an electrical potential ≤0.8V;
in a reducing environment and/or in an electrical potential ≤0.8V and under anaerobic conditions, titrating the alkaline potassium solution comprising the melanin to neutral pH;
in the reducing environment and/or in the electrical potential ≤0.8V and under anaerobic conditions, dialyzing the mixture relative to dH2O, thereby producing a solution comprising PPM;
under anaerobic conditions, freezing the solution comprising PPM; and
lyophilizing the solution comprising PPM to remove water; thereby producing PPM.

### Claim 8 (depends on 7)

The method of claim 7 wherein the dialyzing is conducted under cold conditions.

### Claim 9 (depends on 7)

The method of claim 7 wherein the dialyzing is conducted using a low cutoff dialysis membrane or filter.

### Claim 10

A method for producing a battery with increased safety, wherein the battery comprises an anode(−) compartment and a cathode(+) compartment, the method comprising:
providing a battery anode mixture;
providing lithiated pyomelanin (LPM), sodiated pyomelanin (SPM) and/or potassiated pyomelanin (PPM);
providing a battery electrolyte, wherein the battery electrolyte is non-aqueous or a proton-releasing chemical; and
adding the LPM, SPM and/or PPM to the battery anode mixture, thereby producing a battery anode mixture comprising the LPM, SPM and/or PPM, wherein the battery anode mixture comprising the LPM, SPM and/or PPM is in sufficiently low abundance so that when the battery is short-circuited or demand on the battery for electricity is large, heat released during discharge of the battery is less than a specific heat capacity of the battery, thereby:
increasing safety of the battery by avoiding formation of metallic lithium (Lio), sodium (Nao) and/or potassium (Ko) in the battery,
lowering risk of overheating of the battery and/or lowering risk of explosion of the battery, and
producing a battery with increased safety.

### Claim 11 (depends on 10)

The method of claim 10 wherein the battery anode mixture is a carbon anode mixture.

### Claim 12 (depends on 10)

The method of claim 10 wherein the LPM, SPM and/or PPM is added to and/or coated on a conductive surface of the anode compartment.