# US 2019/0057863 A1 · Methods and apparatus for doping engineering and threshold voltage tuning by integrated deposition of titanium nitride and aluminum films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0057863 A1
- Document ID: US20190057863A1
- Status: Published application
- Kind: A1
- Application number: 16/104,352
- Filed: 2018-08-17
- Published: 2019-02-21
- Earliest claimed: 2017-08-18
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: YIXIONG YANG; PAUL F. MA; WEI V. TANG; WENYU ZHANG; SHIH CHUNG CHEN; CHEN HAN LIN; CHI-CHOU LIN; YI XU; YU LEI; NAOMI YOSHIDA; LIN DONG; SIDDARTH KRISHNAN
- Web page: https://patentgrep.com/patent/US20190057863A1

## CPC

- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10D 64/01: Manufacture or treatment
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/01332: {Making the insulator}
- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods and apparatus for forming a semiconductor structure, including depositing a doping stack having a first surface atop a high-k dielectric layer, wherein the doping stack includes at least one first metal layer having a first surface, at least one second metal layer comprising a first aluminum dopant and a first surface, wherein the second metal layer is atop the first surface of the first metal layer, and at least one third metal layer atop the first surface of the second metal layer; depositing an anneal layer atop the first surface of the doping stack; annealing the structure to diffuse at least the first aluminum dopant into the high-k dielectric layer; removing the anneal layer; and depositing at least one work function layer atop the first surface of the doping stack.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
depositing a doping stack having a first surface atop a high-k dielectric layer, wherein the doping stack comprises at least one first metal layer having a first surface, at least one second metal layer comprising a first aluminum dopant and a first surface, wherein the second metal layer is atop the first surface of the first metal layer, and at least one third metal layer atop the first surface of the second metal layer;
depositing an anneal layer atop the first surface of the doping stack;
annealing to diffuse at least the first aluminum dopant into the high-k dielectric layer;
removing the anneal layer; and
depositing at least one work function layer atop the first surface of the doping stack.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first metal layer and third metal layer is TiN.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second metal layer is an aluminum composition comprising: aluminum, titanium aluminide, titanium-aluminum carbide, titanium aluminum nitride, aluminum nitride, aluminum carbide, aluminum oxide, hafnium aluminide carbide, or combinations thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein annealing comprises heating the doping stack to a temperature at or above 700° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the annealing layer comprises polysilicon.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in the first metal layer has a thickness of about 2 angstroms to about 10 angstroms.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second metal layer has a thickness of about 2 angstroms to about 10 angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein the third metal layer has a thickness of about 5 angstroms to about 15 angstroms.

### Claim 9 (depends on 1)

The method of claim 1, wherein the high-k dielectric layer comprises HfAlO, HfAlON, HfSiAlON, HfLaON, and combinations thereof.

### Claim 10 (depends on 1)

The method according to claim 1, wherein in the high-k dielectric layer, the first metal layer, second metal layer, and third metal layer may be formed by one of physical vapor deposition, chemical vapor deposition, and atomic layer deposition.

### Claim 11

A method of treating a high-k dielectric layer comprising:
depositing a first titanium nitride layer atop a high-k dielectric layer;
depositing a first aluminum layer atop the first titanium nitride layer;
depositing a second titanium nitride layer atop the first aluminum layer; and
annealing the high-k dielectric layer, first titanium nitride layer, first aluminum layer and second titanium nitride layer at a temperature above 900° C.

### Claim 12 (depends on 11)

The method of claim 11, wherein prior to annealing, a first reaction prevention layer is applied atop the second titanium nitride layer.

### Claim 13 (depends on 11)

The method of claim 11, wherein the first aluminum layer is a film having a thickness of about 2 angstroms to about 10 angstroms.

### Claim 14 (depends on 11)

The method of claim 11, wherein annealing at a temperature above 900° C. diffuses aluminum from the first aluminum layer at least one of into or onto the high-k dielectric layer.

### Claim 15

A method of treating a high-k dielectric layer disposed on a substrate, comprising:
(a) sequentially depositing a first titanium nitride layer, a first aluminum layer, and second titanium nitride layer atop a high-k dielectric layer; and
(b) heating the high-k dielectric layer to a peak temperature of about 900° C. to about 1200° C., wherein aluminum from the first aluminum layer diffuses at least one of into or onto the high-k dielectric layer.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the second titanium nitride layer is formed to be thicker than the first titanium nitride layer.

### Claim 17 (depends on 15)

The method of claim 15, wherein in the first titanium nitride layer has a thickness of about 2 angstroms to about 10 angstroms.

### Claim 18 (depends on 15)

The method of claim 15, wherein the first aluminum layer has a thickness of about 2 angstroms to about 10 angstroms.

### Claim 19 (depends on 15)

The method of claim 15, wherein second titanium nitride layer has a thickness of about 5 angstroms to about 15 angstroms.

### Claim 20 (depends on 15)

The method of claim 15, wherein the first titanium nitride layer has a thickness of about 2 angstroms to about 10 angstroms, and the second titanium nitride layer has a thickness of about 5 angstroms to about 15 angstroms.