# US 2019/0056653 A1 · Reflective mask blank and reflective mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0056653 A1
- Document ID: US20190056653A1
- Status: Published application
- Kind: A1
- Application number: 16/056,765
- Filed: 2018-08-07
- Published: 2019-02-21
- Earliest claimed: 2017-08-15
- Assignees: AGC Inc.
- Applicants: Agc Inc.
- Inventors: Hirotomo KAWAHARA; Hiroshi HANEKAWA; Toshiyuki UNO
- Web page: https://patentgrep.com/patent/US20190056653A1

## CPC

- G03F 1/40: Electrostatic discharge [ESD] related features, e.g. antistatic coatings or a conductive metal layer around the periphery of the mask substrate
- G03F 1/24: Reflection masks; Preparation thereof
- G03F 1/38: Masks having auxiliary features, e.g. special coatings or marks for alignment or testing; Preparation thereof
- G03F 1/48: Protective coatings
- G03F 1/52: Reflectors
- G03F 1/54: Absorbers, e.g. of opaque materials
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A reflective mask blank includes a backside conductive film on a back surface of a substrate. The backside conductive film has a laminated structure including a stress compensation layer and a conductive layer in this order from the substrate side. The conductive layer includes a metal nitride. The stress compensation layer has a compressive stress and the stress compensation layer includes at least one compound selected from the group consisting of oxides, oxynitrides, and nitrides, each having an absorption coefficient (k) over the wavelength range of 400 nm to 800 nm being 0.1 or less. The conductive layer has a thickness of 5 nm or more and 30 nm or less. The backside conductive film has a total thickness of 50 nm or more.

## Claims

### Claim 1

A reflective mask blank, comprising:
a backside conductive film on a back surface of a substrate,
wherein the backside conductive film has a laminated structure comprising a stress compensation layer and a conductive layer in this order from the substrate side,
wherein the conductive layer comprises a metal nitride,
wherein the stress compensation layer has a compressive stress,
wherein the stress compensation layer comprises at least one compound selected from the group consisting of oxides, oxynitrides, and nitrides, each having an absorption coefficient (k) over the wavelength range of 400 nm to 800 nm being 0.1 or less,
wherein the conductive layer has a thickness of 5 nm or more and 30 nm or less, and
wherein the backside conductive film has a total thickness of 50 nm or more.

### Claim 2 (depends on 1)

The reflective mask blank according to claim 1,
wherein the backside conductive film has a compressive stress with a total stress of 50 Pa·m to 400 Pa·m.

### Claim 3 (depends on 1)

The reflective mask blank according to claim 1,
wherein the stress compensation layer has a compressive stress with a film internal stress per unit film thickness of 300 MPa to 2,000 MPa.

### Claim 4 (depends on 1)

The reflective mask blank according to claim 1,
wherein the stress compensation layer has a refractive index (n) over the wavelength range of 400 nm to 800 nm of 1.7 or more.

### Claim 5 (depends on 1)

The reflective mask blank according to claim 1,
wherein the compound in the stress compensation layer comprises at least one element selected from the group consisting of Sn, Ta, Zr, Zn, Ti, Nb, Si, and Al.

### Claim 6 (depends on 1)

The reflective mask blank according to claim 1,
wherein the metal nitride in the conductive layer comprises at least one element selected from the group consisting of Cr, Ta, Ti, Zr, and Nb.

### Claim 7 (depends on 1)

The reflective mask blank according to claim 1,
wherein the conductive layer has a refractive index (n) at a wavelength of 532 nm of 3.5 or less and an absorption coefficient at a wavelength of 532 nm of 4.0 or less.

### Claim 8 (depends on 1)

The reflective mask blank according to claim 1,
wherein the backside conductive film has a sheet resistance (Rs) of 250 Ω/square or less.

### Claim 9 (depends on 1)

The reflective mask blank according to claim 1,
wherein the backside conductive film has transmittance over the wavelength range of 400 nm to 800 nm of 10% or more.

### Claim 10 (depends on 1)

The reflective mask blank according to claim 1, which comprises a reflective layer which reflects EUV light and an absorber layer which absorbs EUV light on/above a front surface of the substrate in this order from the substrate side.

### Claim 11 (depends on 10)

A reflective mask obtained by forming a pattern in the absorber layer of the reflective mask blank according to claim 10.