# US 2019/0055636 A1 · Method for making alloy matrix composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0055636 A1
- Document ID: US20190055636A1
- Status: Published application
- Kind: A1
- Application number: 15/869,567
- Filed: 2018-01-12
- Published: 2019-02-21
- Earliest claimed: 2017-08-17
- Assignees: Tsinghua University; Hon Hai Precision Industry Co., Ltd.
- Applicants: Tsinghua University; Hon Hai Precision Industry Co., Ltd.
- Inventors: LUN-QIAO XIONG; WEN-ZHEN LI; LIN ZHU
- Web page: https://patentgrep.com/patent/US20190055636A1

## CPC

- B32B 9/007: {comprising carbon, e.g. graphite, composite carbon}
- C22C 47/20: by subjecting to pressure and heat an assembly comprising at least one metal layer or sheet and one layer of fibres or filaments
- B32B 3/04: characterised by {at least one} layer folded at the edge, e.g. over another layer {; characterised by at least one layer enveloping or enclosing a material}
- B32B 5/16: characterised by features of a layer formed of particles, e.g. chips, powder {or granules (layer formed of natural mineral particles B32B19/00; layer being formed of wood fibres, chips or particles B32B21/02)}
- B32B 9/04: comprising such {particular} substance as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a glass layer B32B17/06; layered products with at least two ceramic layers composed mainly of ceramic B32B18/00)}
- B32B 9/041: {of metal}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- B32B 15/16: next to a particulate layer
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- C22C 1/1094: {comprising an after-treatment}
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- C22C 49/14: characterised by the fibres or filaments
- B32B 2255/06: on metal layer
- B32B 2255/205: Metallic coating
- B32B 2264/10: Inorganic particles
- B32B 2264/102: Oxide or hydroxide
- B32B 2307/402: Coloured
- B32B 2307/732: Dimensional properties
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C22C 2026/002: {Carbon nanotubes}
- C22C 2047/005: {Working of filaments or rods into fibre reinforced metal by mechanical deformation}
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method for making alloy matrix composite, comprising: providing a metal matrix composite, the metal matrix composite includes a metal body and a reinforcement body; placing an alloying element layer on a surface of the metal matrix composite to obtain a first composite structure; rolling the first composite structure to obtain a middle composite structure; repeatedly folding and rolling the middle composite structure to obtain a second composite structure; annealing the second composite structure to obtain the alloy matrix composite.

## Claims

### Claim 1

A method for making alloy matrix composite, comprising:
providing a metal matrix composite, wherein the metal matrix composite comprises at least one metal body and at least one reinforcement body;
placing an alloying element layer on a surface of the metal matrix composite to obtain a first composite structure;
rolling the first composite structure to obtain a middle composite structure;
repeatedly folding and rolling the middle composite structure to obtain a second composite structure;
annealing the second composite structure to obtain the alloy matrix composite.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal body is made of copper, aluminum, silver, or gold.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reinforcement body is made of carbon nanotube structure, graphene, particles of Al2O3 or Si3N4.

### Claim 4 (depends on 3)

The method of claim 3, wherein the carbon nanotube structure comprises a plurality of carbon nanotubes, wherein the plurality of carbon nanotubes is arranged in a disorder manner.

### Claim 5 (depends on 3)

The method of claim 3, wherein the carbon nanotube structure has a film structure.

### Claim 6 (depends on 5)

The method of claim 5, wherein the film structure comprises a drawn carbon nanotube film, a pressed carbon nanotube film, and a flocculated carbon nanotube film.

### Claim 7 (depends on 1)

The method of claim 1, wherein placing an alloying element layer on a surface of the metal matrix composite, comprises: stacking the alloying element layer on the surface of the metal matrix composite.

### Claim 8 (depends on 1)

The method of claim 1, wherein placing an alloying element layer on a surface of the metal matrix composite, comprises: plating the alloying element layer on the surface of the metal matrix composite by electroplating or electroless plating.

### Claim 9 (depends on 1)

The method of claim 1, wherein placing an alloying element layer on a surface of the metal matrix composite, comprises: folding the metal matrix composite and providing the alloying element layer between the folded metal matrix composite.

### Claim 10 (depends on 1)

The method of claim 1, before repeatedly folding and rolling the middle composite structure, roughening a surface of the middle composite structure.

### Claim 11 (depends on 1)

The method of claim 1, wherein the second composite structure comprises a plurality of sandwiched structures, the plurality of sandwiched structures is stacked one by one.

### Claim 12 (depends on 11)

The method of claim 11, wherein each of the plurality of sandwich structures comprises two layers of the metal matrix composite, and the alloy element layer are sandwiched between the two layers of the metal matrix composites.

### Claim 13 (depends on 1)

The method of claim 1, wherein the annealing temperature is in range from about 100° C. to about 600° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the annealing time is in range from about 1 hour to about 24 hours.