# US 2019/0055619 A1 · Method of producing grain-oriented electrical steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0055619 A1
- Document ID: US20190055619A1
- Status: Published application
- Kind: A1
- Application number: 16/079,669
- Filed: 2017-03-07
- Published: 2019-02-21
- Earliest claimed: 2016-03-09
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Takeshi IMAMURA; Minoru TAKASHIMA; Yuiko EHASHI; Yasuyuki HAYAKAWA
- Web page: https://patentgrep.com/patent/US20190055619A1

## CPC

- C21D 9/46: for sheet metals
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- H01F 1/14783: {with insulating coating}
- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- C21D 2201/05: Grain orientation
- C22C 2202/02: Magnetic
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

To provide a grain-oriented electrical steel sheet that has better magnetic property than conventional ones, in hot band annealing of the hot rolled steel sheet obtained by a predetermined step, an average heating rate from ordinary temperature to 400° C. is set to 50° C./s or more, and a time to reach 900° C. from 400° C. is set to 100 sec or less.

## Claims

### Claim 1

A method of producing a grain-oriented electrical steel sheet, comprising:
heating a steel slab at 1300° C. or less, the steel slab having a chemical composition containing
C: 0.002 mass % or more and 0.100 mass % or less,
Si: 2.00 mass % or more and 6.50 mass % or less,
Mn: 0.02 mass % or more and 1.00 mass % or less,
S: 50 mass ppm or less,
N: 50 mass ppm or less,
Se: 50 mass ppm or less,
acid-soluble Al: less than 100 mass ppm, and
a balance being Fe and inevitable impurities;
subjecting the steel slab to hot rolling, to obtain a hot rolled steel sheet;
subjecting the hot rolled steel sheet to hot band annealing;
subjecting the hot rolled steel sheet after the hot band annealing to cold rolling once, or twice or more with intermediate annealing performed therebetween, to obtain a cold rolled steel sheet having a final sheet thickness;
subjecting the cold rolled steel sheet to primary recrystallization annealing; and
applying an annealing separator to a surface of the cold rolled steel sheet after the primary recrystallization annealing, and thereafter subjecting the cold rolled steel sheet to secondary recrystallization annealing,
wherein in the hot band annealing, an average heating rate from ordinary temperature to 400° C. is set to 50° C./s or more, and a time to reach 900° C. from 400° C. is set to 100 sec or less.

### Claim 2 (depends on 1)

The method of producing a grain-oriented electrical steel sheet according to claim 1,
wherein the chemical composition further contains one or more selected from
Sb: 0.01 mass % or more and 0.50 mass % or less,
Sn: 0.01 mass % or more and 0.50 mass % or less,
Ni: 0.005 mass % or more and 1.5 mass % or less,
Cu: 0.005 mass % or more and 1.5 mass % or less,
Cr: 0.005 mass % or more and 0.1 mass % or less,
P: 0.005 mass % or more and 0.5 mass % or less,
Mo: 0.005 mass % or more and 0.5 mass % or less,
Ti: 0.0005 mass % or more and 0.1 mass % or less,
Nb: 0.0005 mass % or more and 0.1 mass % or less, and
Bi: 0.005 mass % or more and 0.1 mass % or less.