# US 2019/0053988 A1 · Method for producing cellulose fibers suitable for use in a thickening composition, method for producing a thickening composition, and method for thickening a composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0053988 A1
- Document ID: US20190053988A1
- Status: Published application
- Kind: A1
- Application number: 16/166,942
- Filed: 2018-10-22
- Published: 2019-02-21
- Earliest claimed: 2013-04-22
- Assignees: Nissan Chemical Industries, Ltd.
- Applicants: Nissan Chemical Industries, Ltd.
- Inventors: Hisato HAYASHI; Takehisa IWAMA
- Web page: https://patentgrep.com/patent/US20190053988A1

## CPC

- A61K 8/027: {Fibers; Fibrils}
- A61K 8/06: Emulsions
- A61K 8/20: Halogens; Compounds thereof
- A61K 8/23: Sulfur; Selenium; Tellurium; Compounds thereof
- A61K 8/24: Phosphorous; Compounds thereof
- A61K 8/27: Zinc; Compounds thereof
- A61K 8/345: {containing more than one hydroxy group}
- A61K 8/365: Hydroxycarboxylic acids; Ketocarboxylic acids
- A61K 8/44: Aminocarboxylic acids or derivatives thereof, e.g. aminocarboxylic acids containing sulfur; Salts; Esters or N-acylated derivatives thereof
- A61K 8/442: {substituted by amido group(s)}
- A61K 8/463: {containing sulfuric acid derivatives, e.g. sodium lauryl sulfate}
- A61K 8/466: {containing sulfonic acid derivatives; Salts}
- A61K 8/60: Sugars; Derivatives thereof
- A61K 8/602: {Glycosides, e.g. rutin}
- A61K 8/676: {Ascorbic acid, i.e. vitamin C}
- A61K 8/73: Polysaccharides
- A61K 8/731: {Cellulose; Quaternized cellulose derivatives}
- A61K 8/733: {Alginic acid; Salts thereof}
- A61K 8/736: {Chitin; Chitosan; Derivatives thereof}
- A61K 8/8147: {Homopolymers or copolymers of acids; Metal or ammonium salts thereof, e.g. crotonic acid, (meth)acrylic acid; Compositions of derivatives of such polymers}
- A61K 31/717: Celluloses
- A61K 45/06: Mixtures of active ingredients without chemical characterisation, e.g. antiphlogistics and cardiaca
- A61L 26/0004: {containing inorganic materials}
- A61L 26/0052: {Mixtures of macromolecular compounds}
- A61Q 19/00: Preparations for care of the skin
- C08L 1/02: Cellulose; Modified cellulose
- C08L 5/14: Hemicellulose; Derivatives thereof
- A61K 2800/10: General cosmetic use
- A61K 2800/412: Microsized, i.e. having sizes between 0.1 and 100 microns
- A61K 2800/48: Thickener, Thickening system
- A61K 2800/591: Mixtures of compounds not provided for by any of the codes A61K2800/592 - A61K2800/596
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- A61Q: SPECIFIC USE OF COSMETICS OR SIMILAR TOILETRY PREPARATIONS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Described are a method for producing cellulose fibers suitable for use in a thickening composition, a method for producing a thickening composition that contains the cellulose fibers, and a method for thickening a composition. The method for producing the cellulose fibers includes grinding a composition containing cellulose fibers and an aqueous solution to produce a dispersion containing cellulose fibers having an average fiber diameter (D) in a range of from 0.001 to 100 μm in the aqueous solution.

## Claims

### Claim 1

A method for producing cellulose fibers suitable for use in a thickening composition, the method comprising:
grinding a composition comprising cellulose fibers and an aqueous solution to produce a dispersion comprising cellulose fibers having an average fiber diameter (D) in a range of from 0.001 to 100 μm in the aqueous solution,
wherein the grinding does not comprise a chemical treatment of the cellulose material,
and the cellulose fibers comprise hemicellulose and amorphous regions.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the produced cellulose fibers have a ratio (L/D) of an average fiber length (L) to the average fiber diameter (D) in a range of from 5 to 500.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the produced cellulose fibers have an average fiber diameter (D) of 0.001 to 0.05 μm and a ratio (L/D) of an average fiber length (L) to the average fiber diameter (D) of 5 to 500.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the produced cellulose fibers have a crystallinity of less than 80%.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the grinding is performed using wet grinding.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the grinding comprises ejecting the composition from a pair of nozzles at a pressure in a range of from 150 to 250 MPa.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the grinding is performed at least 10 times.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the concentration of cellulose in the composition before grinding is in a range of from 0.1% to 30% by mass.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the concentration of cellulose is in the range of 0.1% to 10% by mass, and the aqueous solution is water.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the method further comprises dispersing cellulose fibers in the aqueous solution before the grinding.

### Claim 11 (depends on 1)

A method for producing a thickening composition, the method comprising:
obtaining a dispersion of cellulose fibers in an aqueous solution, the dispersion being produced by the method according to claim 1; and
adding an electrolyte to the dispersion to produce the thickening composition,
wherein the thickening composition comprises 0.0001 to 30 parts by mass of the electrolyte with respect to 1 part by mass of the cellulose fibers.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising adding at least one polar solvent to the obtained dispersion.

### Claim 13 (depends on 11)

The method according to claim 11, further comprising adding at least one polyalcohol to the obtained dispersion, an amount of the at least one polyalcohol to be added is in a range of from 1 part by mass to 100 parts by mass with respect to 1 part by mass of the cellulose fibers.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the produced thickening composition has a dynamic viscosity coefficient η′ measured in a cone plate at a dynamic displacement of 0.5 deg and a frequency of 1 Hz in a static state at 25° C. for 2 hours is at least 150% of η′ at 25° C. for 0 hour, a thickening composition containing 1% by mass of cellulose fibers and 0.01% by mass of an electrolyte is used to determine the dynamic viscosity.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the produced thickening composition is thixotropic.

### Claim 16 (depends on 11)

The method according to claim 11, the method comprising adjusting a pH of the produced thickening composition to be in a range of from 3 to 11.

### Claim 17 (depends on 11)

A method for producing a cosmetic, the method comprising:
obtaining a thickening composition produced according to claim 11, and
adding at least one surfactant or at least one oil component,
wherein an amount of the at least one oil component to be added is in a range of from 0.01% to 99% by mass with respect to the total mass of the cosmetic, and
an amount of the surfactant to be added is in a range of from 0.001% to 20% by mass with respect to the total mass of the cosmetic.

### Claim 18

A method for thickening a composition, the method comprising:
obtaining a thickening composition comprising:
an electrolyte; and
cellulose fibers having an average fiber diameter (D) of 0.001 to 100 μm and comprising hemicellulose and amorphous regions;
obtaining a composition to be thickened; and
thickening the composition to be thickened by forming a homogenous mixture comprising the thickening composition and the composition to be thickened.

### Claim 19 (depends on 18)

The method according to claim 18, wherein
a ratio (L/D) of an average fiber length (L) to the average fiber diameter (D) is 5 to 500;
the cellulose has a crystallinity of less than 80%; and
an amount of the electrolyte in the thickening composition is in a range of from 0.0001 parts by mass to 30 parts by mass with respect to 1 part by mass of the cellulose fibers.

### Claim 20 (depends on 18)

The method according to claim 18, wherein
the cellulose fibers in the thickening composition are kraft pulp; and
the thickening results in forming a gelled composition that is thixotropic.