# US 2019/0027633 A1 · Fabricating thin-film optoelectronic devices with modified surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0027633 A1
- Document ID: US20190027633A1
- Status: Published application
- Kind: A1
- Application number: 16/144,636
- Filed: 2018-09-27
- Published: 2019-01-24
- Earliest claimed: 2014-05-23
- Assignees: Flisom AG; Empa
- Applicants: Flisom AG; Empa
- Inventors: Patrick REINHARD; Fabian PIANEZZI; Benjamin BISSIG; Stephan BUECHELER; Ayodhya Nath TIWARI
- Web page: https://patentgrep.com/patent/US20190027633A1

## CPC

- H10F 71/128: {Annealing}
- H10F 10/167: comprising Group I-III-VI materials, e.g. CdS/CuInSe2 [CIS] heterojunction photovoltaic cells
- H10F 19/30: comprising thin-film photovoltaic cells
- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- H10F 77/1265: {characterised by the dopants}
- H10F 77/148: {Shapes of potential barriers}
- H10F 77/1698: {the metallic or insulating substrates being flexible}
- H10F 77/211: {for photovoltaic cells}
- H10P 14/3241: {being conductive materials}
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- Y02E 10/541: CuInSe2 material PV cells
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method (200) for fabricating thin-film optoelectronic devices (100), the method comprising: providing a substrate (110), forming a back-contact layer (120); forming at least one absorber layer (130) made of an ABC chalcogenide material, adding at least one alkali metal (235), and forming at least one cavity (236, 610, 612, 613) at the surface of the absorber layer wherein forming of said at least one cavity is by dissolving away from said surface of the absorber layer at least one crystal aggregate comprising at least one alkali crystal comprising at least one alkali metal. The method (200) is advantageous for more environmentally-friendly production of photovoltaic devices (100) on flexible substrates with high photovoltaic conversion efficiency and faster production rate.

## Claims

### Claim 1

A thin-film optoelectronic device, comprising:
a substrate;
a back-contact layer;
an absorber layer comprising:
an ABC chalcogenide material, wherein A represents one or more elements selected from a group consisting of Cu and Ag, B represents one or more elements selected from a group consisting of In, Ga, and Al, and C represents one or more elements selected from a group consisting of S, Se, and Te;
one or more alkali metals; and
a plurality of cavities.

### Claim 2 (depends on 1)

The device of claim 1, wherein the plurality of cavities are formed at a first surface of the absorber layer.

### Claim 3 (depends on 2)

The device of claim 2, further comprising a front-contact layer, wherein the absorber layer is disposed between the front-contact layer and the back-contact layer and the first surface faces the front-contact layer.

### Claim 4 (depends on 2)

The device of claim 2, wherein the plurality of cavities cover between about 15% and about 80% of the first surface of the absorber layer.

### Claim 5 (depends on 1)

The device of claim 1, wherein the plurality of cavities have an average depth of at least 50 nm.

### Claim 6 (depends on 1)

The device of claim 1, wherein the plurality of cavities have a shape formed from dissolving a crystal that included at least one of the one or more alkali metals.

### Claim 7 (depends on 1)

The device of claim 1, wherein the one or more alkali metals comprises potassium.

### Claim 8 (depends on 7)

The device of claim 7, wherein the one or more alkali metals further comprises sodium.

### Claim 9 (depends on 1)

The device of claim 1, wherein
the one or more alkali metals comprises potassium, and
the absorber layer comprises a first surface, and
a sputter depth profile of the absorber layer comprises an upper peak for counts of potassium at a depth ranging from a first surface of the absorber layer to a depth of about 0.5 μm from the first surface.

### Claim 10 (depends on 9)

The device of claim 9, wherein the upper peak of potassium on the sputter depth profile comprises a base having a width in a range from about 0.1 μm to about 0.5 μm.

### Claim 11 (depends on 1)

The device of claim 1, wherein
the one or more alkali metals comprises potassium,
a curve for a copper to selenium content in an energy dispersive X-ray line scan graph of the absorber layer comprises an extended region of low and about constant Cu/Se extending from a first surface of the absorber layer into a first portion of a depth of the absorber layer, and
the first portion has a depth in a range from about 0.05 μm to about 0.5 μm from the first surface.

### Claim 12 (depends on 1)

The device of claim 1, wherein
the one or more alkali metals comprises potassium,
the absorber layer further comprises +1/+2 elements, and
an X-ray photoelectron spectrometry curve of the absorber layer comprises a Cd 3d5/2 peak that is at least about 60% greater in height than for a curve of a corresponding absorber layer that does not comprise potassium.

### Claim 13 (depends on 1)

The device of claim 1, wherein the plurality of cavities have a mean cavity area in a range from about 0.1×10−15 m2 to about 0.8×10−15 m2.

### Claim 14 (depends on 1)

The device of claim 1, wherein the absorber layer includes a plurality of walls forming the plurality of cavities and the plurality of walls comprise cadmium.

### Claim 15

A thin-film optoelectronic device, comprising:
a substrate;
a back-contact layer;
a front-contact layer;
an absorber layer disposed between the front-contact layer and the back-contact layer, the absorber layer comprising:
an ABC chalcogenide material, wherein A represents one or more elements selected from a group consisting of Cu and Ag, B represents one or more elements selected from a group consisting of In, Ga, and Al, and C represents one or more elements selected from a group consisting of S, Se, and Te;
one or more alkali metals including potassium; and
a first surface facing the front-contact layer, wherein the first surface includes a plurality of cavities.

### Claim 16 (depends on 15)

The device of claim 15, wherein the plurality of cavities cover between about 25% and about 45% of the first surface of the absorber layer.

### Claim 17 (depends on 15)

The device of claim 15, wherein the plurality of cavities have an average depth of at least 50 nm.

### Claim 18 (depends on 15)

The device of claim 15, wherein the one or more alkali metals further comprises sodium.

### Claim 19 (depends on 15)

The device of claim 15, wherein the plurality of cavities have a mean cavity area in a range from about 0.1×10−15 m2 to about 0.8×10−15 m2.

### Claim 20 (depends on 15)

The device of claim 15, wherein the absorber layer includes a plurality of walls forming the plurality of cavities and the plurality of walls comprise cadmium.