# US 2019/0010356 A1 · Hard abrasive particle-free polishing of hard materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0010356 A1
- Document ID: US20190010356A1
- Status: Published application
- Kind: A1
- Application number: 15/645,777
- Filed: 2017-07-10
- Published: 2019-01-10
- Earliest claimed: 2017-07-10
- Assignees: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Applicants: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Inventors: RAJIV K. SINGH; ARUL ARJUNAN; DEEPIKA SINGH; CHAITANYA GINDE; PUNEET N. JAWALI
- Web page: https://patentgrep.com/patent/US20190010356A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 37/00: Lapping machines or devices; Accessories (B24B3/00 takes precedence)
- B24B 37/044: {characterised by the composition of the lapping agent}
- C09G 1/04: Aqueous dispersions (C09G1/02 takes precedence)
- C09K 3/1409: {Abrasive particles per se (preparation of diamond C01B32/25)}
- H10P 52/402: {of semiconductor materials}
- H10P 52/403: {of conductive or resistive materials}
- H10P 90/129: {by polishing}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of CMP includes providing a slurry solution including ≥1 per-compound oxidizer in a concentration between 0.01 M and 2 M with a pH from 2 to 5 or 8 to 11, and ≥1 buffering agent which provides a buffering ratio ≥1.5 that compares an amount of a strong acid needed to reduce the pH from 9.0 to 3.0 as compared to an amount of strong acid to change the pH from 9.0 to 3.0 without the buffering agent. The slurry solution is exclusive any hard slurry particles or has only soft slurry particles that have throughout a Vickers hardness <300 Kg/mm2 or Mohs Hardness <4. The slurry solution is dispensed on a hard surface having a Vickers hardness >1,000 kg/mm2 is pressed by a polishing pad with the slurry solution in between while rotating the polishing pad relative to the hard surface.

## Claims

### Claim 1

A slurry for chemical-mechanical polishing (CMP), comprising:
an aqueous medium;
at least one per-compound oxidizer with a concentration between 0.01 M and 2.0 M;
a pH level from 2 to 5 or from 8 to 11;
at least one buffering agent different from said per-compound oxidizer that provides a buffering ratio of at least 1.5 which compares an amount of a strong acid needed to reduce said pH level from 9.0 to 3.0 with said buffering agent in a slurry solution comprising said aqueous medium and said per-compound oxidizer as compared to an amount of said strong acid needed to change reduce said pH level from 9.0 to 3.0 in said slurry solution without said buffering agent;
wherein said slurry is exclusive of any hard slurry particles, or has only soft slurry particles that have throughout a Vickers hardness less than 300 Kg/mm2 or a Mohs Hardness less than (<) 4.

### Claim 2 (depends on 1)

The slurry of claim 1, wherein said slurry solution further comprises transition metal ions in a concentration from 0.03 M to 1 M in addition to any transition metals ions that may be in said per-compound oxidizer.

### Claim 3 (depends on 1)

The slurry of claim 1, wherein said slurry includes said soft slurry particles which comprise a metal oxide formed in-situ in said slurry solution from a decomposition of said per-compound oxidizer.

### Claim 4 (depends on 1)

The slurry of claim 1, wherein said buffering agent comprises at least one of a surfactant and at least 2 different valences states of Mn ions including said per-compound oxidizer chosen from +7, +4, +2, and +3.

### Claim 5 (depends on 1)

The slurry of claim 1, wherein said per-compound oxidizer comprises potassium permanganate or sodium permanganate.

### Claim 6 (depends on 4)

The slurry of claim 4, wherein said buffering agent comprises said surfactant.

### Claim 7 (depends on 1)

The slurry of claim 1, wherein said slurry further comprises at least one alkali metal ion besides alkali metal ion in said per-compound oxidizer if said per-compound oxidizer includes an alkali metal ion.

### Claim 8

A method of chemical mechanical polishing (CMP) hard surfaces, comprising:
providing a slurry solution comprising:
an aqueous medium;
at least one per-compound oxidizer with a concentration between 0.01 M and 2 M;
a pH level from 2 to 5 or from 8 to 11;
at least one buffering agent different from said per-compound oxidizer that provides a buffering ratio of at least 1.5 which compares an amount of a strong acid needed to reduce said pH level from 9.0 to 3.0 with said buffering agent in said slurry solution as compared to an amount of said strong acid needed to change reduce said pH level from 9.0 to 3.0 in said slurry solution without said buffering agent;
said slurry solution being exclusive any hard slurry particles or having only soft slurry particles that have throughout a Vickers hardness less than 300 Kg/mm2 or a Mohs Hardness less than (<) 4,
dispensing said slurry solution on a hard surface having a Vickers hardness >1,000 kg/mm2, and
pressing with a polishing pad with said slurry solution on said hard surface in between while rotating said polishing pad relative to said hard surface.

### Claim 9 (depends on 8)

The method of claim 8, wherein said hard surface comprises a carbide, a nitride, or a mixture thereof.

### Claim 10 (depends on 8)

The method of claim 8, wherein said slurry solution further comprises transition metal ions in a concentration from 0.03 M to 1 M in addition to any transition metals ions that may be in said per-compound oxidizer.

### Claim 11 (depends on 8)

The method of claim 8, wherein said polishing pad comprise a polymeric pad having a Shore D hardness less than 100, wherein a polishing pressure used for said pressing is less than 15 psi.

### Claim 12 (depends on 8)

The method of claim 8, wherein said slurry solution further includes said soft slurry particles which comprise a metal oxide formed in-situ in said slurry solution from a decomposition of said per-compound oxidizer.

### Claim 13 (depends on 8)

The method of claim 8, wherein said buffering agent comprises at least one of a surfactant and at least 2 different valences states of Mn ions including said per-compound oxidizer chosen from +7, +4, +2, and +3.

### Claim 14 (depends on 8)

The method of claim 8, wherein said per-compound oxidizer comprises potassium permanganate or sodium permanganate.

### Claim 15 (depends on 13)

The method of claim 13, wherein said buffering agent comprises said surfactant.

### Claim 16 (depends on 8)

The method of claim 8, wherein said slurry solution further comprises at least one alkali metal ion besides an alkali metal ion in said per-compound oxidizer if said per-compound oxidizer includes an alkali metal ion.