# US 2018/0375978 A1 · Film for applying compressive stress to ceramic materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0375978 A1
- Document ID: US20180375978A1
- Status: Published application
- Kind: A1
- Application number: 16/015,428
- Filed: 2018-06-22
- Published: 2018-12-27
- Earliest claimed: 2017-06-23
- Assignees: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Applicants: Sinmat, Inc.; University of Florida Research Foundation, Inc.
- Inventors: RAJIV K. SINGH; DEEPIKA SINGH
- Web page: https://patentgrep.com/patent/US20180375978A1

## CPC

- H04M 1/0266: {for a display module assembly}
- B32B 7/02: Physical, chemical or physicochemical properties
- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- C03C 17/225: {Nitrides}
- C23C 14/0676: {Oxynitrides}
- C23C 16/308: {Oxynitrides}
- C30B 29/20: Aluminium oxides
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- C03C 2217/28: Other inorganic materials
- C03C 2217/281: Nitrides
- C03C 2218/322: Oxidation
- C04B 2111/805: {Transparent material}
- G06F 1/1637: {Details related to the display arrangement, including those related to the mounting of the display in the housing}
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)

## Abstract

A method to provide compressive stress to substrates includes depositing a film on a ceramic substrate at a deposition temperature (Td) to form an article, the film having a difference relative to the ceramic substrate at Td in a coefficient thermal expansion (CTE) of at least 1.0×10−6/K and a difference in a refractive index >0.10. At least a portion of the thickness the film is converted in at least one of composition, phase and microstructure by lowering or raising the temperature from Td to reach a changed temperature (Tc) that is at least 100° C. different from Td. The film converting conditions result in the converted film portion providing a difference in refractive index at the Tc between the converted film and the ceramic substrate of ≤|0.10|. The temperature of the article is then lowered to room temperature.

## Claims

### Claim 1

A method to provide compressive stress to substrates, comprising:
depositing a film on a ceramic substrate at a deposition temperature (Td) to form an article, said film having a difference in a coefficient thermal expansion (CTE) relative to said ceramic substrate at said Td of at least 1.0×10−6/K and a difference in a refractive index of greater than (>) 0.10;
converting said film comprising lowering or raising a temperature from said Td to reach a changed temperature (Tc) that is at least 100° C. different from said Td, wherein conditions for said converting result in said film becoming in at least a portion of its thickness a converted film in at least one of (i) composition change such that there is at least one of an increase in oxygen content by at least (≥) 10 mole percent, a decrease in nitrogen content by at least (≥) 10 mole percent, a decrease in carbon content by at least (≥) 10 mole percent, (ii) a change in phase, and (iii) a microstructure change with an average grain size increase of at least (≥) 20 percent, so that a difference in said refractive index at said Tc of said converted film and said ceramic substrate is ≤|0.10|, and
lowering a temperature of said article from said Tc to room temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein said substrate comprises sapphire and wherein said film before said converting comprises AlON, ALN, or SiON.

### Claim 3 (depends on 1)

The method of claim 1, when said converting comprises flowing one or more of carbon, oxygen or nitrogen containing gases.

### Claim 4 (depends on 1)

The method of claim 1, wherein said article is optically transparent.

### Claim 5 (depends on 1)

The method of claim 1, wherein said substrate comprises a silica-based glass, sapphire, alumina, or a spinel.

### Claim 6 (depends on 1)

The method of claim 1, wherein said portion of said converted film is under a compressive stress, and wherein said substrate is under a tensile stress.

### Claim 7 (depends on 1)

The method of claim 1, wherein said article comprises a display screen of a cellular phone.

### Claim 8 (depends on 1)

The method of claim 1, wherein said portion of said converted film is from 10% to 80%.

### Claim 9 (depends on 1)

The method of claim 1, wherein after said converting said difference in said refractive index of said film and said ceramic substrate is ≤|0.05|.

### Claim 10 (depends on 1)

The method of claim 1, wherein after said converting a compressive stress in said film is 1 Mpa to 10 GPa.

### Claim 11 (depends on 1)

The method of claim 1, wherein after said converting said film includes at least 10 percent aluminum.

### Claim 12

A cellular phone, comprising:
a radio frequency (RF) part coupled to an antenna including a transceiver, an RF frequency up converter and RF frequency down converter and coupled by a Digital-to-Analog Converter (DAC) and an Analog-to-Digital Converter (ADC) to at least one processor;
wherein a transparent display screen for said cellular phone includes a transparent film that in at least a portion of its thickness that comprises a material different in at least one of composition and phase from an underlining transparent ceramic substrate,
wherein a difference in a refractive index of said film and said ceramic substrate is ≤|0.10|.

### Claim 13 (depends on 12)

The cellular phone of claim 12, wherein said difference in said refractive index said film and said ceramic substrate is ≤|0.05|.

### Claim 14 (depends on 12)

The cellular phone of claim 12, wherein said portion of said film is under compressive stress, and wherein said substrate is under tensile stress.

### Claim 15 (depends on 12)

The cellular phone of claim 12,
wherein said ceramic substrate comprises a single crystal sapphire substrate with a thickness ranging from 100 microns to 3 mm;
wherein said portion of said film comprises alpha alumina or an AlON polycrystalline phase, and
wherein a compressive stress in said film is 1 Mpa to 10 GPa.

### Claim 16 (depends on 12)

The cellular phone of claim 12, wherein said ceramic substrate is sapphire.

### Claim 17 (depends on 12)

The cellular phone of claim 12, wherein said film includes at least 10 percent aluminum.