# US 2018/0370273 A1 · Process for protecting a document, protective device comprising an adhesive layer and document

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0370273 A1
- Document ID: US20180370273A1
- Status: Published application
- Kind: A1
- Application number: 16/062,527
- Filed: 2016-12-15
- Published: 2018-12-27
- Earliest claimed: 2015-12-16
- Assignees: Fasver
- Applicants: Fasver
- Inventors: Eric Philippe; Laurence Bes
- Web page: https://patentgrep.com/patent/US20180370273A1

## CPC

- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B42D 25/351: Translucent or partly translucent parts, e.g. windows
- B42D 25/455: using heat
- B42D 25/465: using chemicals or adhesives
- C09J 5/06: involving heating of the applied adhesive
- C09J 7/35: Heat-activated
- B32B 2307/412: Transparent
- B41M 7/0027: {using protective coatings or layers by lamination or by fusion of the coatings or layers}
- C09J 2203/338: as tamper-evident tape or label
- C09J 2467/00: Presence of polyester
- C09J 2467/006: in the substrate
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B42D: BOOKS; BOOK COVERS; LOOSE LEAVES; PRINTED MATTER CHARACTERISED BY IDENTIFICATION OR SECURITY FEATURES; PRINTED MATTER OF SPECIAL FORMAT OR STYLE NOT OTHERWISE PROVIDED FOR; DEVICES FOR USE THEREWITH AND NOT OTHERWISE PROVIDED FOR; MOVABLE-STRIP WRITING OR READING APPARATUS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

The invention relates to a process for protecting variable inscriptions of a document in which: a transparent film is bonded to a face of said document with a view to protecting variable inscriptions of said document, by at least one adhesive layer comprising at least one thermoplastic polymer having a glass transition temperature between 40° C. and 110° C. and having a hydroxyl value between 3 mg of KOH/g and 60 mg of KOH/g and/or an acid value between 2 mg of KOH/g and 150 mg of KOH/g, said adhesive layer comprises a crosslinking agent having at least 2.8 functions selected from the group formed of isocyanates, carbodiimides, aziridines and alkoxysilanes, during the bonding, a crosslinking of said adhesive layer is carried out. The invention also relates to a protective device and to a document.

## Claims

### Claim 1

A process for protecting a document, comprising:
bonding a transparent film to a face of said document with a view to protecting variable inscriptions of said document, by at least one adhesive layer comprising at least one thermoplastic polymer, wherein said thermoplastic polymer is chosen from the group made up of thermoplastic polymers having a hydroxyl number, measured according to the standard DIN 53 240/2, of between 3 mg of KOH/g and 60 mg of KOH/g, thermoplastic polymers having an acid number, measured according to the standard DIN EN ISO 2114, of between 2 mg of KOH/g and 150 mg of KOH/g, copolymers thereof and blends thereof,
wherein said thermoplastic polymer has a glass transition temperature, measured by differential scanning calorimetry, of between 40° C. and 110° C.,
wherein said adhesive layer also comprises at least one crosslinking agent, each crosslinking agent: being chosen from the group of aliphatic compounds comprising between 4 and 50 carbon atoms, having on average at least 2.8 functions, chosen from the group made up of isocyanates, carbodiimides, aziridines and alkoxysilanes, per molecule of crosslinking agent,
wherein, during the bonding of said transparent film to said document, crosslinking of said thermoplastic polymer and of said crosslinking agent of the adhesive layer is carried out.

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein, prior to crosslinking of said thermoplastic polymer and of said crosslinking agent, said adhesive layer comprises 0.5% to 10% by weight of crosslinking agent relative to the total weight of said thermoplastic polymer.

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein said crosslinking of said adhesive layer is carried out at a temperature of between 60° C. and 220° C.

### Claim 4 (depends on 1)

The process as claimed in claim 1, further comprising hot laminating, under pressure, said document coated with said transparent film.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein said thermoplastic polymer is chosen from the group of thermoplastic polymers having, before said crosslinking, a weight-average molecular weight, measured by size exclusion chromatography, of between 3000 g/mol and 65 000 g/mol.

### Claim 6

A protective device for a document having variable inscriptions to be protected, said protective device comprising:
at least one transparent film bearing at least one adhesive layer comprising at least one thermoplastic polymer,
wherein said thermoplastic polymer is chosen from the group made up of thermoplastic polymers having a hydroxyl number, measured according to the standard DIN 53 240/2, of between 3 mg of KOH/g and 60 mg of KOH/g, thermoplastic polymers having an acid number, measured according to the standard DIN EN ISO 2114, of between 2 mg of KOH/g and 150 mg of KOH/g, copolymers thereof and blends thereof,
wherein said thermoplastic polymer has a glass transition temperature, measured by differential scanning calorimetry, between 40° C. and 110° C., and
wherein adhesive layer also comprises at least one crosslinking agent, each crosslinking agent chosen from the group of aliphatic compounds comprising between 4 and 50 carbon atoms, having on average at least 2.8 functions, chosen from the group made up of isocyanates, carbodiimides, aziridines and alkoxysilanes, per molecule of crosslinking agent.

### Claim 7 (depends on 6)

The device as claimed in claim 6, wherein said adhesive layer comprises between 0.5% and 10% by weight of crosslinking agent relative to the total weight of said thermoplastic polymer.

### Claim 8 (depends on 6)

The device as claimed in claim 6, wherein said transparent film comprises a plurality of superimposed layers.

### Claim 9 (depends on 6)

The device as claimed in claim 6, wherein said transparent film comprises at least one layer, in particular at least one thermoplastic extreme layer.

### Claim 10 (depends on 6)

The device as claimed in claim 6, wherein said thermoplastic polymer is chosen from the group made up of thermoplastic polymers having a weight-average molecular weight, measured by size exclusion chromatography, of between 3000 g/mol and 65 000 g/mol.

### Claim 11 (depends on 6)

The device as claimed in claim 6, wherein said adhesive layer comprises at least one thermoplastic material chosen from the group made up of polyurethanes, polyesters, polyacrylics, polyethers, polyvinyl butyrals, polyvinyl acetals, cellulose, copolymers thereof and blends thereof.

### Claim 12

A document comprising:
a base sheet;
variable inscriptions associated with said base sheet; and
at least one adhesive layer comprising at least one thermoplastic polymer, said adhesive layer extending in contact with an extreme layer of said base sheet,
wherein said thermoplastic polymer is chosen from the group made up of thermoplastic polymers having a hydroxyl number, measured according to standard DIN 53 240/2, of between 3 mg of KOH/g and 60 mg of KOH/g, thermoplastic polymers having an acid number, measured according to the standard DIN EN ISO 2114, of between 2 mg of KOH/g and 150 mg of KOH/g, copolymers thereof and blends thereof,
wherein said thermoplastic polymer has a glass transition temperature, measured by differential scanning calorimetry, of between 40° C. and 110° C., and
wherein said adhesive layer also comprises at least one crosslinking agent, each crosslinking agent: being chosen from the group of aliphatic compounds comprising between 4 and 50 carbon atoms, having on average at least 2.8 functions, chosen from the group made up of isocyanates, carbodiimides, aziridines and alkoxysilanes, per molecule of crosslinking agent.

### Claim 13 (depends on 12)

The document as claimed in claim 12, wherein at least one transparent film extends in contact with said adhesive layer.