# US 2018/0323469 A1 · Method for preparing solid electrolyte and all solid state battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323469 A1
- Document ID: US20180323469A1
- Status: Published application
- Kind: A1
- Application number: 15/830,224
- Filed: 2017-12-04
- Published: 2018-11-08
- Earliest claimed: 2017-05-08
- Assignees: Hyundai Motor Company; Kia Motors Corporation; Korea Institute of Science and Technology
- Applicants: Hyundai Motor Company; Kia Motors Corporation; Korea Institute of Science and Technology
- Inventors: Jae Min Lim; Ju Yeong Seong; Yong Jun Jang; Hun Gi Jung; Hyoung Chul Kim; Eu Deum Jung; Bin Na Yoon
- Web page: https://patentgrep.com/patent/US20180323469A1

## CPC

- H01M 10/0562: Solid materials
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for preparing a solid electrolyte for an all-solid state battery, may include obtaining a slurry by dispersing a first raw material comprising lithium sulfide; and a second raw material selected from the group consisting of silicon sulfide, phosphorus sulfide, germanium sulfide, boron sulfide, and a combination thereof in a solvent; and drying the slurry.

## Claims

### Claim 1

A method for preparing a solid electrolyte for an all-solid state battery, the method comprising:
obtaining a slurry by dispersing a first raw material comprising lithium sulfide; and a second raw material selected from the group consisting of silicon sulfide, phosphorus sulfide, germanium sulfide, boron sulfide, and a combination thereof in a solvent; and
drying the slurry.

### Claim 2 (depends on 1)

The method of claim 1, wherein the method does not comprise milling the first raw material and the second raw material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the slurry is obtained by further dispersing a third raw material comprising any one or more of a transition metal element and a halogen element in the solvent.

### Claim 4 (depends on 1)

The method of claim 1, wherein the solvent is selected from the group consisting of an ester-based solvent, an ether-based solvent, and a combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the solvent is selected from the group consisting of methyl propionate, ethyl propionate, propyl propionate, and a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the drying is carried out under a vacuum or inert gas atmosphere.

### Claim 7 (depends on 1)

The method of claim 1, wherein the drying is carried out at a temperature of about 100° C. to about 200° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the solid electrolyte is a sulfide-based solid electrolyte comprising at least lithium (Li), phosphorus (P), and sulfur (S).

### Claim 9 (depends on 1)

The method of claim 1, wherein the solid electrolyte comprises Li2S—P2S5.

### Claim 10 (depends on 1)

A method for preparing an all-solid state battery, the method comprising:
adding a positive electrode active material to the slurry obtained by dispersing the first raw material and the second raw material of claim 1 in a solvent and mixing the mixture;
obtaining a composite powder comprising a solid electrolyte and a positive electrode active material by drying the slurry; and
forming a positive electrode by hot-pressing the composite powder.

### Claim 11 (depends on 10)

The method of claim 10, wherein one selected from the group consisting of a conductive material, a binder, and a combination thereof is further added to the slurry and the mixture is mixed.

### Claim 12 (depends on 10)

The method of claim 10, wherein the method does not comprise milling the first raw material, the second raw material, and the positive electrode active material.

### Claim 13 (depends on 10)

The method of claim 10, wherein the positive electrode active material is selected from the group consisting of a lithium metal oxide having a layered structure, a lithium metal oxide having a spinel structure, a lithium metal phosphorus oxide having an olivine structure, and a combination thereof.

### Claim 14 (depends on 10)

The method of claim 10, wherein the solvent is selected from the group consisting of methyl propionate, ethyl propionate, propyl propionate, and a combination thereof.

### Claim 15 (depends on 10)

The method of claim 10, wherein the drying is carried out at a temperature of about 100° C. to about 200° C. under a vacuum or inert gas atmosphere.

### Claim 16 (depends on 11)

The method of claim 11, wherein the composite powder comprises a positive electrode active material, a solid electrolyte, and a conductive material at a mass ratio of 65 to 80:10 to 25:10 to 20.

### Claim 17 (depends on 10)

The method of claim 10, wherein the hot-pressing is carried out at a temperature of about 100° C. to about 200° C. for about 5 minutes to about 60 minutes.

### Claim 18 (depends on 10)

The method of claim 10, wherein the hot-pressing is carried out under a pressure of about 1 ton to about 10 tons.

### Claim 19 (depends on 10)

The method of claim 10, wherein a positive electrode-electrolyte layer composite is formed by
applying the composite powder in a mold;
applying an electrolyte powder onto the composite powder; and
hot-pressing the composite powder and the electrolyte powder.

### Claim 20 (depends on 19)

The method of claim 19, wherein the electrolyte powder is selected from the group consisting of an oxide-based solid electrolyte powder, a sulfide-based solid electrolyte powder, and a combination thereof.