# US 2018/0323428 A1 · Cathode active material for non-aqueous electrolyte secondary battery and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323428 A1
- Document ID: US20180323428A1
- Status: Published application
- Kind: A1
- Application number: 16/034,586
- Filed: 2018-07-13
- Published: 2018-11-08
- Earliest claimed: 2013-05-22
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Tomoko NAKAYAMA; Rei KOKADO; Kensaku MORI
- Web page: https://patentgrep.com/patent/US20180323428A1

## CPC

- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01B 1/08: oxides
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/30: Three-dimensional structures
- C01P 2002/76: by a space-group or by other symmetry indications
- C01P 2006/12: Surface area
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/052: Li-accumulators
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The purpose of the present invention is to easily provide at low cost, a cathode active material for non-aqueous electrolyte secondary batteries, which exhibits high particle strength and high weather resistance, while enabling achievement of excellent charge and discharge capacity and excellent output characteristics in cases where the cathode active material is used as a cathode material of a non-aqueous electrolyte secondary battery. A slurry of from 500 g/L to 2000 g/L is formed by adding water to a powder of a lithium nickel composite oxide represented by the general formula (A): LizNi1-x-yCoxMyO2, where 0.10≤x≤0.20, 0≤y≤0.10, 0.97≤z≤1.20, and M represents at least one element selected from among Mn, V, Mg, Mo, Nb, Ti and Al); the slurry is washed with water by stirring; and after filtration, the resulting material is subjected to a heat treatment at a temperature of from 120° C. to 550° C. (inclusive) in an oxygen atmosphere having an oxygen concentration of 80% by volume or more.

## Claims

### Claim 1

A manufacturing method for manufacturing a cathode active material for a non-aqueous electrolyte secondary battery, comprising steps of forming a 500 g/L to 2000 g/L slurry by adding water to a powder of a lithium nickel composite oxide that is represented by a general formula (A): LizNi1-x-yCoxMyO2, where 0.10≤x≤0.20, 0≤y≤0.10, 0.97≤z≤1.20, and M is at least one element that is selected from among Mn, V, Mg, Mo, Nb, Ti and Al; washing the slurry by mixing; filtering the slurry; and performing heat treatment at a temperature of no less than 120° C. and no greater than 550° C. in an oxygen atmosphere having an oxygen concentration of 80% by volume or more.

### Claim 2 (depends on 1)

The manufacturing method for manufacturing a cathode active material for a non-aqueous electrolyte secondary battery according to claim 1, wherein a temperature of the water that is used during the washing process is 10° C. to 50° C.

### Claim 3 (depends on 1)

The manufacturing method for manufacturing a cathode active material for a non-aqueous electrolyte secondary battery according to claim 1, wherein the temperature during the heat treatment is 120° C. or greater but less than 400° C.

### Claim 4 (depends on 1)

The manufacturing method for manufacturing a cathode active material for a non-aqueous electrolyte secondary battery according to claim 1, wherein a rate of temperature rise during the heat treatment is 2° C./min to 10° C./min.

### Claim 5 (depends on 1)

The manufacturing method for manufacturing a cathode active material for a non-aqueous electrolyte secondary battery according to claim 1, wherein a moisture content of the cathode active material after the heat treatment is 0.2% by mass or less.