# US 2018/0323424 A1 · Negative electrode active material, mixed negative electrode active material, negative electrode for nonaqueous electrolyte secondary battery, lithium ion secondary battery, production method of negative electrode active material, and production method of lithium ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323424 A1
- Document ID: US20180323424A1
- Status: Published application
- Kind: A1
- Application number: 15/772,623
- Filed: 2016-10-31
- Published: 2018-11-08
- Earliest claimed: 2015-11-18
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Takakazu HIROSE; Hiromichi KAMO
- Web page: https://patentgrep.com/patent/US20180323424A1

## CPC

- H01M 4/364: {as mixtures}
- C01B 33/32: Alkali metal silicates ({C01B33/24} , C01B33/26 take precedence)
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/66: Selection of materials
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/86: by NMR- or ESR-data
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A negative electrode active material comprising: particles of negative electrode active material, wherein the particles of negative electrode active material contain particles of silicon compound containing a silicon compound (SiOx:0.5≤x≤1.6), and wherein the particles of silicon compound have, as chemical shift values obtained from a 29Si-MAS-NMR spectrum, an intensity A of a peak derived from amorphous silicon obtained in −40 to −60 ppm, an intensity B of a peak derived from silicon dioxide obtained in the vicinity of −110 ppm, and an intensity C of a peak derived from Si obtained in the vicinity of −83 ppm, which satisfy the following formula 1 and formula 2. B≤1.5×A (1) B<C (2)

## Claims

### Claim 1

A negative electrode active material comprising:
particles of negative electrode active material,
wherein the particles of negative electrode active material contain particles of silicon compound containing a silicon compound (SiOx:0.5≤x≤1.6), and
wherein the particles of silicon compound have, as chemical shift values obtained from a 29Si-MAS-NMR spectrum, an intensity A of a peak derived from amorphous silicon obtained in −40 to −60 ppm, an intensity B of a peak derived from silicon dioxide obtained in the vicinity of −110 ppm, and an intensity C of a peak derived from Si obtained in the vicinity of −83 ppm, which satisfy the following formula 1 and formula 2.
B≤1.5×A (1)
B<C (2)

### Claim 2 (depends on 1)

The negative electrode active material according to claim 1, wherein the particles of negative electrode active material contain at least one kind or more of Li2SiO3 and Li4SiO4.

### Claim 3 (depends on 1)

The negative electrode active material according to claim 1, wherein the chemical shift value obtained from the 29Si-MAS-NMR spectrum has a peak in the vicinity of −130 ppm.

### Claim 4 (depends on 1)

The negative electrode active material according to claim 1, wherein the particles of silicon compound have a half value width (2θ) of a diffraction peak derived from a Si(111) crystal plane obtained by X-ray diffractometry of 1.2° or more and a crystallite size corresponding to the crystal plane of 7.5 nm or less.

### Claim 5 (depends on 1)

The negative electrode active material according to claim 1, wherein a test cell formed of a negative electrode containing a mixture of the negative electrode active material and a carbon-based active material and a counter electrode lithium is prepared, in the test cell, charge/discharge formed of charge during which a current is flowed so as to insert lithium into the negative electrode active material and discharge during which the current is flowed so as to detach lithium from the negative electrode active material is carried out 30 times, and when a graph showing a relationship between a differential value dQ/dV obtained by differentiating a discharge capacity Q by a potential V of the negative electrode based on the counter electrode lithium and the potential V is depicted in each charge/discharge, the potential V of the negative electrode during discharges on or after X times (1≤X≤30) has a peak in the range of from 0.40 V to 0.55 V.

### Claim 6 (depends on 1)

The negative electrode active material according to claim 1, wherein the particles of negative electrode active material have a median diameter of 1.0 μm or more and 15 μm or less.

### Claim 7 (depends on 1)

The negative electrode active material according to claim 1, wherein the particles of negative electrode active material contain a carbon material on a superficial part.

### Claim 8 (depends on 7)

The negative electrode active material according to claim 7, wherein an average thickness of the carbon material is 10 nm or more and 5000 nm or less.

### Claim 9 (depends on 1)

A mixed negative electrode active material comprises the negative electrode active material according to claim 1 and a carbon-based active material.

### Claim 10 (depends on 9)

A negative electrode for nonaqueous electrolyte secondary batteries comprising:
the mixed negative electrode active material according to claim 9,
wherein a ratio of a mass of the negative electrode active material relative to a total mass of the negative electrode active material and the carbon-based active material is 6% by mass or more.

### Claim 11 (depends on 9)

A negative electrode for nonaqueous electrolyte secondary batteries comprising:
a negative electrode active material layer formed with the mixed negative electrode active material according to claim 9; and
a negative electrode current collector,
wherein the negative electrode active material layer is formed on the negative electrode current collector; and
the negative electrode current collector includes carbon and sulfur, and each of contents thereof is 70 mass ppm or less.

### Claim 12 (depends on 1)

A lithium ion secondary battery comprising:
a negative electrode containing the negative electrode active material according to claim 1.

### Claim 13

A method of producing a negative electrode active material containing particles of negative electrode active material containing particles of silicon compound comprising:
preparing particles of negative electrode active material containing particles of silicon compound containing a silicon compound (SiOx:0.5≤x≤1.6); and
selecting, from the particles of negative electrode active material, particles of negative electrode active material in which, as chemical shift values obtained from a 29Si-MAS-NMR spectrum, an intensity A of a peak derived from amorphous silicon obtained in −40 to −60 ppm, an intensity B of a peak derived from a silicon dioxide region obtained in the vicinity of −110 ppm, and an intensity C of a peak derived from Si obtained in the vicinity of −83 ppm satisfy the following formula 1 and formula 2,
wherein producing the negative electrode active material with the selected particles of negative electrode active material.
B≤1.5×A (1)
B<C (2)

### Claim 14 (depends on 13)

A production method of a lithium ion secondary battery comprising:
preparing a negative electrode using the negative electrode active material produced according to the production method of the negative electrode active material according to claim 13; and
producing a lithium ion secondary battery with the prepared negative electrode.