# US 2018/0323371 A1 · Maintaining Coercive Field after High Temperature Anneal for Magnetic Device Applications with Perpendicular Magnetic Anisotropy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323371 A1
- Document ID: US20180323371A1
- Status: Published application
- Kind: A1
- Application number: 16/022,862
- Filed: 2018-06-29
- Published: 2018-11-08
- Earliest claimed: 2017-04-03
- Assignees: Headway Technologies, Inc.
- Applicants: Headway Technologies, Inc.
- Inventors: Huanlong Liu; Yuan-Jen Lee; Jian Zhu; Guenole Jan; Luc Thomas; Po-Kang Wang; Ru-Ying Tong; Jodi Mari Iwata
- Web page: https://patentgrep.com/patent/US20180323371A1

## CPC

- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H10N 50/01: Manufacture or treatment
- H01F 10/14: containing iron or nickel ({H01F10/126} , H01F10/13, H01F10/16 take precedence)
- H01F 10/32: Spin-exchange-coupled multilayers, e.g. nanostructured superlattices {(applying spin-exchange-coupled multilayers to substrates H01F41/302)}
- H01F 41/14: for applying magnetic films to substrates
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A magnetic tunnel junction with perpendicular magnetic anisotropy (PMA MTJ) is disclosed wherein a free layer interfaces with a tunnel barrier and has a second interface with an oxide layer. A lattice-matching layer adjoins an opposite side of the oxide layer with respect to the free layer and is comprised of CoXFeYNiZLWMV or an oxide or nitride of Ru, Ta, Ti, or Si, wherein L is one of B, Zr, Nb, Hf, Mo, Cu, Cr, Mg, Ta, Ti, Au, Ag, or P, and M is one of Mo, Mg, Ta, Cr, W, or V, (x+y+z+w+v)=100 atomic %, x+y>0, and each of v and w are >0. The lattice-matching layer grows a BCC structure during annealing thereby promoting BCC structure growth in the oxide layer that results in enhanced free layer PMA and improved thermal stability.

## Claims

### Claim 1

A magnetic memory element formed between a first electrode and a second electrode, comprising:
(a) a tunnel barrier layer formed between a reference layer and a free layer;
(b) the free layer with a first surface that forms a first interface with the tunnel barrier layer thereby promoting perpendicular magnetic anisotropy (PMA) in the free layer;
(c) an oxide layer that forms a second interface with the free layer at a second surface thereof that is on an opposite side of the free layer with respect to the tunnel barrier layer, and wherein both of the oxide layer and free layer have a body centered cubic (BCC) structure that enhances PMA in the free layer; and
(d) a first lattice-matching layer that adjoins an opposite side of the oxide layer with respect to the second interface, wherein the first lattice-matching layer is an oxide or nitride of Ru, Ta, Ti, or Si, or has a CoXFeYNiZLWMV composition wherein L is non-magnetic metal, M is one of Mo, Mg, Ta, Cr, W, Ru, or V, (x+y+z+w+v)=100 atomic %, x+y>0, and each of v and w are >0, and wherein the first lattice-matching layer has a BCC structure to assist a growth of the BCC structure in the oxide layer.

### Claim 2 (depends on 1)

The magnetic memory element of claim 1 wherein L is one of B, Zr, Nb, Hf, Mo, Cu, Cr, Mg, Ta, Ti, Au, Ag, or P.

### Claim 3 (depends on 1)

The magnetic memory element of claim 1 further comprised of a second lattice-matching layer that is a single layer or multilayer structure that adjoins an opposite side of the first lattice-matching layer with respect to the oxide layer, and wherein the second lattice matching layer is a single layer or multilayer structure comprised of one or more of Mo, Mg, Ta, Cr, W, Ru, and V.

### Claim 4 (depends on 1)

The magnetic memory element of claim 1 wherein the oxide layer is one of MgTaOx, MgO, SiOx, SrTiOx, BaTiOx, CaTiOx, LaAlOx, MnOx, VOx, Al2O3, TiOx, BOx, and HfOx, or is a laminate of one or more of the aforementioned oxides.

### Claim 5 (depends on 3)

The magnetic memory element of claim 3 wherein the first lattice-matching layer is the CoXFeYNiZLWMV layer and each of the second lattice matching layer and CoXFeYNiZLWMV layer has a thickness from about 2 to 10 Angstroms.

### Claim 6 (depends on 3)

The magnetic memory element of claim 3 further comprised of a third lattice matching layer having an CoXFeYNiZLW composition where w>0 and x+y>0 that is formed between the first lattice matching layer and the second lattice matching layer, and wherein the first lattice matching layer is the oxide or nitride of Ru, Ta, Ti, or Si.

### Claim 7 (depends on 6)

The magnetic memory element of claim 6 wherein the first lattice matching layer is conductive, and a total thickness of the first, second, and third lattice matching layers is from about 2 to 100 Angstroms.

### Claim 8 (depends on 1)

The magnetic memory element of claim 1 further comprised of a seed layer, and a hard mask to give a seed layer/reference layer/tunnel barrier/free layer/oxide layer/first lattice-matching layer/hard mask stack in a bottom spin valve configuration in which the seed layer contacts the first electrode and the hard mask contacts a bottom surface of the second electrode.

### Claim 9 (depends on 3)

The magnetic memory element of claim 3 further comprised of a seed layer, and a hard mask to give a seed layer/reference layer/tunnel barrier/free layer/oxide layer/first lattice-matching layer/second lattice matching layer/hard mask stack in a bottom spin valve configuration in which the seed layer contacts the first electrode and the hard mask contacts a bottom surface of the second electrode.

### Claim 10 (depends on 1)

The magnetic memory element of claim 1 further comprised of a seed layer, and a hard mask to give a seed layer/first lattice-matching layer/oxide layer/free layer/tunnel barrier/reference layer/hard mask stack in a top spin valve configuration in which the seed layer contacts the first electrode and the hard mask contacts a bottom surface of the second electrode.

### Claim 11 (depends on 3)

The magnetic memory element of claim 3 further comprised of a seed layer, and a hard mask to give a seed layer/second lattice-matching layer/first lattice matching layer/oxide layer/free layer/tunnel barrier/reference layer/hard mask stack in a top spin valve configuration in which the seed layer contacts the first electrode and the hard mask contacts a bottom surface of the second electrode.

### Claim 12

A method of forming a magnetic memory element with a stack of layers, comprising:
(a) sequentially depositing a reference layer, a tunnel barrier, and a free layer on a substrate wherein the free layer forms a first interface with the tunnel barrier thereby inducing or enhancing perpendicular magnetic anisotropy (PMA) in the free layer;
(b) forming an oxide layer on a top surface of the free layer to form a second interface that induces or enhances PMA in the free layer;
(c) forming a first lattice-matching layer on the oxide layer, wherein the first lattice-matching layer is amorphous as deposited and is comprised of a CoXFeYNiZLWMV layer, an oxide or nitride of Ru, Ta, Ti, and Si, or a layer that is made of a magnetic material that is a CoXFeYNiZLW alloy wherein L is a non-magnetic element, M is one of Mo, Mg, Ta, Cr, W, Ru, or V, (x+y+z+w+v)=100 atomic %, x+y>0, and each of v and w are >0;
(d) depositing a hard mask as an uppermost layer in the stack of layers; and
(e) annealing the stack of layers at a temperature proximate to 400° C. so that the first lattice-matching layer grows a BCC structure to promote a growth of a BCC structure in the oxide layer.

### Claim 13 (depends on 12)

The method of claim 12 wherein L is one of B, Zr, Nb, Hf, Mo, Cu, Cr, Mg, Ta, Ti, Au, Ag, or P.

### Claim 14 (depends on 12)

The method of claim 12 further comprised of depositing a second lattice-matching layer that is a single layer or multilayer structure and comprises one or more M elements selected from Mo, Mg, Ta, Cr, W, Ru, and V on the first lattice-matching layer before the hard mask is formed.

### Claim 15 (depends on 12)

The method of claim 12 wherein the oxide layer is one of MgTaOx, MgO, SiOx, SrTiOx, BaTiOx, CaTiOx, LaAlOx, MnOx, VOx, Al2O3, TiOx, BOx, and HfOx, or is a laminate of one or more of the aforementioned oxides.

### Claim 16 (depends on 14)

The method of claim 14 wherein deposition of the second lattice-matching layer on the first lattice-matching layer forms a single layer of CoXFeYNiZLWMV, or forms bilayer stack with a CoXFeYNiZLW/M or a CoXFeYNiZLWMV/M configuration wherein an M element layer contacts the hard mask.

### Claim 17 (depends on 14)

The method of claim 14 wherein deposition of the second lattice-matching layer on the first lattice-matching layer made of CoXFeYNiZLW forms a trilayer stack with a CoXFeYNiZLW/CoXFeYNiZLWMV/M configuration wherein an M element layer contacts the hard mask.

### Claim 18 (depends on 12)

The method of claim 12 wherein the substrate is a seed layer or a first electrode, and the first electrode is a bottom electrode in a Magnetoresistive Random Access Memory (MRAM) device or in a spin-torque MRAM, or the first electrode is a main pole layer in a spin torque oscillator (STO) device.

### Claim 19 (depends on 12)

The method of claim 12 wherein the first lattice matching layer is the oxide or nitride of Ru, Ta, Ti, or Si, and the method is further comprised of depositing a second lattice matching layer with the CoXFeYNiZLW alloy composition on the first lattice matching layer, and then depositing a third lattice matching layer that is one or more of the M elements on the second lattice matching layer before the hard mask is formed.

### Claim 20

A method of forming a magnetic memory element with a stack of layers, comprising:
(a) depositing a first lattice-matching layer that is a single layer or a multilayer structure, and comprises one or more M elements selected from Mo, Mg, Ta, Cr, W, Ru, and V on a substrate;
(b) depositing a second lattice-matching layer on the first lattice matching layer, wherein the second lattice-matching layer is amorphous as deposited and is comprised of a magnetic material with a CoXFeYNiZLW composition wherein L is a non-magnetic element, (x+y+z+w)=100 atomic %, x+y>0, and w is >0;
(c) forming an oxide layer on the second lattice-matching layer;
(d) depositing a free layer that contacts a top surface of the oxide layer to form a first interface which induces or enhances perpendicular magnetic anisotropy (PMA) in the free layer;
(e) sequentially forming a tunnel barrier, reference layer, and a hard mask wherein the tunnel barrier contacts a top surface of the free layer to form a second interface that induces or enhances PMA in the free layer; and
(f) annealing the stack of layers at a temperature of about 400° C. so that the second lattice-matching layer grows a BCC structure to match a growth of a BCC structure in the oxide layer.

### Claim 21 (depends on 20)

The method of claim 20 wherein L is one of B, Zr, Nb, Hf, Mo, Cu, Cr, Mg, Ta, Ti, Au, Ag, or P.

### Claim 22 (depends on 20)

The method of claim 20 wherein the oxide layer is one of MgTaOx, MgO, SiOx, SrTiOx, BaTiOx, CaTiOx, LaAlOx, MnOx, VOx, Al2O3, TiOx, BOx, and HfOx, or is a laminate of one or more of the aforementioned oxides.

### Claim 23 (depends on 20)

The method of claim 20 wherein depositing the second lattice-matching layer on the first lattice-matching layer forms a single lattice-matching layer with a CoXFeYNiZLWMV composition wherein (x+y+z+w+v)=100 atomic %, x+y>0, and each of v and w are >0, and wherein the single lattice matching layer adjoins the oxide layer, and grows a BCC structure during the annealing of the stack of layers thereby promoting a BCC structure growth in the oxide layer.

### Claim 24 (depends on 20)

The method of claim 20 wherein deposition of the second lattice-matching layer on the first lattice-matching layer forms a bilayer stack with a M/CoXFeYNiZLW or a M/CoXFeYNiZLWMV configuration wherein the CoXFeYNiZLWMV or CoXFeYNiZLW layer contacts the oxide layer, and the CoXFeYNiZLWMV or CoXFeYNiZLW layer grows a BCC structure during the annealing of the stack of layers to promote a BCC structure growth in the oxide layer.

### Claim 25 (depends on 20)

The method of claim 20 wherein deposition of the second lattice-matching layer on the first lattice-matching layer forms a trilayer stack with a M/CoXFeYNiZLWMV/CoXFeYNiZLW configuration in which the CoXFeYNiZLW layer contacts the oxide layer, and the CoXFeYNiZLW layer grows a BCC structure during the annealing of the stack of layers to promote a BCC structure growth in the oxide layer.

### Claim 26 (depends on 20)

The method of claim 20 wherein the substrate is a seed layer or a first electrode, and the first electrode is a bottom electrode in a Magnetoresistive Random Access Memory (MRAM) device or in a spin-torque MRAM, or the first electrode is a main pole layer in a spin torque oscillator (STO) device.

### Claim 27 (depends on 20)

The method of claim 20 further comprised of depositing a third lattice matching layer on the second lattice matching layer before the oxide layer is deposited, wherein the third lattice matching layer is an oxide or nitride of Ru, Ta, Ti, or Si.