# US 2018/0323346 A1 · Light-emitting element having zno transparent electrode and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323346 A1
- Document ID: US20180323346A1
- Status: Published application
- Kind: A1
- Application number: 15/757,636
- Filed: 2016-08-23
- Published: 2018-11-08
- Earliest claimed: 2015-09-03
- Assignees: Seoul Viosys Co., Ltd.
- Applicants: Seoul Viosys Co., Ltd.
- Inventors: Jin Woong Lee; Chan Seob Shin; Keum Ju Lee; Seom Geun Lee; Myoung Hak Yang
- Web page: https://patentgrep.com/patent/US20180323346A1

## CPC

- H10H 20/833: Transparent materials
- G02F 1/133603: {with LEDs}
- H10H 20/814: having reflecting means, e.g. semiconductor Bragg reflectors
- H10H 20/8252: {characterised by the dopants}
- H10H 20/857: Interconnections, e.g. lead-frames, bond wires or solder balls
- C30B 7/005: {Epitaxial layer growth}
- C30B 29/16: Oxides
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/032: {of electrodes}
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/8316: {Multi-layer electrodes comprising at least one discontinuous layer}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A light-emitting electrode having a ZnO transparent electrode and a method for manufacturing the same are provided. A light-emitting element according to an embodiment comprises: a light-emitting structure comprising a first conductive semiconductor layer, an active layer, and a second conductive semiconductor layer; and a ZnO transparent electrode, which is positioned on the second conductive semiconductor layer, which makes an Ohmic contact with the second conductive semiconductor layer, and which comprises monocrystalline ZnO, wherein the diffraction angle of a peak of the ZnO transparent electrode, which results from X-ray diffraction (XRD) omega 2theta (ω2θ) scan, is in the range of ±1% with regard to the diffraction angle of a peak of the second conductive semiconductor layer, which results from XRD ω2θ scan, and the FWHM of a main peak of the ZnO transparent electrode, which results from XRD omega (ω) scan, is equal to or less than 900 arcsec.

## Claims

### Claim 1

A light emitting diode comprising:
a light emitting structure comprising a first conductivity type semiconductor layer, an active layer disposed on the first conductivity type semiconductor layer, and a second conductivity type semiconductor layer disposed on the active layer; and
a ZnO transparent electrode disposed on the second conductivity type semiconductor layer to form ohmic contact with the second conductivity type semiconductor layer and comprising monocrystalline ZnO
wherein a diffraction angle of a peak of the ZnO transparent electrode obtained by XRD (X-Ray Diffraction) ω2θ scanning is in the range of ±1% with respect to a diffraction angle of a peak of the second conductivity type semiconductor layer obtained by XRD ω2θ scanning and a main peak of the ZnO transparent electrode obtained by XRD ω scanning has a full width at half maximum (FWHM) of 900 arcsec or less.

### Claim 2 (depends on 1)

The light emitting diode according to claim 1, wherein the diffraction angle of the peak of the ZnO transparent electrode obtained by XRD ω2θ scanning is in the range of ±0.5% with respect to the diffraction angle of the peak of the second conductivity type semiconductor layer obtained by XRD ω2θ scanning.

### Claim 3 (depends on 1)

The light emitting diode according to claim 1, wherein the main peak of the ZnO transparent electrode obtained by XRD ω scanning has an FWHM of 870 arcsec or less.

### Claim 4 (depends on 1)

The light emitting diode according to claim 1, wherein the ZnO transparent electrode has a thickness of 800 nm or more.

### Claim 5 (depends on 1)

The light emitting diode according to claim 1, wherein the ZnO transparent electrode comprises a ZnO seed layer and a ZnO bulk layer disposed on the ZnO seed layer, the ZnO bulk layer having a greater thickness than the ZnO seed layer.

### Claim 6 (depends on 5)

The light emitting diode according to claim 5, wherein the thickness of the ZnO bulk layer is between 90% and 100% of the thickness of the ZnO transparent electrode.

### Claim 7 (depends on 5)

The light emitting diode according to claim 5, wherein the ZnO seed layer comprises undoped ZnO and the ZnO bulk layer comprises monocrystalline ZnO doped with at least one of silver (Ag), indium (In), tin (Sn), zinc (Zn), cadmium (Cd), gallium (Ga), aluminum (Al), magnesium (Mg), titanium (Ti), molybdenum (Mo), nickel (Ni), copper (Cu), gold (Au), platinum (Pt), rhodium (Rh), iridium (Ir), ruthenium (Ru), or palladium (Pd).

### Claim 8 (depends on 1)

The light emitting diode according to claim 1, wherein the ZnO transparent electrode comprises a plurality of voids.

### Claim 9 (depends on 1)

The light emitting diode according to claim 1, wherein the second conductivity type semiconductor layer has a c-plane as a growth plane and the monocrystalline ZnO of the ZnO transparent electrode has a wurtzite crystal structure.

### Claim 10

A method of manufacturing a light emitting diode, comprising:
forming a light emitting structure, the light emitting structure comprising a first conductivity type semiconductor layer, an active layer disposed on the first conductivity type semiconductor layer, and a second conductivity type semiconductor layer disposed on the active layer; and
forming a ZnO transparent electrode on the second conductivity type semiconductor layer to form ohmic contact with the second conductivity type semiconductor layer, wherein a diffraction angle of a peak of the ZnO transparent electrode obtained by XRD ω2θ scanning is in the range of ±1% with respect to a diffraction angle of a peak of the second conductivity type semiconductor layer obtained by XRD ω2θ scanning and a main peak of the ZnO transparent electrode obtained by XRD ω scanning has a full width at half maximum (FWHM) of 900 arcsec or less.

### Claim 11 (depends on 10)

The method of manufacturing a light emitting diode according to claim 10, wherein the forming the ZnO transparent electrode comprises:
forming a ZnO seed layer on the second conductivity type semiconductor layer; and
forming a ZnO bulk layer on the ZnO seed layer using the ZnO seed layer as a seed.

### Claim 12 (depends on 11)

The method of manufacturing a light emitting diode according to claim 11, wherein the forming the ZnO seed layer comprises:
forming a ZnO layer on the second conductivity type semiconductor layer by spin coating; and
subjecting the ZnO layer to heat treatment, and
the ZnO seed layer forms ohmic contact with the second conductivity type semiconductor layer.

### Claim 13 (depends on 11)

The method of manufacturing a light emitting diode according to claim 11, wherein the forming the ZnO bulk layer comprises:
forming monocrystalline ZnO on the ZnO seed layer through hydrothermal synthesis; and
subjecting the monocrystalline ZnO to heat treatment.

### Claim 14 (depends on 13)

The method of manufacturing a light emitting diode according to claim 13, wherein the forming the ZnO bulk layer comprises forming a plurality of voids in the ZnO bulk layer.

### Claim 15 (depends on 10)

The method of manufacturing a light emitting diode according to claim 10, wherein the ZnO transparent electrode is formed to a thickness of 800 nm or more.

### Claim at position 16

16-32. (canceled)