# US 2018/0323079 A1 · Methods for processing semiconductor wafers having a polycrystalline finish

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0323079 A1
- Document ID: US20180323079A1
- Status: Published application
- Kind: A1
- Application number: 15/764,272
- Filed: 2016-09-29
- Published: 2018-11-08
- Earliest claimed: 2015-09-30
- Assignees: SunEdison Semiconductor Limited (UEN201334164H)
- Applicants: SunEdison Semiconductor Limited (UEN201334164H)
- Inventors: Alexis GRABBE; Hui WANG; Alex CHU
- Web page: https://patentgrep.com/patent/US20180323079A1

## CPC

- H10P 52/403: {of conductive or resistive materials}
- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3456: {Polycrystalline}
- H10P 70/277: {the processing being a planarisation of conductive layers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES

## Abstract

A method of processing a semiconductor wafer includes depositing a silicon layer on the semiconductor wafer. A first slurry is applied to the semiconductor wafer and the silicon layer is polished to smooth the silicon layer. A second slurry is applied to the semiconductor wafer. The second slurry includes a greater amount of a caustic agent than the first slurry.

## Claims

### Claim 1

A method of processing a semiconductor wafer comprising:
depositing a silicon layer on the semiconductor wafer;
applying a first slurry to the semiconductor wafer;
polishing the silicon layer to smooth the silicon layer;
applying a second slurry to the semiconductor wafer, the second slurry including a greater amount of a caustic agent than the first slurry.

### Claim 2 (depends on 1)

The method of claim 1 wherein the silicon layer is a polycrystalline silicon layer, the layer having a reduced roughness after polishing and the polycrystalline grain boundary being reduced by polishing.

### Claim 3 (depends on 1)

The method of claim 1 wherein the silicon layer is polished using the first slurry for a predetermined time, the predetermined time being in the range between about 1 minute and about 5 minutes.

### Claim 4 (depends on 1)

The method of claim 1 wherein predetermined time is approximately 2 minutes.

### Claim 5 (depends on 1)

The method of claim 1 wherein the silicon layer is polished using the second slurry for a predetermined time, the predetermined time being in the range between about 5 minutes and about 15 minutes.

### Claim 6 (depends on 1)

The method of claim 1 wherein the caustic agent is potassium hydroxide.

### Claim 7 (depends on 1)

The method of claim 1 wherein the pH of the second slurry is greater than the pH of the first slurry.

### Claim 8 (depends on 1)

The method of claim 1 further comprising cleaning the semiconductor wafer to facilitate growth on the silicon layer prior to polishing the silicon layer.

### Claim 9 (depends on 8)

The method of claim 8 further comprising forming a silicon oxide layer on the silicon layer prior to polishing the silicon layer.

### Claim 10 (depends on 9)

The method of claim 9 wherein cleaning the semiconductor wafer comprises cleaning the semiconductor wafer using a standard clean 1 (SC1).

### Claim 11

A method of processing a semiconductor wafer comprising:
depositing a silicon layer on the semiconductor wafer;
positioning the semiconductor wafer on a first wafer polishing apparatus;
polishing the silicon layer while the semiconductor wafer is positioned on the first wafer polishing apparatus such that a first portion of the silicon layer is removed;
positioning the semiconductor wafer on a second wafer polishing apparatus; and
polishing the silicon layer while the semiconductor wafer is positioned on the second wafer polishing apparatus such that a second portion of the silicon layer is removed.

### Claim 12 (depends on 11)

The method of claim 11 wherein between about 0.3 um and about 1 um of the thickness of the silicon layer is removed while the silicon layer is polished on the first wafer polishing apparatus.

### Claim 13 (depends on 11)

The method of claim 11 wherein between about 0.1 um and about 0.5 um of the thickness of the silicon layer is removed while the silicon layer is polished on the second wafer polishing apparatus.

### Claim 14 (depends on 11)

The method of claim 11 further comprising applying a first slurry to the semiconductor wafer while the semiconductor wafer is on the first wafer polishing apparatus.

### Claim 15 (depends on 14)

The method of claim 14 further comprising applying a second slurry to the semiconductor wafer while the semiconductor wafer is on the first wafer polishing apparatus, the second slurry including a greater amount of a caustic agent than the first slurry.

### Claim 16

A method of processing a semiconductor wafer comprising:
depositing a silicon layer on the semiconductor wafer;
cleaning the semiconductor wafer to facilitate growth on the silicon layer; and
polishing the semiconductor wafer to smooth the silicon layer after the semiconductor wafer is cleaned.

### Claim 17 (depends on 16)

The method of claim 16 further comprising forming a silicon oxide layer on the silicon layer prior to polishing the semiconductor wafer.

### Claim 18 (depends on 17)

The method of claim 17 wherein cleaning the semiconductor wafer comprises cleaning the semiconductor wafer using a standard clean 1 (SC1).

### Claim 19 (depends on 18)

The method of claim 18 further comprising cleaning the semiconductor wafer after polishing the semiconductor wafer.

### Claim 20 (depends on 16)

The method of claim 16 wherein the semiconductor wafer is polished using a first slurry and a second slurry, the second slurry including a greater amount of a caustic agent than the first slurry.