# US 2018/0321562 A1 · Boa liquid crystal display panel and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0321562 A1
- Document ID: US20180321562A1
- Status: Published application
- Kind: A1
- Application number: 16/030,853
- Filed: 2018-07-09
- Published: 2018-11-08
- Earliest claimed: 2015-07-20
- Assignees: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Applicants: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Inventors: Mian Zeng
- Web page: https://patentgrep.com/patent/US20180321562A1

## CPC

- G02F 1/136209: {Light shielding layers, e.g. black matrix, incorporated in the active matrix substrate, e.g. structurally associated with the switching element}
- G02F 1/133516: {Methods for their manufacture, e.g. printing, electro-deposition or photolithography}
- G02F 1/1341: Filling or closing of cells
- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G02F 1/136227: {Through-hole connection of the pixel electrode to the active element through an insulation layer}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- H10D 30/6723: {having light shields}
- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 86/0212: {comprising manufacture, treatment or coating of substrates}
- H10D 86/0231: {using masks, e.g. half-tone masks}
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/60: wherein the TFTs are in active matrices
- G02F 1/133302: {Rigid substrates, e.g. inorganic substrates}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 2201/121: common or background
- G02F 2201/123: pixel
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for manufacturing a BOA liquid crystal display panel is provided. The BOA liquid crystal display panel is structured to have a TFT entirely located on a first black matrix and further, a second black matrix is arranged between the TFT and the passivation protection layer such that the second black matrix and the first black matrix completely enclose the TFT to block light emitting from a backlight module located under an array substrate in a direction toward an active layer and also to block reflecting light irradiating the active layer from lateral sides and a top side to better prevent light irradiating the active layer of the TFT for preventing photo leakage current, ensuring stable performance of the TFT device, and improving image displaying quality. The method helps overcome the issue of photo leakage current induced by backlighting irradiating the active layer of the TFT.

## Claims

### Claim 1

A method for manufacturing a black matrix on array (BOA) liquid crystal display panel, comprising, after formation of a first black matrix made of black resin provided on a lower substrate that is located at one side of an array substrate, forming a thin-film transistor (TFT) that is entirely located on and in direct contact with the first black matrix; and forming a color resist layer and a common electrode on a surface of a color filter (CF) substrate, wherein the TFT comprises source/drain terminals and an active layer that are directly formed on the first black matrix and at least partly in direct contact with the first black matrix.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a second black matrix is further formed on the TFT such that the second black matrix and the first black matrix completely enclose the TFT, and the first black matrix and the second black matrix are formed by using the same mask.

### Claim 3 (depends on 1)

The method according to claim 1 comprising the following steps:
(1) providing a lower substrate, coating a layer of black resin on the lower substrate, using a first mask to subject the black resin to patterning treatment so as to form the first black matrix;
(2) sputtering-coating or vapor-depositing a metal film on the first black matrix and the lower substrate and using a second mask to subject the metal film to patterning treatment so as to form the source/drain terminals located on the first black matrix;
(3) successively depositing a semiconductor film and an insulation film on the source/drain terminals and the first black matrix through chemical vapor deposition and then sputtering-coating or vapor-depositing another metal film, and using a third mask to simultaneously subject said another metal film, the insulation film, and the semiconductor film to patterning treatment so as to form the active layer, a gate insulation layer, and a gate terminal that are sequentially formed on the source/drain terminals and the first black matrix,
wherein the source/drain terminals, the active layer, the gate insulation layer, and the gate terminal collectively constitute the TFT;
(4) depositing a passivation protection layer on the TFT and the lower substrate through chemical vapor deposition and using a fourth mask to subject the passivation protection layer to patterning treatment to form a via extending through the passivation protection layer so as to expose a portion of the source/drain terminals;
(5) depositing an indium tin oxide (ITO) film on the passivation protection layer and using a fifth mask to subject the ITO film to patterning treatment so as to form a pixel electrode, in such a way that the pixel electrode is set in contact with the source/drain terminals through the via thereby completing the manufacture of the array substrate; and
(6) providing an upper substrate and sequentially forming the color resist layer and the common electrode layer on the upper substrate to complete the manufacture of the CF substrate, and
then, laminating the array substrate and the CF substrate together, filling liquid crystal molecules between the array substrate and the CF substrate to form a liquid crystal layer, and subjecting the array substrate and the CF substrate to packaging.

### Claim 4 (depends on 2)

The method according to claim 2 comprising the following steps:
(1) providing a lower substrate, coating a layer of black resin on the lower substrate, using a first mask to subject the black resin to patterning treatment so as to form the first black matrix;
(2) sputtering-coating or vapor-depositing a metal film on the first black matrix and the lower substrate and using a second mask to subject the metal film to patterning treatment so as to form the source/drain terminals located on the first black matrix;
(3) successively depositing a semiconductor film and an insulation film on the source/drain terminals and the first black matrix through chemical vapor deposition and then sputtering-coating or vapor-depositing another metal film, and using a third mask to simultaneously subject said another metal film, the insulation film, and the semiconductor film to patterning treatment so as to form the active layer, a gate insulation layer, and a gate terminal that are sequentially formed on the source/drain terminals and the first black matrix,
wherein the source/drain terminals, the active layer, the gate insulation layer, and the gate terminal constitute the TFT;
(4) coating another layer of black resin on the TFT and the lower substrate and using the first mask to subject said another layer of the black resin to patterning treatment to form the second black matrix such that the second black matrix and the first black matrix completely enclose the TFT;
(5) depositing a passivation protection layer on the second black matrix and the lower substrate through chemical vapor deposition and using a fourth mask to subject the passivation protection layer to patterning treatment to form a via extending through the passivation protection layer and the second black matrix so as to expose a portion of the source/drain terminals;
(6) depositing an indium tin oxide (ITO) film on the passivation protection layer and using a fifth mask to subject the ITO film to patterning treatment so as to form a pixel electrode, in such a way that the pixel electrode is set in contact with the source/drain terminals through the via thereby completing the manufacture of the array substrate; and
(7) providing an upper substrate and sequentially forming a color resist layer and a common electrode layer on the upper substrate to complete the manufacture of the CF substrate, and
then, laminating the array substrate and the CF substrate together, filling liquid crystal molecules between the array substrate and the CF substrate to form a liquid crystal layer, and subjecting the array substrate and the CF substrate to packaging.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the gate terminal and the source/drain terminals are each formed of a material comprising one of molybdenum, titanium, aluminum, copper, and nickel, or a stacked combination of multiple ones thereof and the gate insulation layer and the passivation protection layer are each formed of a material of silicon oxides, silicon nitrides, or a combination thereof.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the gate terminal and the source/drain terminals are each formed of a material comprising one of molybdenum, titanium, aluminum, copper, and nickel, or a stacked combination of multiple ones thereof and the gate insulation layer and the passivation protection layer are each formed of a material of silicon oxides, silicon nitrides, or a combination thereof.