# US 2018/0321176 A1 · Carbon material supported hollow metal oxide nanoparticles, methods and applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0321176 A1
- Document ID: US20180321176A1
- Status: Published application
- Kind: A1
- Application number: 16/029,913
- Filed: 2018-07-09
- Published: 2018-11-08
- Earliest claimed: 2013-03-21
- Assignees: Cornell University; Huazhong University of Science and Technology
- Applicants: Cornell University; Huazhong University of Science and Technology
- Inventors: Yingchao Yu; Héctor D. Abruña; Deli Wang; Weidong Zhou; Liu Hongfang; Qin Shuang
- Web page: https://patentgrep.com/patent/US20180321176A1

## CPC

- G01N 27/308: {at least partially made of carbon}
- H01G 11/24: characterised by structural features of the materials making up or comprised in the electrodes, e.g. form, surface area or porosity; characterised by the structural features of powders or particles used therefor
- H01G 11/30: characterised by their material
- H01G 11/32: Carbon-based
- H01G 11/46: Metal oxides
- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/366: {as layered products}
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/362: {Composites}
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing a material composition comprising a hollow transition metal oxide nanoparticle supported upon a carbon material support includes a solution impregnation process step, followed by a thermal reduction process step and finally a thermal oxidation process step. The material composition, an electrode and an electrical component such as but not limited to a battery are all predicated at least in-part upon the material composition prepared in accord with the foregoing method. The foregoing material composition, electrode, battery and method may ultimately provide a LIB with enhanced performance.

## Claims

### Claim 1

A material composition comprising:
a carbon material support; and
a hollow transition metal oxide nanoparticle supported upon the carbon material support, wherein the hollow transition metal oxide nanoparticle material has a hollow volume percentage from about 20 to about 60 percent,
wherein the hollow volume includes:
a primary void of greater than about 50 nm;
a plurality of secondary voids of less than about 10 nm; and
a uniform elemental distribution of metal and oxygen across the nanoparticle.

### Claim 2 (depends on 1)

The material composition of claim 1, wherein the hollow transition metal oxide nanoparticle has:
a particle size from about 50 to about 300 nanometers; and
a pore size from about 5 to about 100 nanometers.

### Claim 3 (depends on 1)

The material composition of claim 1, wherein the carbon material support comprises a carbon material selected from the group consisting of amorphous carbon, crystalline carbon, graphitic carbon, graphene, graphene oxide, carbon nanotube, and carbon microtube carbon material supports.

### Claim 4 (depends on 1)

The material composition of claim 1, wherein the hollow transition metal oxide nanoparticle comprises a transition metal selected from the group consisting of cobalt, iron, manganese, nickel, titanium, copper, zinc, and vanadium transition metals.

### Claim 5

An electrode comprising:
a conductive substrate; and
a coating located upon the conductive substrate and including a material composition comprising:
a carbon material support; and
a hollow transition metal oxide nanoparticle supported upon the carbon material support, wherein the hollow transition metal oxide nanoparticle material has a hollow volume percentage from about 20 to about 60 percent,
wherein the hollow volume includes:
a primary void of greater than about 50 nm;
a plurality of secondary voids of less than about 10 nm; and
a uniform elemental distribution of metal and oxygen across the nanoparticle.

### Claim 6 (depends on 5)

The electrode of claim 5, wherein the transition metal oxide nanoparticle has:
a particle size from about 50 to about 300 nanometers; and
a pore size from about 5 to about 100 nanometers; and

### Claim 7 (depends on 5)

The electrode of claim 5, wherein the carbon material support comprises a carbon material selected from the group consisting of amorphous carbon, crystalline carbon, graphitic carbon, graphene, graphene oxide, carbon nanotube, and carbon microtube carbon material supports.

### Claim 8 (depends on 5)

The electrode of claim 5, wherein the hollow transition metal oxide nanoparticle includes a transition metal selected from the group consisting of cobalt, iron, manganese, nickel, titanium, copper, zinc, and vanadium transition metals.

### Claim 9

A method for preparing a material composition comprising:
impregnating a carbon material support with a transition metal salt to form a transition metal salt impregnated carbon material support;
thermally annealing the transition metal salt impregnated carbon material support within a reducing environment to provide a reduced transition metal particle supported on the carbon material support; and
thermally annealing the reduced transition metal particle supported on the carbon material support within an oxidizing environment to provide a hollow transition metal oxide nanoparticle supported on the carbon material support, wherein:
the hollow transition metal oxide nanoparticle has a hollow volume percentage from about 20 to about 60 percent, wherein the hollow volume includes:
a primary void of greater than about 50 nm;
a plurality of secondary voids of less than about 10 nm; and
a uniform elemental distribution of metal and oxygen across the nanoparticle.

### Claim 10 (depends on 9)

The method of claim 9, wherein the hollow transition metal oxide nanoparticle has:
a particle size from about 50 to about 300 nanometers; and
a pore size from about 5 to about 100 nanometers.

### Claim 11 (depends on 9)

The method of claim 9, wherein the impregnating is undertaken in solvent selected from the group consisting of water and a low molecular weight alcohol.

### Claim 12 (depends on 9)

The method of claim 9, wherein the carbon material support is selected from the group consisting of amorphous carbon, crystalline carbon, graphitic carbon, graphene, graphene oxide, carbon nanotube, and carbon microtube carbon material supports.

### Claim 13 (depends on 9)

The method of claim 9, wherein the transition metal salt is characterized by the formula MLx, where:
M is one or more of cobalt, iron, nickel, manganese, titanium, copper, zinc, and vanadium; and
L is one or more of chloride, sulfate, and nitrate; and x ranges from 1 to 4.

### Claim 14 (depends on 9)

The method of claim 9, wherein the reducing environment is selected from the group consisting of:
a hydrogen gas and a mixture of hydrogen gas and up to about 90 percent inert gas; and
a liquid-based reducing reagent selected from the group consisting of sodium citrate solution, ascorbic acid solution, sodium borate hydrate solution, and hydrazine.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
a reducing temperature is from about 100° C. to about 800° C.; and
a reducing time is from about 1 hour to about 10 hours.

### Claim 16 (depends on 9)

The method of claim 9, wherein the oxidizing environment comprises at least one of:
an oxidizing gas selected from the group consisting of oxygen, air, and a mixture of oxygen with an inert gas; and
a liquid-based oxidizing reagent selected from the group consisting of hydrogen peroxide, and aqueous nitric acid.

### Claim 17 (depends on 16)

The method of claim 16, wherein:
the oxidizing temperature is from about 100° C. to about 800° C.; and
the oxidizing time is from about 1 hour to about 10 hours.

### Claim 18 (depends on 9)

The method of claim 9, wherein the hollow transition metal oxide nanoparticle is described by the formula MxOy where:
M includes one or more transition metal elements selected from the group consisting of Co, Fe, Mn, Ni, Ti, Cu, Zn, and V;
O is oxygen;
x ranges from 1 to 3;
y ranges from 1 to 4; and
x and y are not limited to integers.