A high purity cobalt chloride having a purity of 5N (99.999%) or higher and a manufacturing method of the high purity cobalt chloride via electrolysis are provided. In the method, cobalt having a purity of 5N or higher is used as an anode, a diluted hydrochloric acid bath having a pH of 1.5 to 3.0 is used as an electrolytic solution, the cobalt anode and a cathode plate are partitioned with an anion exchange membrane, and electrodeposition of the cobalt onto the cathode plate is thereby inhibited. The manufacturing method is capable of providing high purity cobalt chloride at a higher purity and at a lower production cost than conventional methods. Under circumstances where demands for cobalt chloride may increase, cobalt chloride needs to be manufactured at high volume and at low cost, and the method disclosed herein provides a technique capable of satisfying the foregoing requirements.
A manufacturing method of high purity cobalt chloride via electrolysis, wherein cobalt having a purity of 5N (99.999%) or higher is used as an anode, a diluted hydrochloric acid bath having a pH of 1.5 to 3.0 is used as an electrolytic solution, the cobalt anode and a cathode plate are partitioned with an anion exchange membrane, and electrodeposition of the cobalt which became eluted into the hydrochloric acid bath onto the cathode plate is thereby inhibited.
The manufacturing method of high purity cobalt chloride via electrolysis according to claim 11, wherein the thus prepared cobalt chloride solution is evaporated to dryness and concentrated, thereafter removed, filtered and separated, and the filtered cobalt chloride is subsequently dried.