# US 2018/0311721 A1 · Method for forming a joint using a self-piercing rivet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0311721 A1
- Document ID: US20180311721A1
- Status: Published application
- Kind: A1
- Application number: 15/988,665
- Filed: 2018-05-24
- Published: 2018-11-01
- Earliest claimed: 2012-07-16
- Assignees: Henrob Limited
- Applicants: Henrob Limited
- Inventors: Russell John Trinick
- Web page: https://patentgrep.com/patent/US20180311721A1

## CPC

- B21J 15/025: {Setting self-piercing rivets}
- B21J 15/36: Rivet sets, i.e. tools for forming heads; Mandrels for expanding parts of hollow rivets
- F16B 5/04: by means of riveting (rivets F16B19/04)
- F16B 19/086: {Self-piercing rivets}
- Y10T 29/49943: Riveting
- B21J: FORGING; HAMMERING; PRESSING METAL; RIVETING; FORGE FURNACES (rolling of metal B21B; making particular products by forging or pressing B21K; cladding or plating B23K; finishing surfaces by hammering B23P9/04; compacting surfaces by blasting with particulate material B24C1/10; general features of presses, presses for consolidating scrap B30B; furnaces in general F27)
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A joint is formed in a stack of at least two sheets of light metal alloy, using a self-piercing rivet that is fully hollow. The rivet is coated at least along a portion of its bore by a lubricant and pierces the upper surface thereof and such that the shank deforms outwardly to interlock with the materials but without penetration to the die side of the material. The outside diameter of the shank of the rivet is 5.4 mm or less. The die has a volume that is less than 60% or 70% of the effective solid volume of the rivet.

## Claims

### Claim 1

A method for forming a joint in a stack of at least two sheets of material, at least one of the sheets being a light metal alloy, using a self-piercing rivet comprising the steps of: positioning the material over a die; providing a substantially cylindrical self-piercing rivet that is fully hollow so as to define a bore that extends along its entire length, the rivet having been coated at least along a portion of its bore by a lubricant; positioning the rivet over the sheet material at a position opposite the die; using a punch to set the rivet and force it into the sheet material such that it pierces an upper surface thereof and such that a shank of the rivet deforms outwardly to interlock with the material but without penetration to the die side of the material; wherein the rivet has a shank with an outside diameter of 5.4 mm or less, and the die has a volume that is 60% or less of an effective solid volume of the rivet.

### Claim 2 (depends on 1)

A method according to claim 1, where the sheets have an ultimate tensile strength in the range of 50-600 MPa.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the sheets have an ultimate tensile strength in the range of 180 MPa-600 MPa.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the die has a die cavity having a maximum depth in the range of 0.5 mm to 2.0 mm.

### Claim 5 (depends on 1)

A method according to claim 1, in which the stack of sheet material has a thickness of at least 6.0 mm.

### Claim 6 (depends on 1)

A method according to claim 1, in which the stack of sheet material has a thickness of at least 1.0 mm.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the rivet is coated with lubricant along a full length of its bore.

### Claim 8 (depends on 7)

A method according to claim 7, wherein the rivet is further coated with lubricant on at least part of an exterior surface of a shank of the rivet.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the lubricant is a dry film.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the sheet material is high strength aluminum alloy having an ultimate tensile strength in the range of 330-600 MPa.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the sheet material is wrought magnesium alloy having an ultimate tensile strength in the range of 180-440 MPa.

### Claim 12 (depends on 1)

A method according to claim 1, wherein a diameter of the bore of the rivet is at least 3.1 mm.

### Claim 13 (depends on 1)

A method according to claim 1, wherein an outside diameter of the shank is 3.36 mm or less.

### Claim 14 (depends on 13)

A method according to claim 13, wherein an inside diameter of the bore of the rivet is at least 2.0 mm.

### Claim 15 (depends on 1)

A method according to claim 1, wherein the rivet has a countersunk head.

### Claim 16 (depends on 1)

A method according to claim 1, wherein the rivet has at least one formation at an upper portion of the bore, the method including allowing the sheet material to deform such that a slug of material from the upper sheet and inside the bore engages with said at least one formation.

### Claim 17 (depends on 1)

A method according to claim 1, wherein the at least one formation comprises a groove or recess.

### Claim 18 (depends on 17)

A method according to claim 17, further comprising using a punch to insert the rivet into the sheet material, the punch having a projection that contacts the slug of material so as to deform it outwardly.

### Claim 19 (depends on 1)

A method for manufacturing a component or product including forming a joint in accordance with the method of claim 1.

### Claim 20

A method for forming a joint in a stack of at least two sheets material, at least one of the sheets being a light metal alloy, using a self-piercing rivet comprising the steps of: positioning the material over a die; providing a substantially cylindrical self-piercing rivet that is fully hollow so as to define a bore that extends along its entire length, the rivet having been coated at least along a portion of its bore by a lubricant; positioning the rivet over the sheet material at a position opposite the die; using a punch to set the rivet and force it into the sheet material such that it pierces an upper surface thereof and such that a shank of the rivet deforms outwardly to interlock with the material but without penetration to the die side of the material; wherein the die has a volume that is 70% or less of an effective solid volume of the rivet.

### Claim 21 (depends on 20)

A method according to claim 20, wherein the die volume is 60% or less of the effective solid volume of the rivet.

### Claim 22 (depends on 20)

A method for manufacturing a component or product including forming a joint in accordance with the method of claim 20.