# US 2018/0265411 A1 · Method of making refractory article resistant to high temperature shock and creep

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0265411 A1
- Document ID: US20180265411A1
- Status: Published application
- Kind: A1
- Application number: 15/461,344
- Filed: 2017-03-16
- Published: 2018-09-20
- Earliest claimed: 2017-03-16
- Assignees: Magneco/Metrel, Inc.
- Applicants: Magneco/Metrel, Inc.
- Inventors: Michael W. ANDERSON; Daniel SNYDER; Lara BINZ; Eric BORING
- Web page: https://patentgrep.com/patent/US20180265411A1

## CPC

- C04B 33/22: Grog products
- C04B 35/6316: {Binders based on silicon compounds}
- C04B 35/66: Monolithic refractories or refractory mortars, including those whether or not containing clay {(making or repairing of linings F27D1/16)}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/5427: millimeter or submillimeter sized, i.e. larger than 0,1 mm
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A method of making a refractory article having excellent high-temperature thermal shock resistance and creep resistance is provided. The method includes the step of providing a refractory composition primarily composed of chamotte having controlled particle sizes. The refractory composition may also include mullite, fused silica, calcined alumina and microsilica having controlled particle sizes, and further includes an aqueous colloidal silica binder. The refractory composition is then formed into a refractory article, which is dried and hardened.

## Claims

### Claim 1

A method of making a refractory article, comprising the following steps:
providing a refractory composition that includes, based on the weight of the composition, about 50% to about 90% by weight chamotte, about 5% to about 25% by weight mullite, about 3% to about 20% by weight fused silica, and about 3% to about 30% by weight of an aqueous colloidal silica binder;
forming the refractory article; and
drying the refractory article.

### Claim 2 (depends on 1)

The method of claim 1, wherein the refractory article is a refractory part.

### Claim 3 (depends on 1)

The method of claim 1, wherein the refractory article is a refractory container.

### Claim 4 (depends on 1)

The method of claim 1, wherein the refractory article is a refractory liner.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step of drying the refractory article comprises drying at room temperature for at least about 15 minutes, followed by baking at a temperature of at least about 100° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the chamotte comprises a first chamotte component having particles sizes ranging from 2380 to 6730 microns, a second chamotte component having particle sizes ranging from 841 to less than 2380 microns, and a third chamotte component having particle sizes less than 841 microns.

### Claim 7 (depends on 6)

The method of claim 6, wherein the chamotte comprises about 35% to about 65% by weight of the first chamotte component, about 10% to about 35% by weight of the second chamotte component, and about 15% to about 45% by weight of the third chamotte component, based on the weight of the chamotte.

### Claim 8 (depends on 1)

The method of claim 1, wherein the forming step comprises the step of casting the refractory composition into a mold.

### Claim 9 (depends on 8)

The method of claim 8, wherein the casting step comprises pouring the refractory composition.

### Claim 10 (depends on 8)

The method of claim 8, wherein the coating step comprises pumping the refractory composition.

### Claim 11

A method of making a refractory article, comprising the steps of:
providing dry ingredients that include, based on the weight of the composition, about 50% to about 90% by weight chamotte, about 5% to about 25% by weight mullite, and about 3% to about 20% by weight fused silica;
adding an aqueous colloidal silica binder to the dry ingredients, and mixing the aqueous colloidal silica binder with the dry ingredients to form the refractory composition;
forming the refractory composition into a refractory article; and
drying the refractory article.

### Claim 12 (depends on 11)

The method of claim 11, further comprising the step of casting the refractory composition.

### Claim 13 (depends on 12)

The method of claim 12, wherein the refractory composition is poured or pumped into a mold.

### Claim 14 (depends on 11)

The method of claim 11, wherein the chamotte comprises a first chamotte component having particle sizes ranging from 2380 to 6730 microns, a second chamotte component having particle sizes ranging from 841 to less than 2380 microns, and a third chamotte component having particle sizes less than 841 microns.

### Claim 15 (depends on 14)

The method of claim 14, wherein the chamotte comprises about 35% to about 65% by weight of the first chamotte component, about 10% to about 35% by weight of the second chamotte component, and about 15% to about 45% by weight of the third chamotte component, based on the weight of the chamotte.

### Claim 16 (depends on 11)

The method of claim 11, wherein the mullite has particle sizes less than 44 microns.

### Claim 17 (depends on 11)

The method of claim 11, wherein the refractory composition further comprises about 0.5% to about 4% by weight calcined alumina.

### Claim 18 (depends on 11)

The method of claim 11, wherein the refractory composition further comprises about 0.5% to about 4% by weight microsilica.

### Claim 19

A method of making a refractory article, comprising the steps of:
providing dry ingredients that include chamotte, the chamotte including about 35% to about 65% by weight of a first chamotte component having particle sizes ranging from 2380 to 6730 microns, about 10% to about 35% by weight of a second chamotte component having particle sizes ranging from about 841 to less than 2380 microns and about 15% to about 45% by weight of a third chamotte component having particle sizes less than 841 microns;
adding an aqueous colloidal silica binder to the dry ingredients, and mixing the aqueous colloidal silica binder with the dry ingredients to form the refractory composition;
forming the refractory composition into a refractory article; and
drying the refractory article.

### Claim 20 (depends on 19)

The method of claim 19, wherein the refractory composition further comprises about 5% to about 25% by weight mullite, and about 3% to about 20% by weight fused silica.