# US 2018/0076341 A1 · Silicon-containing semiconductor structures, methods of making the same and devices including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0076341 A1
- Document ID: US20180076341A1
- Status: Published application
- Kind: A1
- Application number: 15/559,081
- Filed: 2016-03-21
- Published: 2018-03-15
- Earliest claimed: 2015-03-19
- Assignees: Specmat Limited
- Applicants: Specmat, Inc.
- Inventors: Horia M. Faur; Maria Faur; Gregory C. Knight; Arjun Mendiratta
- Web page: https://patentgrep.com/patent/US20180076341A1

## CPC

- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 71/107: {Continuous treatment of the devices, e.g. roll-to roll processes or multi-chamber deposition}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/129: {Passivating}
- H10F 77/122: comprising only Group IV materials
- H10F 77/311: {for photovoltaic cells}
- H10P 50/642: {Chemical etching}
- H10P 90/15: {by making porous regions on the surface}
- Y02E 10/50: Photovoltaic [PV] energy
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A semiconductor system includes a silicon substrate and a porous silicon region disposed on the silicon substrate. The porous silicon region is configured to passivate the surface of the silicon substrate via a field effect and to reduce reflection loss on the silicon substrate via an appropriate refractive index. The porous silicon region is manufactured by a stain etching process, which retrofits existing tools for junction isolation and Phosphorus Silicon Glass (PSG) etch in solar cell manufacturing. The retrofitted tools for junction isolation and PSG etch achieves multiple purposes in a single step, including etch-back, PSG etch, antireflection coating, and passivation of the front surface of the solar cell.

## Claims

### Claim at position 1

1-67. (canceled)

### Claim 68

A semiconductor system comprising:
a silicon substrate doped with a dopant at a concentration from about 1016 cm−3 to about 1021 cm−3 and characterized by a first band gap energy; and
a porous silicon region disposed on the silicon substrate and characterized by a second band gap energy greater than the first band gap energy,
wherein the semiconductor system is configured to exhibit an electric field, generated at least partially by a difference between the first band gap energy and the second band gap energy, on an interface between the silicon substrate and the porous silicon region,
wherein the porous silicon region is configured to passivate a surface of the silicon substrate via, at least partially, an electric force induced by the electric field on a minority charge carrier in the silicon substrate, the electric force configured to be at a direction from the porous silicon region to the silicon substrate so as to increase a passivated lifetime of the minority charge carrier and passivate the surface of the silicon substrate.

### Claim 69 (depends on 68)

The semiconductor system of claim 68, wherein:
the dopant comprises phosphorous; and
a first energy potential of a first valence band in the porous silicon region is greater than a second energy potential of a second valence band in the silicon substrate so as to create the electric field.

### Claim 70 (depends on 68)

The semiconductor system of claim 68, wherein:
the dopant comprises boron; and
a first energy potential of a first conduction band in the porous silicon region is greater than a second energy potential of the second conduction band in the porous silicon region so as to create the electric field.

### Claim 71 (depends on 68)

The semiconductor system of claim 68, wherein:
the dopant comprises aluminum; and
a first energy potential of a first conduction band in the porous silicon region is greater than a second energy potential of the second conduction band in the porous silicon region so as to create the electric field.

### Claim 72 (depends on 71)

The semiconductor system of claim 71, further comprising:
at least one aluminum contact, electrically coupled to the silicon substrate, to transport majority charge carriers in the semiconductor substrate out of the semiconductor system.

### Claim 73 (depends on 68)

The semiconductor system of claim 68, wherein:
the dopant comprises gallium; and
a first energy potential of a first conduction band in the porous silicon region is greater than a second energy potential of the second conduction band in the porous silicon region so as to create the electric field.

### Claim 74 (depends on 68)

The semiconductor system of claim 68, wherein the porous silicon region is configured to have a refractive index of about 1.2 to about 3.4 so as to reduce reflection loss on the surface of the silicon substrate.

### Claim 75 (depends on 68)

The semiconductor system of claim 68, further comprising:
a silicon nitride layer disposed on the porous silicon region, wherein a first refractive index of the silicon nitride layer is smaller than a second refractive index of the porous silicon region.

### Claim 76 (depends on 68)

The semiconductor system of claim 68, wherein the surface of the silicon substrate is textured.

### Claim 77 (depends on 68)

The semiconductor system of claim 68, wherein a porosity of the porous silicon region is about 25% to about 95%.

### Claim 78 (depends on 68)

The semiconductor system of claim 68, wherein a porosity of the porous silicon region is about 25% to about 60%.

### Claim 79 (depends on 68)

The semiconductor system of claim 68, wherein a thickness of the porous silicon region is about 3 nm to about 30 nm.

### Claim 80 (depends on 68)

The semiconductor system of claim 68, wherein a thickness of the porous silicon region is about 5 nm to about 20 nm.

### Claim 81 (depends on 68)

The semiconductor system of claim 68, wherein the passivated lifetime of the minority charge carrier is about 10 microseconds to about 1000 microseconds.

### Claim 82 (depends on 68)

The semiconductor system of claim 68, wherein the difference between the first band gap energy and the second band gap energy is greater than 500 meV.

### Claim 83 (depends on 68)

The semiconductor system of claim 68, wherein the porous silicon region is configured to increase a sheet resistance of the silicon substrate by about 5% to about 20%.

### Claim 84

A method of facilitating fabrication of a solar cell via a stain etching process using a junction isolation/phosphosilicate glass (PSG) etch processing tool, the method comprising:
(A) placing a first stain etching solution in a first reservoir coupled to a PSG etch tank in the junction isolation/PSG etch processing tool through a first chemical dosing unit of the PSG etch processing tool;
(B) placing at least a portion of a silicon substrate for the solar cell in the PSG etch tank and allowing contact, in the PSG etch tank, between the silicon substrate and the first stain etching solution in the first reservoir;
(C) removing possible PSG on a front side of the silicon substrate during a first time period via the contact between the silicon substrate and the first stain etching solution;
(D) etching back at least a portion of the front side of the silicon substrate during a second time period via the contact between the silicon substrate and the first stain etching solution; and
(E) passivating the front side of the silicon substrate and reducing a reflection loss on the front side of the silicon substrate, at least partially, by creating a front side porous silicon region on the front side of the silicon substrate during a third time period via the contact between the silicon substrate and the first stain etching solution,
wherein at least a portion of the second time period and the third time period is concurrent.

### Claim 85 (depends on 84)

The method of claim 84, wherein at least a portion of the first time period, the second time period, and the third time period is concurrent.

### Claim 86 (depends on 84)

The method of claim 84, further comprising:
(F) placing a second stain etching solution in a second reservoir coupled to a junction isolation process tank through a second chemical dosing unit of the junction isolation/PSG etch processing tool;
(G) placing at least a portion of the silicon substrate for the solar cell in the junction isolation process tank and allowing contact, in the junction isolation process tank, between the silicon substrate and the second stain etching solution in the second reservoir; and
(H) creating a back side porous silicon region on a back side of the silicon substrate via the contact between the silicon substrate and the second stain etching solution so as to passivate the back side of the silicon substrate.

### Claim 87 (depends on 86)

The method of claim 86, further comprising:
(I) doping the back side of the silicon substrate with a first doping material, before creating the back side porous silicon region.

### Claim 88 (depends on 87)

The method of claim 87, wherein Step (I) comprises at least one of a thermal diffusion process, an ion implantation process or a laser doping process.

### Claim 89 (depends on 87)

The method of claim 87, further comprising:
(J) doping the front side of the silicon substrate with a second doping material, before creating the front side porous silicon region.

### Claim 90 (depends on 87)

The method of claim 87, further comprising:
(K) depositing a silicon nitride (SiNx) layer over the front side porous silicon layer via a plasma enhanced chemical vapor deposition (PECVD) process.

### Claim 91

A solar cell comprising:
a silicon substrate comprising an emitter region on a front side of the silicon substrate and a base region on a back side of the silicon substrate;
a front side passivation layer disposed on the emitter region, wherein the front side passivation layer comprises a first porous silicon region in contact with the emitter region;
an antireflection and passivation coating, disposed on the front side passivation layer, to reduce reflection loss on the front side of the silicon substrate and further increase a minority carrier lifetime of minority charge carriers in the emitter region; and
a back side passivation layer disposed on the base region, wherein the back side passivation layer comprises a second porous silicon region.

### Claim 92 (depends on 91)

The solar cell of claim 91, further comprising:
a back surface field (BSF) layer disposed between the base region and the second porous silicon region.

### Claim 93 (depends on 91)

The solar cell of claim 91, wherein at least one of the first porous silicon region and the second porous silicon region has a porosity of about 25% to about 95%.

### Claim 94 (depends on 91)

The solar cell of claim 91, wherein at least one of the first porous silicon region and the second porous silicon region has a porosity of about 25% to about 60%.

### Claim 95 (depends on 91)

The solar cell of claim 91, wherein at least one of the first porous silicon region and the second porous silicon region has a thickness of about 3 nm to about 30 nm.

### Claim 96 (depends on 91)

The solar cell of claim 91, further comprising:
a plurality of metal contacts electrically coupled to a first doped region in the emitter region and formed through the antireflection and passivation coating and the front side passivation layer, wherein the first doped region has a first doping concentration greater than a second doping concentration of a second doped region at least partially underneath the front side passivation layer.