# US 2018/0026179 A1 · Fully Compensated Synthetic Ferromagnet for Spintronics Applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0026179 A1
- Document ID: US20180026179A1
- Status: Published application
- Kind: A1
- Application number: 15/707,373
- Filed: 2017-09-18
- Published: 2018-01-25
- Earliest claimed: 2015-11-23
- Assignees: Headway Technologies, Inc.
- Applicants: Headway Technologies, Inc.
- Inventors: Jian Zhu; Guenole Jan; Yuan-Jen Lee; Huanlong Liu; Ru-Ying Tong; Po-Kang Wang
- Web page: https://patentgrep.com/patent/US20180026179A1

## CPC

- H10N 50/10: Magnetoresistive devices
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H01F 10/16: containing cobalt ({H01F10/126} , H01F10/13 take precedence)
- H01F 10/30: characterised by the composition of the intermediate layers {, e.g. seed, buffer, template, diffusion preventing, cap layers (H01F10/06 and H01F10/32 take precedence)}
- H01F 10/32: Spin-exchange-coupled multilayers, e.g. nanostructured superlattices {(applying spin-exchange-coupled multilayers to substrates H01F41/302)}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H10N 50/01: Manufacture or treatment
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A laminated seed layer stack with a smooth top surface having a peak to peak roughness of 0.5 nm is formed by sequentially sputter depositing a first seed layer, a first amorphous layer, a second seed layer, and a second amorphous layer where each seed layer may be Mg and has a resputtering rate 2 to 30× that of the amorphous layers that are TaN, SiN, or a CoFeM alloy. A template layer that is NiCr or NiFeCr is formed on the second amorphous layer. As a result, perpendicular magnetic anisotropy in an overlying magnetic layer that is a reference layer, free layer, or dipole layer is substantially maintained during high temperature processing up to 400° C. and is advantageous for magnetic tunnel junctions in embedded MRAMs, spintronic devices, or in read head sensors. The laminated seed layer stack may include a bottommost Ta or TaN buffer layer.

## Claims

### Claim 1

A multilayer structure for reducing film roughness in a magnetic device, comprising:
(a) a first layer made of a material with a first bond energy, and having a first surface with an “as deposited” first peak to peak roughness;
(b) a second layer that is non-crystalline or nano-crystalline and is made of a material with a second bond energy that is greater than the first bond energy such that deposition of the second layer on the first layer results in resputtering of the first layer to give a first layer with a second surface having a second peak to peak roughness substantially less than the “as deposited” first peak to peak roughness, and the second layer formed on the second surface, the second layer has a third surface with the second peak to peak roughness;
(c) a third layer made of a material with the first bond energy formed on the third surface of the second layer; and
(d) a fourth layer that is non-crystalline or nano-crystalline with the second bond energy, and formed on a top surface of the third layer.

### Claim 2 (depends on 1)

The multilayer structure of claim 1 further comprised of a template layer formed on the top surface of the fourth layer and with a top surface having the second peak to peak roughness, the template layer has a (111) crystal orientation to promote perpendicular magnetic anisotropy (PMA) in an overlying magnetic layer.

### Claim 3 (depends on 1)

The multilayer structure of claim 1 further comprising a buffer layer that is Ta or TaN and is formed on a substrate, the buffer layer contacts a bottom surface of the first layer.

### Claim 4 (depends on 2)

The multilayer structure of claim 2 wherein the template layer is one of NiCr and NiFeCr.

### Claim 5 (depends on 1)

The multilayer structure of claim 1 wherein each of the first layer and third layer is one or more of Mg, Al, Si, C, B, Mn, Rb, Zn, and Ti.

### Claim 6 (depends on 1)

The multilayer structure of claim 1 wherein each of the second layer and fourth layer is one of TaN, SiN, and a CoFeM alloy wherein M is one of B, P, Ta, Zr, Si, Cu, Hf, Mo, W, and Nb with a content which makes the CoFeM alloy amorphous as deposited.

### Claim 7 (depends on 1)

The multilayer structure of claim 1 wherein each of the first layer and third layer has a thickness from about 3 to 20 Angstroms.

### Claim 8 (depends on 1)

The multilayer structure of claim 1 wherein each of the second layer and fourth layer has a thickness from about 2 to 15 Angstroms.

### Claim 9 (depends on 2)

The multilayer structure of claim 2 wherein the overlying magnetic layer contacts the top surface of the template layer, and is a reference layer in a magnetic tunnel junction (MTJ) having a bottom spin valve configuration, or is a free layer in a MTJ with a top spin valve configuration.

### Claim 10 (depends on 1)

The multilayer structure of claim 1 wherein the overlying magnetic layer is a reference layer, free layer, or dipole layer in a magnetic random access memory (MRAM) device, spin torque oscillator (STO), spintronic device, or a read head sensor.

### Claim 11

A magnetic tunnel junction (MTJ), comprising:
(a) a first seed layer (SL1) stack, comprising:
(1) a first smoothing layer formed on a substrate, the first smoothing layer comprises a lower first layer with a first resputtering rate, and an upper second layer that is non-crystalline or nano-crystalline and has a second resputtering rate wherein the first resputtering rate is about 2 to 30 times greater than the second resputtering rate; and
(2) a first template layer formed on a top surface of the upper second layer and with a top surface having a peak to peak roughness of about 0.5 nm, the first template layer has a (111) crystal orientation to promote PMA in an overlying magnetic layer;
(b) a reference layer (RL) formed on the first template layer;
(c) a tunnel barrier layer formed on the RL;
(d) a free layer (FL) on the tunnel barrier layer;
(e) a non-magnetic spacer formed on the FL;
(f) a second seed layer stack (SL2) on the non-magnetic spacer, comprising:
(1) a second smoothing layer formed on the non-magnetic spacer, the second smoothing layer comprises a lower third layer with a third resputtering rate, and an upper fourth layer that is non-crystalline or nano-crystalline and has a fourth resputtering rate wherein the third resputtering rate is about 2 to 30 times greater than the fourth resputtering rate; and
(2) a second template layer formed on a top surface of the upper fourth layer and with a top surface having a peak to peak roughness of about 0.5 nm;
(g) a dipole layer formed on the second template layer; and
(h) an uppermost capping layer.

### Claim 12 (depends on 11)

The MTJ of claim 11 further comprising a buffer layer that is one of Ta or TaN formed on the substrate and contacting a bottom surface of the first smoothing layer.

### Claim 13 (depends on 11)

The MTJ of claim 11 wherein the first template layer is one of NiCr and NiFeCr.

### Claim 14 (depends on 11)

The MTJ of claim 11 wherein each of the lower first layer and lower third layer is one or more of Mg, Al, Si, C, B, Mn, Rb, Zn, and Ti.

### Claim 15 (depends on 11)

The MTJ of claim 11 wherein each of the upper second layer and upper fourth layer is one of TaN, SiN, and a CoFeM alloy wherein M is one of B, P, Ta, Zr, Si, Cu, Hf, Mo, W, and Nb with a content which makes the CoFeM alloy amorphous as deposited.

### Claim 16

A method of forming a magnetic tunnel junction (MTJ), comprising:
(a) forming a first seed layer (SL1) stack, comprising:
(1) sputter depositing a first seed layer with a first bond energy on a substrate, the first seed layer has a first surface with a first peak to peak roughness;
(2) sputter depositing a second seed layer that is non-crystalline or nano-crystalline and with a second bond energy on the first seed layer, the second bond energy is greater than the first bond energy, and results in a second surface on the first seed layer with a second peak to peak roughness substantially less than the first peak to peak roughness, and the second seed layer formed on the second surface, the second seed layer has a third surface with the second peak to roughness; and
(3) sputter depositing a template seed layer on the third surface of the second seed layer, the template seed layer has a (111) crystal orientation with a top surface having the second peak to peak roughness, and promotes perpendicular magnetic anisotropy (PMA) in an overlying magnetic layer; and
(b) depositing the overlying magnetic layer that contacts the top surface of the template layer.

### Claim 17 (depends on 16)

The method of claim 16 further comprised of sputter depositing a buffer layer that is Ta or TaN on the substrate before sputter depositing the first seed layer.

### Claim 18 (depends on 16)

The method of claim 16 wherein the second seed layer is sputter deposited with a process comprising an inert gas that is Ar, a base pressure between 5×10−8 and 5×10−9 torr, a sputter deposition chamber temperature up to 400° C., and a forward power of 20 W to 5000 W applied to one or more targets.

### Claim 19 (depends on 16)

The method of claim 16 wherein the template seed layer is one of NiCr and NiFeCr.

### Claim 20 (depends on 16)

The method of claim 16 wherein the overlying magnetic layer is a reference layer (RL), and the method further comprises forming a tunnel barrier, a free layer (FL), and a capping layer to give a SL1/RL/tunnel barrier/FL/capping layer configuration for the MTJ.

### Claim 21 (depends on 20)

The method of claim 20 further comprised of forming a non-magnetic spacer, a second seed layer (SL2) comprising the first seed layer stack, and a dipole layer on the free layer before depositing the capping layer.

### Claim 22 (depends on 16)

The method of claim 16 wherein forming the first seed layer stack further comprises sputter depositing a third seed layer with the first bond energy that contacts a top surface of the second seed layer, and then sputter depositing a fourth layer with the second bond energy on the third seed layer.

### Claim 23 (depends on 16)

The method of claim 16 wherein the first seed layer is one of Mg, Al, Si, C, B, Mn, Rb, Zn, and Ti.

### Claim 24 (depends on 16)

The method of claim 16 wherein the second seed layer is one of TaN, SiN, and a CoFeM alloy wherein M is one of B, P, Ta, Zr, Si, Cu, Hf, Mo, W, and Nb with a content which makes the CoFeM alloy amorphous as deposited.

### Claim 25 (depends on 16)

The method of claim 16 wherein the first seed layer has a thickness from about 3 to 100 Angstroms.

### Claim 26 (depends on 16)

The method of claim 16 wherein the second seed layer has a thickness from about 1 to 100 Angstroms.