# US 2018/0026156 A1 · Light Emitting Diode and Fabrication Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0026156 A1
- Document ID: US20180026156A1
- Status: Published application
- Kind: A1
- Application number: 15/723,720
- Filed: 2017-10-03
- Published: 2018-01-25
- Earliest claimed: 2015-11-24
- Assignees: Xiamen Sanan Optoelectronics Technology Co., Ltd.
- Applicants: Xiamen Sanan Optoelectronics Technology Co., Ltd.
- Inventors: Jie ZHANG; Xueliang ZHU; Chengxiao DU; Jianming LIU; Chen-ke HSU
- Web page: https://patentgrep.com/patent/US20180026156A1

## CPC

- H10H 20/817: characterised by the crystal structures or orientations, e.g. polycrystalline, amorphous or porous
- H10H 20/0137: {the light-emitting regions comprising nitride materials}
- H10H 20/8252: {characterised by the dopants}
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A light-emitting diode (LED) chip includes from bottom to up: a conductive substrate, a p-type nitride layer, an active layer, an n-type recovery layer, an n-type nitride layer and an n electrode, wherein, the n-type nitride layer has a nitride polarity crystal and a gallium polarity crystal, and the surfaces of the nitride polarity and the gallium polarity regions appear different in height, the n-type recovery layer surface approximate to the n-type nitride layer has consistent mixed polarity with the n-type nitride layer, and the surface far from the n-type nitride layer is a connected gallium polarity surface.

## Claims

### Claim 1

A light-emitting diode (LED) epitaxial structure, comprising:
a substrate, having an upper surface and a bottom surface opposite to each other, wherein a portion of the upper surface is nitrided;
an n-type nitride layer having a nitride polarity crystal and a gallium polarity crystal, formed on the upper surface of the substrate, wherein the nitride polarity crystal is grown over the nitrided portion of the substrate, and surfaces of the nitride polarity and the gallium polarity regions have different heights;
an n-type recovery layer, formed over the n-type nitride layer, wherein the upper surface is a connected gallium polarity surface;
an active layer, formed over the n-type recovery layer; and
a p-type layer, formed over the active layer.

### Claim 2 (depends on 1)

The LED epitaxial structure of claim 1, wherein: the nitrided region on the substrate upper surface is a periodically-arranged band-shaped or block-shaped pattern, with size of 10-200 nm.

### Claim 3 (depends on 1)

The LED epitaxial structure of claim 1, wherein: the nitride polarity crystal and the gallium polarity crystal of the n-type nitride layer are alternatively arranged.

### Claim 4 (depends on 1)

The LED epitaxial structure of claim 1, wherein: the n-type recovery layer is 0.3-1 μm thick with doping concentration of 2E17-5E18 cm−3.

### Claim 5

A vertical light-emitting diode (LED) chip, comprising from bottom up:
a conductive substrate;
a p-type nitride layer;
an active layer;
an n-type recovery layer;
an n-type nitride layer; and
an n electrode;
wherein: the n-type nitride layer has a nitride polarity crystal and a gallium polarity crystal, and the surfaces of the nitride polarity and the gallium polarity regions appear different in height, the n-type recovery layer surface approximate to the n-type nitride layer has consistent mixed polarity with the n-type nitride layer, and the other surface far from the n-type nitride layer is a connected gallium polarity surface.

### Claim 6 (depends on 5)

The vertical LED chip of claim 5, wherein: the nitride polarity crystal and the gallium polarity crystal of the n-type nitride layer are alternatively arranged.

### Claim 7 (depends on 5)

The vertical LED chip of claim 5, wherein: at least half of the upper surface of the n-type nitride layer is a gallium polarity surface.

### Claim 8 (depends on 5)

The vertical LED chip of claim 5, wherein: the n-type recovery layer is 0.3-1 μm thick with doping concentration of 2E17-5E18 cm−3.

### Claim 9

A fabrication method, comprising:
1) providing a substrate having an upper surface and a bottom surface opposite to each other, and nitriding a portion of the upper surface;
2) growing an n-type nitride layer having a nitride polarity crystal and a gallium polarity crystal on the upper surface of the substrate, wherein, the nitride polarity crystal is grown above the nitrided region of the substrate, and the surfaces of the nitride polarity and the gallium polarity regions appear different in height;
3) growing an n-type recovery layer on the n-type nitride layer, wherein, the upper surface is a connected gallium polarity surface;
4) growing an active layer and a p-type nitride layer in sequence on the n-type recovery layer, to form an LED epitaxial structure;
5) providing a conductive substrate, and connecting the conductive substrate to one side surface of the p-type nitride layer of the aforesaid LED epitaxial structure; and
6) removing the substrate of the LED epitaxial structure to expose the surface of the n-type nitride layer, and fabricating an n electrode thereon;
wherein the fabricated LED epitaxial structure comprises:
the substrate, having an upper surface and a bottom surface opposite to each other, wherein a portion of the upper surface is nitrided;
the n-type nitride layer having a nitride polarity crystal and a gallium polarity crystal, formed on the upper surface of the substrate, wherein the nitride polarity crystal is grown over the nitrided portion of the substrate, and surfaces of the nitride polarity and the gallium polarity regions have different heights;
the n-type recovery layer, formed over the n-type nitride layer, wherein the upper surface is a connected gallium polarity surface;
the active layer, formed over the n-type recovery layer; and
the p-type layer, formed over the active layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein: in step 1), the nitrided portion on the substrate upper surface is a periodically-arranged band-shaped or block-shaped pattern, with size of 10-200 nm.

### Claim 11 (depends on 9)

The method of claim 9, wherein: in step 3), improve lateral epitaxial capacity of the gallium polarity region by controlling growth temperature, pressure and growth rate, and form a connected gallium polarity surface after completion.

### Claim 12 (depends on 11)

The method of claim 11, wherein: in step 3), growing temperature is 1,100-1,150° C., pressure is 100-150 torr, and growing rate is below 1 μm/h.

### Claim 13 (depends on 9)

The method of claim 9, wherein: in step 6), remove the substrate to expose the epitaxial structure surface, etch the exposed surface with wet etching, and form surfaces with height difference on the n-type nitride layer surface.

### Claim 14 (depends on 9)

The method of claim 9, wherein: the nitride polarity crystal and the gallium polarity crystal of the n-type nitride layer are alternatively arranged.

### Claim 15 (depends on 9)

The method of claim 9, wherein: at least half of the upper surface of the n-type nitride layer is a gallium polarity surface.

### Claim 16 (depends on 9)

The method of claim 9, wherein: the n-type recovery layer is 0.3-1 μm thick with a doping concentration of 2E17-5E18 cm−3.