# US 2018/0026118 A1 · Multiple step thin film deposition method for high conformality

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0026118 A1
- Document ID: US20180026118A1
- Status: Published application
- Kind: A1
- Application number: 15/174,147
- Filed: 2016-07-22
- Published: 2018-01-25
- Earliest claimed: 2016-07-22
- Assignees: Globalfoundries Inc.
- Applicants: Globalfoundries Inc.
- Inventors: Nicolas L. Breil; Neal A. Makela; Praneet Adusumilli; Domingo A. Ferrer
- Web page: https://patentgrep.com/patent/US20180026118A1

## CPC

- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/405: {Orientations of crystalline planes}
- H10P 14/44: Physical vapour deposition [PVD]
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

During a physical vapor deposition (PVD) process, the ion energy of a depositing species is controlled. By varying the ion energy throughout the process, the degree of conformality of the deposited layer over three-dimensional structures, including the extent to which the deposited layer merges between adjacent structures can be controlled.

## Claims

### Claim 1

A method of forming a semiconductor structure comprising:
forming a plurality of semiconductor fins on a substrate;
forming a plurality of raised active regions on the semiconductor fins;
forming a plasma within a vacuum chamber;
depositing a first portion of a conformal conductive layer over the raised active regions at a first ion energy; and
depositing a second portion of the conformal conductive layer over the first portion at a second ion energy.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first ion energy is less than the second ion energy.

### Claim 3 (depends on 2)

The method of claim 2, wherein the conformal conductive layer does not merge adjacent raised active regions.

### Claim 4 (depends on 2)

The method of claim 2, wherein a self-bias voltage during deposition of the first portion is from 100 to 200 V.

### Claim 5 (depends on 2)

The method of claim 2, wherein a self-bias voltage during deposition of the second portion is from −50 to 90 V.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first ion energy is greater than the second ion energy.

### Claim 7 (depends on 6)

The method of claim 6, wherein the conformal conductive layer merges adjacent raised active regions.

### Claim 8 (depends on 6)

The method of claim 6, wherein a self-bias voltage during deposition of the first portion is from −50 to 90 V.

### Claim 9 (depends on 6)

The method of claim 6, wherein a self-bias voltage during deposition of the second portion is from 100 to 200 V.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first portion and the second portion each comprise titanium.

### Claim 11 (depends on 1)

The method of claim 1, wherein the vacuum chamber pressure is constant during deposition of the conformal conductive layer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the power applied to the plasma is constant during deposition of the conformal conductive layer.

### Claim 13 (depends on 1)

The method of claim 1, wherein the oxygen concentration within the deposited layer is less than 500 ppm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the halide concentration within the deposited layer is less than 500 ppm.

### Claim 15

A method of forming a semiconductor structure within a vacuum chamber comprising:
plasma depositing a first portion of a conformal conductive layer over raised regions disposed on a semiconductor substrate at a first ion energy; and
plasma depositing a second portion of the conformal conductive layer over the first portion at a second ion energy.

### Claim 16 (depends on 15)

The method of claim 15, wherein a self-bias voltage during deposition of the first portion is from −50 to 90 V and a self-bias voltage during deposition of the second portion is from 100 to 200 V.

### Claim 17 (depends on 15)

The method of claim 15, wherein the vacuum chamber pressure is constant during deposition of the conformal conductive layer.

### Claim 18 (depends on 15)

The method of claim 15, wherein the power applied to the plasma is constant during deposition of the conformal conductive layer.

### Claim 19

A semiconductor structure comprising:
a semiconductor substrate having a plurality of fins formed thereon;
epitaxial active regions disposed over of the fins; and
a conductive layer disposed over the epitaxial active regions, wherein the conductive layer on an upper surface of the epitaxial active regions has an apex thickness, a turn thickness and a lateral edge thickness, and a coefficient of variation of the apex thickness, turn thickness and lateral edge thickness is 0.1 to 0.45.

### Claim 20 (depends on 19)

The semiconductor structure of claim 19, wherein the conductive layer merges adjacent active regions.

### Claim 21

A method of forming a semiconductor structure comprising:
forming a plurality of semiconductor fins on a substrate;
forming a plurality of raised active regions on the semiconductor fins;
depositing a first portion of a conductive layer over the raised active regions at a first ion energy; and
depositing a second portion of the conductive layer over the first portion at a second ion energy, wherein the oxygen concentration within the deposited layer is less than 500 ppm.