# US 2018/0025846 A1 · Method for manufacturing high-voltage solid-electrolyte aluminum electrolytic capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2018/0025846 A1
- Document ID: US20180025846A1
- Status: Published application
- Kind: A1
- Application number: 15/548,975
- Filed: 2015-03-03
- Published: 2018-01-25
- Earliest claimed: 2015-02-06
- Assignees: Zhaoqing Beryl Electronic Technology Co., Ltd.
- Applicants: Zhaoqing Beryl Electronic Technology Co., Ltd.
- Inventors: Yongpeng Liu; Yanbin Ma; Yong Yuan; Wei Luo; Ping Zheng; Qiong Liao; Huifeng Li; Dirong Wu; Weiqiao Wu
- Web page: https://patentgrep.com/patent/US20180025846A1

## CPC

- H01G 9/0029: {Processes of manufacture}
- H01G 9/15: Solid electrolytic capacitors (H01G11/00 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A method for manufacturing high-voltage solid electrolyte aluminum-electrolytic capacitor: (1) welding a capacitor core onto an iron bar, applying a voltage for chemical treatment, and then, washing and drying; (2) impregnating the core in dispersion A for 1˜30 minutes; (3) removing the core from dispersion A, creating vacuum and impregnating the core in dispersion A for 1˜10 minutes; (4) keeping the core in dispersion A, breaking the vacuum and performing pressurization, and keeping pressurized state for 1˜10 minutes; (5) keeping the core in the dispersion A, performing depressurization to atmospheric pressure, and keeping atmospheric pressure for 1˜10 minutes; (6) taking the core out, placing in a 65˜100° C. temperature of and drying it for 20˜60 minutes, and then placing in a 135˜165° C. temperature of and drying for 20˜60 minutes; (7) repeating (3) to (6) at least once; and (8) putting the core in an aluminum cover and sealing it, and performing aging treatment.

## Claims

### Claim 1

A method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor, comprising:
(1) welding a capacitor core of a capacitor onto an iron bar, applying a voltage for chemical treatment, and after the chemical treatment, washing and drying the capacitor core;
(2) impregnating the dried capacitor core in a dispersion for 1˜30 minutes;
(3) removing the capacitor core out of the dispersion, creating a vacuum and then impregnating the capacitor core in the dispersion for 1˜10 minutes;
(4) keeping the capacitor core in the dispersion, breaking the vacuum and then performing pressurization, and keeping the pressurized state for 1˜10 minutes;
(5) keeping the capacitor core in the dispersion, performing depressurization to an atmospheric pressure, and keeping the atmospheric pressure for 1˜10 minutes;
(6) taking the capacitor core out, placing the capacitor core in a 65˜100° C. temperature of and drying it for 20˜60 minutes, and then placing the capacitor core in a 135˜165° C. temperature of and drying it for 20˜60 minutes;
(7) repeating steps (3) to (6) at least once;
(8) putting the capacitor core in an aluminum cover and sealing it, and performing aging treatment to obtain a high-voltage solid electrolyte aluminum-electrolytic capacitor, wherein
the dispersion A is a dispersion that comprises conductive polymers.

### Claim 2 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein a vacuum degree of the vacuum created in step (3) is 700˜970 Pa.

### Claim 3 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein the pressurizing in step (4) refers to feeding compressed air until 0.1˜0.6 MPa.

### Claim 4 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein step (7) is to repeat steps (3) to (6) five times.

### Claim 5 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein the dispersion in step (2) is a polymer dispersion, and the polymer dispersion is a poly (3,4-ethylene dioxythiophene).

### Claim 6 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein the capacitor core in step (2) is formed by winding Asahi Kasel ADS040060 electrolytic paper between a JCC anodized foil and a Nanofoil cathode foil.

### Claim 7 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein the manufacturing method comprises:
(1) welding the capacitor core of the capacitor onto the iron bar, applying the voltage for chemical treatment, and after the chemical treatment, washing and drying the capacitor core;
(2) impregnating the dried capacitor core in the dispersion for 15 minutes;
(3) removing the capacitor core out of the dispersion, creating a vacuum to reach an 850 Pa vacuum state and then impregnating the capacitor core in the dispersion for 5 minutes;
(4) keeping the capacitor core in the dispersion, breaking the vacuum and then feeding compressed air until 0.5 MPa, and keeping the pressurized state for 5 minutes;
(5) keeping the capacitor core in the dispersion, performing depressurization to the atmospheric pressure state, and keeping the atmospheric pressure state for 5 minutes;
(6) taking the capacitor core out, placing the capacitor core in an 85° C. low temperature of and drying it for 60 minutes, then placing the capacitor core in a 150° C. high temperature of and drying it for 30 minutes, and taking the capacitor core out;
(7) repeating steps (3) to (6) five times;
(8) putting the capacitor core in an aluminum cover and sealing it, and performing aging treatment to obtain a high-voltage solid electrolyte aluminum-electrolytic capacitor, wherein
the dispersion A is a dispersion that comprises conductive polymers.

### Claim 8 (depends on 1)

The method for manufacturing a high-voltage solid electrolyte aluminum-electrolytic capacitor according to claim 1, wherein the drying in step (1) is specifically: drying the capacitor core in a 50˜100° C. low temperature of for 20˜100 minutes first, and then drying it in a 110˜200° C. high temperature of for 20˜60 minutes.